Growth Mechanism and Photocatalytic Activity of NaNbO3 with Controllable Morphology
Received date: 2016-06-03
Online published: 2016-12-07
Supported by
Supported by National Natural Science Foundation of China (Nos.51272048 and 51172040) and Fundamental Research Funds for the Central Universities (No.N140108001)
Semiconductor photocatalysis for harvasting and utilizaing solar energy to solve worldwide environmental pollution and energy shortage is attracted flourishing interest. A complete understanding of structure-function relationships in well-defined model catalysts is essential to better understanding “real world” photocatalysis as well as rationally design photocatalysts. Well-defined NaNbO3 crystals are successful synthesized via facile hydrothermal method. Systematically characterzation is performed by XRD, Raman, SEM, BET specific surface area analyzer and DRUV-Vis. The results of XRD and Raman show that the as-prepared samples are pure orthorhombic NaNbO3 and NaNbO3 with different morphology possess various mainly exposed facets. On the basis of statistical SEM measurements, it presents that the shape evolution of NaNbO3 is shown to be dependent on the reaction time, from nanowires to a mixture of nanowires and microcubes, and finally to microcubes, and realized the morphology control systhesis of NaNbO3. The possible growth mechanism is proposed combined with previous study, highlighting the crucial role of P123. The photocatalytic performance of the as-prepared NaNbO3 crystals is assessed towards aqueous methyl bule under UV illumination, and compared with that of commercial NaNbO3 powders. DRUV-Vis evidenced that the absorption edge of NaNbO3 nanowires is blue shifted due to quantum size effect. The results show that the photoreactivity is morphology-dependent, with the BET specific surface area normalized reaction rate constants follow the order NaNbO3 nanowires> NaNbO3 microcubes > commercial NaNbO3. The exposed facets play a crucial role in determining the observed photocatalytic activity.
Key words: NaNbO3; photocatalysis; methyl blue; perovskite; P123
Tingting ZHANG , Yang QI , Gang LIU , Minghua LIU . Growth Mechanism and Photocatalytic Activity of NaNbO3 with Controllable Morphology[J]. Acta Metall Sin, 2017 , 53(3) : 376 -384 . DOI: 10.11900/0412.1961.2016.00216
| [1] | Chen C C, Ma W H, Zhao J C.Semiconductor-mediated photodegradation of pollutants under visible-light irradiation[J]. Chem. Soc. Rev., 2010, 39: 4206 |
| [2] | Ma Y, Wang X L, Jia Y S, et al.Titanium dioxide-based nanomaterials for photocatalytic fuel generations[J]. Chem. Rev., 2014, 114: 9987 |
| [3] | Shaham-Waldmann N, Paz Y.Away from TiO2: A critical minireview on the developing of new photocatalysts for degradation of contaminants in water[J]. Mater. Sci. Semicond. Process., 2016, 42: 72 |
| [4] | Jung J H, Lee M, Hong J I, et al.Lead-free NaNbO3 nanowires for a high output piezoelectric nanogenerator[J]. ACS Nano, 2011, 5: 10041 |
| [5] | Zeng W, Tao X-M, Chen S, et al.Highly durable all-fiber nanogenerator for mechanical energy harvesting[J]. Energy Environ. Sci., 2013, 6: 2631 |
| [6] | Dutto F, Raillon C, Schenk K, et al.Nonlinear optical response in single alkaline niobate nanowires[J]. Nano Lett., 2011, 11: 2517 |
| [7] | Yan C L, Nikolova L, Dadvand A, et al.Multiple NaNbO3/Nb2O5 heterostructure nanotubes: A new class of ferroelectric/semiconductor nanomaterials[J]. Adv. Mater., 2010, 22: 1741 |
| [8] | Grabowska E.Selected perovskite oxides: Characterization, preparation and photocatalytic properties——A review[J]. Appl. Catal., 2016, 186B: 97 |
| [9] | Shi H F, Wang T Z, Chen J, et al.Photoreduction of carbon dioxide over NaNbO3 nanostructured photocatalysts[J]. Catal. Lett., 2011, 141: 525 |
| [10] | Li G Q, Yi Z G, Bai Y, et al.Anisotropy in photocatalytic oxidization activity of NaNbO3 photocatalyst[J]. Dalton Trans., 2012, 41: 10194 |
| [11] | Li P, Ouyang S X, Xi G C, et al.The effects of crystal structure and electronic structure on photocatalytic H2 evolution and CO2 reduction over two phases of perovskite-structured NaNbO3[J]. J. Phys. Chem., 2012, 116C: 7621 |
| [12] | Shi H F, Lan B Y, Zhang C L, et al.Nitrogen doping concentration influence on NaNbO3 from first-principle calculations[J]. J. Phys. Chem. Solids, 2014, 75: 74 |
| [13] | Li G Q.Photocatalytic properties of NaNbO3 and Na0.6Ag0.4NbO3 synthesized by polymerized complex method[J]. Mater. Chem. Phys., 2010, 121: 42 |
| [14] | Zielińska B, Borowiak-Palen E, Kalenczuk R J.Preparation, characterization and photocatalytic activity of metal-loaded NaNbO3[J]. J. Phys. Chem. Solids, 2011, 72: 117 |
| [15] | Lv J, Kako T, Li Z S, et al.Synthesis and photocatalytic activities of NaNbO3 rods modified by In2O3 nanoparticles[J]. J. Phys. Chem., 2010, 114C: 6157 |
| [16] | Jiang L Q, Qiu Y, Yi Z G.Potassium niobate nanostructures: Controllable morphology, growth mechanism, and photocatalytic activity[J]. J. Mater. Chem., 2013, 1A: 2878 |
| [17] | Zhou X M, Lan J Y, Liu G, et al.Facet-mediated photodegradation of organic dye over hematite architectures by visible light[J]. Angew. Chem., Int. Ed., 2012, 51: 178 |
| [18] | Lei W Y, Zhang T T, Gu L, et al.Surface-structure sensitivity of CeO2 nanocrystals in photocatalysis and enhancing the reactivity with nanogold[J]. ACS Catal., 2015, 5: 4385 |
| [19] | Shi H F, Li X K, Wang D F, et al.NaNbO3 nanostructures: Facile synthesis, characterization, and their photocatalytic properties[J]. Catal. Lett., 2009, 132: 205 |
| [20] | Xiao Q, Jaatinen E, Zhu H Y.Direct photocatalysis for organic synthesis by using plasmonic-metal nanoparticles irradiated with visible light[J]. Chem. Asian J., 2014, 9: 3046 |
| [21] | Shiratori Y, Magrez A, Dornseiffer J, et al.Polymorphism in micro-, submicro-, and nanocrystalline NaNbO3[J]. J. Phys. Chem., 2005, 109B: 20122 |
| [22] | Rodriguez J A, Ramírez P J, Asara G G, et al.Charge polarization at a Au-TiC interface and the generation of highly active and selective catalysts for the low-temperature water-gas shift reaction[J]. Angew. Chem., Int. Ed., 2014, 53: 11270 |
| [23] | Zhu H Y, Zheng Z F, Gao X P, et al.Structural evolution in a hydrothermal reaction between Nb2O5 and NaOH solution: From Nb2O5 grains to microporous Na2Nb2O62/3H2O fibers and NaNbO3 cubes[J]. J. Am. Chem. Soc., 2006, 128: 2373 |
| [24] | Xu H W, Nyman M, Nenoff T M, et al.Prototype sandia octahedral molecular sieve (SOMS) Na2Nb2O6·H2O: Synthesis, structure and thermodynamic stability[J]. Chem. Mater., 2004, 16: 2034 |
| [25] | Shi H F, Chen G Q, Zhang C L, et al.Polymeric g-C3N4 coupled with NaNbO3 nanowires toward enhanced photocatalytic reduction of CO2 into renewable fuel[J]. ACS Catal., 2014, 4: 3637 |
| [26] | Bannat I, Wessels K, Oekermann T, et al.Improving the photocatalytic performance of mesoporous titania films by modification with gold nanostructures[J]. Chem. Mater., 2009, 21: 1645 |
| [27] | Turchi C S, Ollis D F.Photocatalytic degradation of organic water contaminants: Mechanisms involving hydroxyl radical attack[J]. J. Catal., 1990, 122: 178 |
| [28] | Qu Y Q, Duan X F.Progress, challenge and perspective of heterogeneous photocatalysts[J]. Chem. Soc. Rev., 2013, 42: 2568 |
/
| 〈 |
|
〉 |