Orginal Article

STUDY ON ATOMIC-SCALE STRENGTHENING MECHANISM OF TRANSITION-METAL NITRIDE MNx (M=Ti, Zr, Hf) FILMS WITHIN WIDE COMPOSITION RANGES

  • Kechang HAN ,
  • Yiqi LIU ,
  • Guoqiang LIN ,
  • Chuang DONG ,
  • Kaiping TAI ,
  • Xin JIANG
Expand
  • 1 Key Laboratory for Material Modification by Laser, Ion and Electron Beams, Ministry of Education, Dalian University of Technology, Dalian 116024, China
    2 Institute of Metals Research, Chinese Academy of Sciences, Shenyang 110016, China

Received date: 2016-03-09

  Online published: 2017-01-11

Supported by

Supported by National Natural Science Foundation of China (No.51271047)

Abstract

Transition-metal nitrides have long attracted considerable attention among researchers and ubiquitous applications in various fields due to their renowned mechanical properties. However almost all the discussions of the strengthening mechanism were on conventional meso scale. For further understanding on the atomic scale strengthening mechanism of transition-metal nitrides, three groups of MNx (M=Ti, Zr, Hf) films with different nitrogen contents were synthesized on the Si substrates by magnetic filtering arc ion plating. The morphologies and thickness of the as-deposited films were characterized by FESEM, the microstructures and the residual stresses were characterized by XRD, the XPS and Nano Indenter were used to measure the chemical states and hardness (also the elastic modulus) of as-deposited films, respectively. The results show that all three groups MNx films perform the B1-NaCl single-phase structure within the large composition ranges. The preferred orientation, thickness, grain size and residual stress of the MNx films with different nitrogen contents were not changed so much. While the nanohardness and elastic modulus of MNx both first increased and then decreased with the rise of nitrogen content, and the peak values all existed when x near to 0.82. The strengthening mechanism was discussed and the decisive factor of composition dependent hardness enhancement was found from the atomic-scale chemical bonding states and electronic structure in this work, rather than the conventional meso-scale factors, such as preferred orientation, grain size and residual stress.

Cite this article

Kechang HAN , Yiqi LIU , Guoqiang LIN , Chuang DONG , Kaiping TAI , Xin JIANG . STUDY ON ATOMIC-SCALE STRENGTHENING MECHANISM OF TRANSITION-METAL NITRIDE MNx (M=Ti, Zr, Hf) FILMS WITHIN WIDE COMPOSITION RANGES[J]. Acta Metall Sin, 2016 , 52(12) : 1601 -1609 . DOI: 10.11900/0412.1961.2016.00078

References

[1] Toth L.Transition Metal Carbides and Nitrides. New York: Academic Press, 1971: 18
[2] Sundgren J E.Physics and Chemistry of Protective Coatings. New York: American Institute of Physics, 1986: 79
[3] Liu H X, Jiang Y H, Zhou R, Zhou R F, Jin Q L, Tang B Y.Acta Metall Sin, 2008; 44: 325
[3] (刘洪喜, 蒋业华, 周荣, 周荣锋, 金青林, 汤宝寅. 金属学报, 2008; 44: 325)
[4] Larijani M M, Tabrizi N, Norouzian S, Jafari A, Lahouti S, Haj Hosseini H, Afshari N.Vacuum, 2006; 81: 550
[5] Michael E O, Robert H P, Warren C O.Thin Solid Films, 1989; 181: 357
[6] Arnell R D, Colligon J S, Minnebaev K F, Yurasova V E.Vacuum, 1996; 47: 425
[7] Abdallah B, Naddaf M, A-Kharroub M.Nucl Inst Meth, 2013; 298B: 55
[8] Huang J, Ho C, Yu G.Mater Chem Phys, 2007; 102: 31
[9] Xu J H, Wang X, Ma S L, Liu Y, Xu K W.Chin J Mater Res, 2008; 22: 201
[9] (徐建华, 王昕, 马胜利, 刘阳, 徐可为. 材料研究学报, 2008; 22: 201)
[10] Jhi S, Ihm J, Louie S G, Cohen M L.Nature, 1999; 399: 132
[11] Shin C S, Gall D, Hellgren N, Patscheider J, Petrov I, Greene J E.J Appl Phys, 2003; 93: 6025
[12] Ma C H, Huang J H, Chen H.Thin Solid Films, 2002; 418: 73
[13] Huang M D, Lin G Q, Zhao Y H, Sun C, Wen L S, Dong C.Surf Coat Technol, 2003; 176: 109
[14] Lin G Q, Zhao Y H, Guo H M, Wang D Z, Dong C, Huang R, Wen L S.J Vac Sci Technol, 2004; 22A: 1218
[15] Schmid P E, Sato Sunaga M, Lévy F.J Vac Sci Technol, 1998; 16A: 2870
[16] Duan G F, Zhao G L, Wu L, Lin X X, Han G R.Appl Surf Sci, 2011; 257: 2428
[17] Tsetseris L, Kalfagiannis N, Logothetidis S, Pantelides S T.Phys Rev Lett, 2007; 99: 125503
[18] Mai Z H.X-Ray Characterization of Thin Film Structure. 2nd Ed., Beijing: Science Press, 2015: 80
[18] (麦振洪. 薄膜结构X射线表征.第2版, 北京: 科学出版社, 2015: 80)
[19] Whang K W, Seo Y W.J Vac Sci Technol, 1993; 11A: 1496
[20] Bertoti I, Mohai M, Sullivan J L, Saied S O.Appl Surf Sci, 1995; 84: 357
[21] Chan M H, Lu F H.Thin Solid Films, 2009; 517: 5006
[22] Jiang N, Zhang H J, Bao S N, Shen Y G, Zhou Z F.Physica, 2004; 352B: 118
[23] Ev I M, Strehbtow H H, Ek B N.Thin Solid Films, 1997; 303: 246
[24] Roman D, Bernardi J, Amorim C L G D, de Souza F S, Spinelli A, Giacomelli C, Figueroa C A, Baumvol I J R, Basso R L O.Mater Chem Phys, 2011; 130: 147
Outlines

/