Effect of Bonding Temperature on the Interfacial Micro-structure and Performance of Mild Steel/Austenite Stainless Steel Diffusion-Bonded Joint
Received date: 2016-07-18
Online published: 2017-02-22
Supported by
Supported by National Natural Science Foundation of China (No.51375083)
The Q235A mild steel and AISI304 austenite stainless steel were subjected to solid diffusion welding by vacuum diffusion bonding approach to investigate the influence of welding temperature on the interfacial morphology, microstructural constituents and mechanical properties. The results show that the single ferrite layer (zone II) and carbon-enriched layer (zone III) were formed nearby the bonding interface of Q235A mild steel and AISI304 austenite stainless steel, and heterogeneous microstructure on both sides of interface formed a common grain boundary by diffusion. The strength and toughness of the bonded joint reached the highest values, for welding temperature of approximately 850 ℃, welding pressure of beyond 10 MPa, and welding time of approximately 60 min, which was larger than those of the Q235A mild steel layer. Otherwise, the Cr23C6 carbide easily formed at a relatively lower temperature (≤800 ℃), whereas the secondary carbides and intermetallic compounds formed at a relatively higher temperature (≥900 ℃). Both cases would dramatically deteriorate the strength-toughness of the bonded joint. Therefore, it was proposed that the brittle precipitate phases can be effectively avoided by controlling the welding temperature to approximately 850 ℃, thus ensuring the resulting performance of the bonded joint.
Dawei WANG , Shichao XIU . Effect of Bonding Temperature on the Interfacial Micro-structure and Performance of Mild Steel/Austenite Stainless Steel Diffusion-Bonded Joint[J]. Acta Metall Sin, 2017 , 53(5) : 567 -574 . DOI: 10.11900/0412.1961.2016.00307
| [1] | Khorrami M S, Mostafaei M A, Pouraliakbar H, et al.Study on microstructure and mechanical characteristics of low-carbon steel and ferritic stainless steel joints[J]. Mater. Sci. Eng., 2014, A608: 35 |
| [2] | Mas F, Martin G, Lhuissier P, et al.Heterogeneities in local plastic flow behavior in a dissimilar weld between low-alloy steel and stainless steel[J]. Mater. Sci. Eng., 2016, A667: 156 |
| [3] | Khalifeh A R, Dehghan A, Hajjari E.Dissimilar joining of AISI 304L/St37 steels by TIG welding process[J]. Acta. Metall. Sin.(Engl. Lett.), 2013, 26: 721 |
| [4] | Torkamany M J, Sabbaghzadeh J, Hamedi M J.Effect of laser welding mode on the microstructure and mechanical performance of dissimilar laser spot welds between low carbon and austenitic stainless steels[J]. Mater. Des., 2012, 34: 666 |
| [5] | Haneklaus N, Reuven R, Cionea C, et al.Tube expansion and diffusion bonding of 316L stainless steel tube-to-tube sheet joints using a commercial roller tube expander[J]. J. Mater. Process. Technol., 2016, 234: 27 |
| [6] | Kurt B, ?alik A.Interface structure of diffusion bonded duplex stainless steel and medium carbon steel couple[J]. Mater. Charact., 2009, 60: 1035 |
| [7] | Atabaki M M, Bajgholi M E, Dehkordi E H.Partial transient liquid phase diffusion bonding of zirconium alloy (Zr-2.5Nb) to stainless steel 321[J]. Mater. Des., 2012, 42: 172 |
| [8] | Deng Y Q, Sheng G M, Yin L J.Impulse pressuring diffusion bonding of titanium to stainless steel using a copper interlayer[J]. Rare Met. Mater. Eng., 2015, 44: 1041 |
| [9] | Kundu S, Chatterjee S.Interfacial microstructure and mechanical properties of diffusion-bonded titanium-stainless steel joints using a nickel interlayer[J]. Mater. Sci. Eng., 2006, A425: 107 |
| [10] | Balasubramanian M.Application of Box-Behnken design for fabrication of titanium alloy and 304 stainless steel joints with silver interlayer by diffusion bonding[J]. Mater. Des., 2015, 77: 161 |
| [11] | Yuan X J, Kang C Y.Microstructural characteristics in vacuum TLP (transient liquid phase) bonds using a novel iron-based interlayer based on duplex stainless steel base metal alloyed with a melting-point depressant[J]. Vacuum, 2014, 99: 12 |
| [12] | Wu M F, Kuang H J, Wang F J, et al.Partially transient liquid phase-diffusion bonding on Ti(C, N)-Al2O3 ceramic matrix composites using Zr/Cu/Zr as interlayer[J]. Acta Metall. Sin., 2014, 50: 619 |
| [12] | (吴铭方, 匡鸿锦, 王凤江等. Zr/Cu/Zr部分瞬间液相焊扩散连接Ti(C, N)-Al2O3陶瓷基复合材料[J]. 金属学报, 2014, 50: 619) |
| [13] | Zhang X, Shi X H, Wang J, et al.Effect of bonding temperature on the microstructures and strengths of C/C composite/GH3044 alloy joints by partial transient liquid-phase (PTLP) bonding with multiple interlayers[J]. Acta Metall. Sin.(Engl. Lett.), 2014, 27: 663 |
| [14] | Peng F, Dong X H, Liu K, et al.Effects of strain rate and plastic work on martensitic transformation kinetics of austenitic stainless steel 304[J]. J. Iron Steel Res. Int., 2015, 22: 931 |
| [15] | Li X F, Ding W, Cao J, et al.In situ TEM observation on martensitic transformation during tensile deformation of SUS304 metastable austenitic stainless steel[J]. Acta Metall. Sin.(Engl. Lett.), 2015, 28: 302 |
| [16] | Liu H P, Liu B, Li D Z, et al.Microstructural characterization of welded joint in duplex stainless steel by laser continuous heat treatment[J]. J. Iron Steel Res. Int., 2014, 21: 710 |
| [17] | Abraham S T, Albert S K, Das C R, et al.Assessment of sensitization in AISI 304 stainless steel by nonlinear ultrasonic method[J]. Acta Metall. Sin.(Engl. Lett.), 2013, 26: 545 |
| [18] | Qi Z F.Diffusion and Phase Transition in Solid Metals [M]. Beijing: China Machine Press, 1998: 107 |
| [18] | (戚正风. 固态金属中的扩散与相变 [M]. 北京: 机械工业出版社, 1998: 107) |
| [19] | Zhao Z Y.Alloy Steel Design [M]. Beijing: National Defense Industry Press, 1999: 250 |
| [19] | (赵振业. 合金钢设计 [M]. 北京: 国防工业出版社, 1999: 250) |
| [20] | Cui Z Q.Metal and Heat Treatment [M]. Beijing: China Machine Press, 1993: 234 |
| [20] | (崔忠圻. 金属学与热处理 [M]. 北京: 机械工业出版社, 1993: 234) |
| [21] | Dobrzański L A, Brytan Z, Grande M A, et al.Innovative PM duplex stainless steels obtained basing on the schaeffler diagram[J]. Arch. Mater. Sci. Eng., 2008, 30: 49 |
| [22] | Pacquentin W, Caron N, Oltra R.Effect of microstructure and chemical composition on localized corrosion resistance of a AISI 304L stainless steel after nanopulsed-laser surface melting[J]. Appl. Surf. Sci., 2015, 356: 561 |
| [23] | Gómez X, Echeberria J.Microstructure and mechanical properties of carbon steel A210-superalloy Sanicro 28 bimetallic tubes[J]. Mater. Sci. Eng., 2003, A348: 180 |
| [24] | Ghosh C, Paul A.Elucidation of bifurcation of the kirkendall marker plane in a single phase using physico-chemical approach[J]. Intermetallics, 2008, 16: 955 |
| [25] | Svoboda J, Fischer F D, Abart R.Modeling of diffusional phase transformation in multi-component systems with stoichiometric phases[J]. Acta Mater., 2010, 58: 2905 |
/
| 〈 |
|
〉 |