Orginal Article

ADVANCES IN FRACTURE BEHAVIOR AND STRENGTH THEORY OF METALLIC GLASSES

  • Zhefeng ZHANG ,
  • Ruitao QU ,
  • Zengqian LIU
Expand
  • Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China

Received date: 2016-08-02

  Online published: 2016-11-25

Supported by

Supported by National Natural Science Foundation of China (Nos.51331007, 51301174 and 51501190)

Abstract

Owing to the unique amorphous structure, metallic glasses (MGs) exhibit quite distinctive deformation and fracture behaviors from the conventional crystalline materials. The high strength, brittleness and macroscopic homogenous and isotropic structural features make MGs ideal model materials for the investigations of the strength theory of high-strength materials. Hence the fracture behavior and strength theory of MGs have attracted very extensive interests of researchers from the fields of materials, mechanics and physics. This paper is based on the research works of the authors on the fracture and strength of MGs in the past decade, and concentrates on discussing the current knowledge and recent advances on the fracture behavior and strength theory of ductile and brittle MGs. Firstly, the fracture behaviors of ductile and brittle MGs including tension-compression strength asymmetry, fracture mechanism and ductile-to-brittle transition will be briefly elaborated. Then the strength theories of MGs will be discussed, with our emphasis on the foundation, validation, further development and application of the ellipse criterion. At last, some unsolved issues associated with the fracture and strength of MGs are proposed.

Cite this article

Zhefeng ZHANG , Ruitao QU , Zengqian LIU . ADVANCES IN FRACTURE BEHAVIOR AND STRENGTH THEORY OF METALLIC GLASSES[J]. Acta Metall Sin, 2016 , 52(10) : 1171 -1182 . DOI: 10.11900/0412.1961.2016.00348

References

[1] Ashby M F, Greer A L.Scr Mater, 2006; 54: 321
[2] Wang J, Li R, Hua N, Zhang T.J Mater Res, 2011; 26: 2072
[3] Sun B A, Pan M X, Zhao D Q, Wang W H, Xi X K, Sandor M T, Wu Y.Scr Mater, 2008; 59: 1159
[4] Qu R T, Liu Z Q, Wang R F, Zhang Z F.J Alloys Compd, 2015; 637: 44
[5] Liu Y H, Wang G, Wang R J, Zhao D Q, Pan M X, Wang W H.Science, 2007; 315: 1385
[6] Hofmann D C, Suh J Y, Wiest A, Duan G, Lind M L, Demetriou M D, Johnson W L.Nature, 2008; 451: 1085
[7] Demetriou M D, Launey M E, Garrett G, Schramm J P, Hofmann D C, Johnson W L, Ritchie R O.Nat Mater, 2011; 10: 123
[8] He Q, Cheng Y Q, Ma E, Xu J.Acta Mater, 2011; 59: 202
[9] Wu Y, Xiao Y, Chen G, Liu C T, Lu Z.Adv Mater, 2010; 22: 2770
[10] Liu Z Q, Liu G, Qu R T, Zhang Z F, Wu S J, Zhang T.Sci Rep, 2014; 4: 4167
[11] Ketov S V, Sun Y H, Nachum S, Lu Z, Checchi A, Beraldin A R, Bai H Y, Wang W H, Louzguine-Luzgin D V, Carpenter M A, Greer A L.Nature, 2015; 524: 200
[12] Zhang Y, Wang W H, Greer A L.Nat Mater, 2006; 5: 857
[13] Chu J P, Greene J E, Jang J S C, Huang J C, Shen Y L, Liaw P K, Yokoyama Y, Inoue A, Nieh T G.Acta Mater, 2012; 60: 3226
[14] Sarac B, Schroers J.Nat Commun, 2013; 4: 2158
[15] Qu R T, Zhang Q S, Zhang Z F.Scr Mater, 2013; 68: 845
[16] Qu R T, Zhao J X, Stoica M, Eckert J, Zhang Z F.Mater Sci Eng, 2012; A534: 365
[17] Nieh T G, Yang Y, Lu J, Liu C T.Prog Nat Sci Mater Int, 2012; 22: 355
[18] Sun B A, Wang W H.Prog Mater Sci, 2015; 74: 211
[19] Zhang Z F, Wu F F, He G, Eckert J.J Mater Sci Technol, 2007; 23: 747
[20] Schuh C A, Hufnagel T C, Ramamurty U.Acta Mater, 2007; 55: 4067
[21] Trexler M M, Thadhani N N.Prog Mater Sci, 2010; 55: 759
[22] Greer A L, Cheng Y Q, Ma E.Mater Sci Eng, 2013; R74: 71
[23] Qiao J, Jia H, Liaw P K.Mater Sci Eng, 2016; R100: 1
[24] Hufnagel T C, Schuh C A, Falk M L.Acta Mater, 2016; 109: 375
[25] Zhang Y, Greer A L.Appl Phys Lett, 2006; 89: 071907
[26] Guo H, Yan P F, Wang Y B, Tan J, Zhang Z F, Sui M L, Ma E.Nat Mater, 2007; 6: 735
[27] Spaepen F.Acta Metall, 1977; 25: 407
[28] Wang Z T, Pan J, Li Y, Schuh C A.Phys Rev Lett, 2013; 111: 135504
[29] Leamy H, Wang T, Chen H.Metall Mater Trans, 1972; 3B: 699
[30] Zhang Z F, Zhang H, Shen B L, Inoue A, Eckert J.Philos Mag Lett, 2006; 86: 643
[31] Lewandowski J J, Wang W H, Greer A L.Philos Mag Lett, 2005; 85: 77
[32] Xu J, Ramamurty U, Ma E.JOM, 2010; 62(4): 10
[33] Qu R T, Liu Z Q, Wang G, Zhang Z F.Acta Mater, 2015; 91: 19
[34] Qu R T, Eckert J, Zhang Z F.J Appl Phys, 2011; 109: 083544
[35] Xu J, Ma E.J Mater Res, 2014; 29: 1489
[36] Schroers J, Johnson W L.Phys Rev Lett, 2004; 93: 255506
[37] Zhang Z F, He G, Eckert J, Schultz L.Phys Rev Lett, 2003; 91: 045505
[38] Donovan P E.Acta Metall, 1989; 37: 445
[39] Zhang Z F, Eckert J, Schultz L.Acta Mater, 2003; 51: 1167
[40] Schuh C A, Lund A C.Nat Mater, 2003; 2: 449
[41] Liu Z Q, Qu R T, Zhang Z F.J Appl Phys, 2015; 117: 014901
[42] Li G, Jiang M Q, Jiang F, He L, Sun J.Mater Sci Eng, 2015; A625: 393
[43] Li G, Jiang M Q, Jiang F, He L, Sun J.Appl Phys Lett, 2013; 102: 171901
[44] Qu R T, Stoica M, Eckert J, Zhang Z F.J Appl Phys, 2010; 108: 063509
[45] Pampillo C A.J Mater Sci, 1975; 10: 1194
[46] Spaepen F.Acta Metall, 1975; 23: 615
[47] Argon A S, Salama M.Mater Sci Eng, 1976; 23: 219
[48] Deibler L A, Lewandowski J J.Mater Sci Eng, 2012; A538: 259
[49] Qu R T, Zhang Z F.J Appl Phys, 2013; 114: 193504
[50] Hull D.Fractography: Observing, Measuring and Interpreting Fracture Surface Topography. Cambridge: Cambridge University Press, 1999: 1
[51] Zhao Y Y, Zhang G, Estévez D, Chang C, Wang X, Li R W.JAlloys Compd, 2015; 621: 238
[52] Maa? R, Birckigt P, Borchers C, Samwer K, Volkert C A.Acta Mater, 2015; 98: 94
[53] Sun B A, Yang Y, Wang W H, Liu C T.Sci Rep, 2016; 6: 21388
[54] Wu Y, Li H X, Liu Z Y, Chen G L, Lu Z P.Intermetallics, 2010; 18: 157
[55] Qu R T, Calin M, Eckert J, Zhang Z F.Scr Mater, 2012; 66: 733
[56] Qu R T, Zhang P, Zhang Z F.J Mater Sci Technol, 2014; 30: 599
[57] Sha Z D, Pei Q X, Sorkin V, Branicio P S, Zhang Y W, Gao H.Appl Phys Lett, 2013; 103: 081903
[58] Lei X, Li C, Shi X, Xu X, Wei Y.Sci Rep, 2015; 5: 10537
[59] Yao J H, Wang J Q, Lu L, Li Y.Appl Phys Lett, 2008; 92: 041905
[60] Zhao Y Y, Ma E, Xu J.Scr Mater, 2008; 58: 496
[61] Zheng X L, Wang H, Zheng M S, Wang F H.Notch Strength and Notch Sensitivity of Materials. Beijing: Science Press, 2008: 1
[62] Murali P, Ramamurty U.Acta Mater, 2005; 53: 1467
[63] Kumar G, Rector D, Conner R D, Schroers J.Acta Mater, 2009; 57: 3572
[64] Jiang F, Jiang M Q, Wang H F, Zhao Y L, He L, Sun J.Acta Mater, 2011; 59: 2057
[65] Ketkaew J, Liu Z, Chen W, Schroers J.Phys Rev Lett, 2015; 115: 265502
[66] Han Z H, He L, Hou Y L, Feng J, Sun J.Intermetallics, 2009; 17: 553
[67] Madge S V, Wada T, Louzguine-Luzgin D V, Greer A L, Inoue A.Scr Mater, 2009; 61: 540
[68] Zhang Z F, Wu F F, Gao W, Tan J, Wang Z G, Stoica M, Das J, Eckert J, Shen B L, Inoue A.Appl Phys Lett, 2006; 89: 251917
[69] Xi X K, Zhao D Q, Pan M X, Wang W H, Wu Y, Lewandowski J J.Phys Rev Lett, 2005; 94: 125510
[70] Wang G, Zhao D Q, Bai H Y, Pan M X, Xia A L, Han B S, Xi X K, Wu Y, Wang W H.Phys Rev Lett, 2007; 98: 235501
[71] Shen J, Liang W Z, Sun J F.Appl Phys Lett, 2006; 89: 121908
[72] Meng J X, Ling Z, Jiang M Q, Zhang H S, Dai L H.Appl Phys Lett, 2008; 92: 171909
[73] Jiang M Q, Ling Z, Meng J X, Dai L H.Philos Mag, 2008; 88: 407
[74] Zhao J X, Qu R T, Wu F F, Zhang Z F, Shen B L, Stoica M, Eckert J.J Appl Phys, 2009; 105: 103519
[75] Xia X X, Wang W H.Small, 2012; 8: 1197
[76] Jiang M Q, Meng J X, Gao J B, Wang X L, Rouxel T, Keryvin V, Ling Z, Dai L H.Intermetallics, 2010; 18: 2468
[77] Gao M, Sun B A, Yuan C C, Ma J, Wang W H.Acta Mater, 2012; 60: 6952
[78] Murali P, Guo T F, Zhang Y W, Narasimhan R, Li Y, Gao H J.Phys Rev Lett, 2011; 107: 215501
[79] Singh I, Narasimhan R, Ramamurty U.Phys Rev Lett, 2016; 117: 044302
[80] Liu Z Q, Wang W H, Jiang M Q, Zhang Z F.Philos Mag Lett, 2014; 94: 658
[81] Cheng Y Q, Ma E.Prog Mater Sci, 2011; 56: 379
[82] Madge S V, Louzguine-Luzgin D V, Lewandowski J J, Greer A L.Acta Mater, 2012; 60: 4800
[83] Yuan Z W, Li F G, Wang R T, Wang C P, Li J, Xue F M.Theor Appl Fract Mech, 2014; 74: 96
[84] Johnson W L, Samwer K.Phys Rev Lett, 2005; 95: 195501
[85] Pan J, Chen Q, Liu L, Li Y.Acta Mater, 2011; 59: 5146
[86] Paul B.In: Liebowitz H ed., Fracture, An Advanced Treatise. Vol.II, New York: Academic Press, 1968: 313
[87] Lund A C, Schuh C A.Acta Mater, 2003; 51: 5399
[88] Yu M H.Appl Mech Rev, 2002; 55: 169
[89] Zhang Z F, Eckert J.Phys Rev Lett, 2005; 94: 094301
[90] Chen Y, Jiang M Q, Wei Y J, Dai L H.Philos Mag, 2011; 91: 4536
[91] Coulomb C.Memoires de Mathematique et de Physique, Presentes al' Academie, Royale des Sciences par Divers Savans, et Lus dans ses Assemblees, 1773; 7: 343
[92] Davis L A, Kavesh S.J Mater Sci, 1975; 10: 453
[93] Anand L, Su C.J Mech Phys Solids, 2005; 53: 1362
[94] Lei X, Wei Y, Wei B, Wang W H.Acta Mater, 2015; 99: 206
[95] Qu R T, Zhang Z F.Sci Rep, 2013; 3: 1117
[96] Wu F F, Zhang Z F, Mao S X, Peker A, Eckert J.Phys Rev, 2007; 75B: 134201
[97] Packard C E, Schuh C A.Acta Mater, 2007; 55: 5348
[98] Qu R T, Zhang Z J, Zhang P, Liu Z Q, Zhang Z F.Sci Rep, 2016; 6: 23359
[99] Zhang P, Li S X, Zhang Z F.Mater Sci Eng, 2011; A529: 62
[100] Wang Z, Qu R T, Scudino S, Sun B A, Prashanth K G, Louzguine-Luzgin D V, Chen M W, Zhang Z F, Eckert J.NPG Asia Mater, 2015; 7: e229
[101] Wang W H, Wang R J, Li F Y, Zhao D Q, Pan M X.Appl Phys Lett, 1999; 74: 1803
[102] Wang W H.J Appl Phys, 2006; 99: 093506
[103] Wang W H.Prog Mater Sci, 2012; 57: 487
[104] Liu Z Q, Wang R F, Qu R T, Wang W H, Zhang Z F.J Appl Phys, 2014; 115: 203513
[105] Liu Z Q, Zhang Z F.J Appl Phys, 2014; 115: 163505
[106] Liu Z Q, Zhang Z F.Appl Phys Lett, 2013; 103: 181909
[107] Liu Z Q, Zhang Z F.J Appl Phys, 2013; 114: 243519
[108] Chen H S, Wang T T.J Appl Phys, 1970; 41: 5338
Outlines

/