INFLUENCE OF SUBSTRATE MECHANICAL PROPER-TIES ON DEPOSITION BEHAVIOUR OF 316L STAINLESS STEEL POWDER
Received date: 2016-04-21
Online published: 2017-01-11
Nowadays the theory of critical velocity of particles in cold spray has been already accepted generally. In the familiar semi-empirical formulas of the theory, only the properties and conditions of particles have been considered but there is no consideration of substrate. Yet most researches for effect of substrates' properties implied hardness of substrate was the most essential. However, little attention has been devoted to influence of other mechanical properties (e.g. Young's modulus and Poisson's ratio) and their cooperation on the deposition behavior. In order to study the effect systematically, 316L stainless steel particles were deposited by wipe test on six different substrates with a widely range of mechanical properties including Young's modulus, hardness and Poisson's ratio. They are pure Al, pure Cu, 7075T6 Al alloy, mild steel, Inconel625 and Ti6Al4V. The specimens have been investigated from morphology, cross-section and deposition efficiency. It is found that not only hardness but also Young's modulus and Poisson's ratio can affect deformation and deposition of bonded particles through playing a role in energy partition and bonding mechanism. In the case, the deformation of deposited particles is dependent on energy accepted by the particles, while the deposition efficiency is related to the bonding mechanism and energy accepted by substrate. According to the deformation level of the deposited particles, there are two kinds of substrate materials. On the one hand, bonding between particles with little deformation and their substrates is mainly dependent on mechanical interlock, in which both hardness and Young′s modulus of the substrates are lower than that of the particle. Then a parameter, Epara, has been calculated to predict the tendency of deposition efficiency for the situations. AZ91 alloy has been employed as substrate material in confirmatory experiment. Its result indicates that Epara is available for tendency prediction of the deposition efficiency of spherical-like deposited particle. On the other hand, the bonding mechanism of deposited particle with obviously flattening is more complex. In this situation, either hardness or Young′s modulus of the substrates is higher than that of the particle. The more area of fresh metal contacts on the interface, the higher deposition efficiency is.
Guanglu MA , Xinyu CUI , Yanfang SHEN , CINCA Nuria , M. GUILEMANY Josep , Tianying XIONG . INFLUENCE OF SUBSTRATE MECHANICAL PROPER-TIES ON DEPOSITION BEHAVIOUR OF 316L STAINLESS STEEL POWDER[J]. Acta Metall Sin, 2016 , 52(12) : 1610 -1618 . DOI: 10.11900/0412.1961.2016.00154
| [1] | Alkhimov A P, Kosarev V F, Papyrin A N.Soviet Phys-Doklady, 1990; 35: 1047 |
| [2] | Li W Y, Yu M.Surf Technol, 2010; 39(5): 95 |
| [2] | (李文亚, 余敏. 表面技术, 2010; 39(5): 95) |
| [3] | Tokarev A O.Met Sci Heat Treat, 1996; 38(3): 136 |
| [4] | Assadi H, G?rtner F, Stoltenhoff T, Kreye H.Acta Mater, 2003; 51: 4379 |
| [5] | Schmidt T, G?rtner F, Assadi H, Kreye H.Acta Mater, 2006; 54: 729 |
| [6] | Meng X M, Zhang J B, Liang Y L, Zhao J.Bao-Steel Technol, 2011; (5): 37 |
| [6] | (孟宪明, 张俊宝, 梁永立, 赵杰. 宝钢技术, 2011; (5): 37) |
| [7] | Wu X K, Zhang J S, Zhou X L, Cui H, Liu J C.Sci China Technol Sci, 2012; 55: 357 |
| [8] | Christoulis D K, Guetta S, Guipont V, Jeandin M.J Therm Spray Technol, 2011; 20: 523 |
| [9] | Marrocco T, McCartney D G, Shipway P H, Sturgeon A J.J Therm Spray Technol, 2006; 15: 263 |
| [10] | Bae G, Xiong Y, Kumar S, Kang K, Lee C.Acta Mater, 2008; 56: 4858 |
| [11] | Yin S, Suo X K, Su J Q, Guo Z W, Liao H L, Wang X F. J Therm Spray Technol, 2014; 23: 76 |
| [12] | Gao P H, Li C J, Yang G J, Li Y G, Li C X.Appl Surf Sci, 2010; 256: 2263 |
| [13] | Taguchi G.System of Experimental Design: Engineering Methods to Optimize Quality and Minimize Costs. New York: UNIPUB/Kraus International Publications, 1987: 1 |
| [14] | Taguchi G, Chowdhury S, Wu Y.Taguchi's Quality Engineering Handbook. New Jersey: Wiley-Interscience, 2004: 56 |
| [15] | King P C, Zahiri S H, Jahedi M.Acta Mater, 2008; 56: 5617 |
| [16] | Dykhuizen R C, Smith M F.J Therm Spray Technol, 1998; 7: 205 |
| [17] | Jodoin B, Raletz F, Vardelle M.Surf Coat Technol, 2006; 200: 4424 |
| [18] | Grujicic M, Zhao C L, Tong C, DeRosset W S, Helfritch D.Mater Sci Eng, 2004; A368: 222 |
| [19] | Ajdelsztajn L, Schoenung J M, Jodoin B, Kim G E.Metall Mater Trans, 2005; 36A: 657 |
| [20] | Jen T, Li L, Cui W, Chen Q, Zhang X.Int J Heat Mass Trans, 2005; 48: 4384 |
| [21] | Samareh B, Dolatabadi A. J Fluids Eng, 2008; 130: 081702 |
| [22] | Stolenhoff T, Kreye H, Ritchter H J.J Therm Spray Technol, 2002; 11: 542 |
| [23] | Samareh B, Stier O, Luther V, Dolatabadi A.J Therm Spray Technol, 2009; 18: 934 |
| [24] | Zhang D, Shipway P H, McCartney D G.China Surf Eng, 2008; 21(4): 1 |
| [24] | (Zhang D, Shipway P H, McCartney D G. 中国表面工程, 2008; 21(4): 1) |
| [25] | Schmidt T, Assadi H, G?rtner F, Richter H, Stoltenhoff T, Kreye H, Klassen T.J Therm Spray Technol, 2009; 18: 794 |
| [26] | Li W Y, Li C J, Wang Y Y, Yang G J.Acta Metall Sin, 2005; 41: 282 |
| [26] | (李文亚, 李长久, 王豫跃, 杨冠军. 金属学报, 2005; 41: 282) |
| [27] | Fukanuma H, Ohno N, Sun B, Huang R.Surf Coat Technol, 2006; 201: 1935 |
| [28] | Wu X K, Zhou X L, Wang J G, Zhang J S.Acta Metall Sin, 2010; 46: 385 |
| [28] | (巫湘坤, 周香林, 王建国, 张济山. 金属学报, 2010; 46: 385) |
| [29] | Xiang J Y, Song R B, Hou D P, Ren P D.Mater Sci Technol, 2011; 19(4): 128 |
| [29] | (项建英, 宋仁伯, 侯东坡, 任培东. 材料科学与工艺, 2011; 19(4): 128) |
| [30] | Ma G L, Kong L Y, Li T F, Cinca N, Guilemany J M, Xiong T Y. Rare Met Mater Eng#/magtechI#, 2016; accepted |
| [30] | (马广璐, 孔令艳, 李铁藩, Nuria Cinca, Josep M Guilemany, 熊天英. 稀有金属材料与工程, 2016; 录用) |
| [31] | Grujicic M, Zhao C L, DeRosset W S, Helfritch D.Mater Des, 2004; 25: 681 |
| [32] | McCune R C, Donlon W T, Popoola O O, Cartwright E L.J Therm Spray Technol, 2000; 9: 73 |
| [33] | Grujicic M, Saylora J R, Beasleya D E, De Rosset W S, Helfritch D.Appl Surf Sci, 2003; 219: 211 |
| [34] | Trompetter W J, Markwitz A, Hyland M, Munroe P.J Therm Spray Technol, 2005; 14: 524 |
| [35] | Li W Y, Zhang C, Guo X, Li C J, Liao H, Coddet C.Appl Surf Sci, 2007; 254: 517 |
| [36] | Bolesta A, Fomin V M, Sharafutdinov M R, Tolochko B P.Nucl Instrum Methods Phys Res, 2001; 470A: 249 |
| [37] | Johnson K L. Contact Mechanics.Cambridge: Cambridge University Press, 1985: 363 |
| [38] | Levin B F, Vecchio K S, Dupont J N, Marder A R.Metall Mater Trans, 1999; 30A: 1763 |
| [39] | Rahmati S, Ghaei A. J Therm Spray Technol, 2014; 23: 530 |
/
| 〈 |
|
〉 |