Orginal Article

DIELECTRIC BARRIER DISCHARGE PLASMA ASSISTED BALL MILLING TECHNOLOGY AND ITS APPLICATIONS IN MATERIALS FABRICATION

  • Min ZHU ,
  • Zhongchen LU ,
  • Renzong HU ,
  • Liuzhang OUYANG
Expand
  • 1 School of Materials Science and Engineering, South China University of Technology, Guangzhou 510640, China
    2 Key Laboratory of Advanced Energy Storage Materials of Guangdong Province, South China University of Technology, Guangzhou 510640, China
    3 School of Mechanical and Automotive Engineering, South China University of Technology, Guangzhou 510640, China

Received date: 2016-08-03

  Online published: 2016-08-30

Supported by

Supported by National Natural Science Foundation of China (No.51231003), National Basic Research Program of China (No.2010CB631300), Science Fund for Creative Research Groups of the National Natural Science Foundation of China (No.NSFC51621001), Natural Science Foundation of Guangdong Province (No.05200618) and Guangdong Provincial Laboratory System Construction Project (No.2012A061400002)

Abstract

The development of external field assisted milling technologies and their application in materials fabrication have been briefly described. A recent developed milling method named as dielectric barrier discharge plasma assisted ball milling (DBDP-milling) was introduced. A combination of heating effect and high energy electron bombardment effect produced by plasma, as well as the milling mechanical effect was induced simultaneously in the DBDP-milling, which can effectively promote the powder refinement, activation and chemical reaction. On this basis, the DBDP-milling method was applied in the fabrication of cemented carbide, anode materials for lithium ion batteries, hydrogen storage materials, and so on. The studies have indicated that DBDP-milling could improve the efficiency of mill, produce unique structure and thus enhanced properties. In addition, DBDP-milling is also possible to establish a new material production process. Research results have demonstrated that the DBDP-milling method has a great potential in refinement, surface modification, mechanical alloying, composite fabrication and gas-solid reaction of powder materials for different applications.

Cite this article

Min ZHU , Zhongchen LU , Renzong HU , Liuzhang OUYANG . DIELECTRIC BARRIER DISCHARGE PLASMA ASSISTED BALL MILLING TECHNOLOGY AND ITS APPLICATIONS IN MATERIALS FABRICATION[J]. Acta Metall Sin, 2016 , 52(10) : 1239 -1248 . DOI: 10.11900/0412.1961.2016.00360

References

[1] Benjamin J S.Metall Trans, 1970; 1: 2943
[2] Koch C C.Nanostruct Mater, 1993; 2: 109
[3] Dai L Y, Chen Q L, Lin S F, Ouyang L Z.Mater Rev, 2009; 23(2): 59
[3] (戴乐阳, 陈清林, 林少芬, 欧阳柳章. 材料导报, 2009; 23(2): 59)
[4] Dai L Y, Zeng M Q, Tong Y Q, Ouyang L Z, Zhu M, Li Y Y.J Funct Mater, 2005; 36: 1158
[4] (戴乐阳, 曾美琴, 童燕青, 欧阳柳章, 朱敏, 李元元. 功能材料, 2005; 36: 1158)
[5] Mordyuk B N, Prokopenko G I.Ultrasonics, 2004; 42: 43
[6] Calka A, Radlinski A P.Mater Sci Eng, 1991; A134: 1350
[7] Wang D P, Li X D, Chang Y, Qi M.J Rare Earth (Engl Lett), 2013; 31: 366
[8] Chelvane J A, Palit M, Basumatary H, Pandian S.J Magn Magn Mater, 2013; 343: 144
[9] Luton M J, Jayanth C S, Disko M M, Matrasa1 S, Vallon J. In: Kear B H, McCandlish L E, Polk D E, Siegel R W eds., MRS Proceedings, Cambridge University Press, 1988; 132: 79
[10] Chung K H, He J H, Shin D H.Mater Sci Eng, 2003; A356: 23
[11] Calka A, Wexler D.Nature, 2002; 419: 147
[12] Calka A, Wexler D.J Metastable Nanocryst Mater, 2004; 20: 111
[13] Mosbah A, Calka A, Wexler D.J Alloys Compd, 2006; 424: 279
[14] Varin R A, Chiu C, Li S, Calka A, Wexler D.J Alloys Compd, 2004; 370: 230
[15] Calka A, Mosbah A, Stanford N, Balaz P.J Alloys Compd, 2008; 455: 285
[16] Needham S A, Calka A, Wang G X, Mosbah A, Liu H K.Electochem Commun, 2006; 8: 434
[17] Yuan Q, Zheng Y, Yu H.Int J Refract Met Hard Mater, 2009; 27: 121
[18] Quan Y, Zheng Y, Yu H Z.Trans Nonferrous Met Soc China, 2011; 21: 1545
[19] Zhu M, Dai L Y, Cao B, Zeng M Q, Ouyang L Z, Tong Y Q, Li B.China Patent, ZL200510036231, 2007)
[19] (朱敏, 戴乐阳, 曹彪, 曾美琴, 欧阳柳章, 童燕青, 李北. 中国专利, ZL200510036231, 2007)
[20] Wang X X.High Volt Eng, 2009; 35(1): 1
[20] (王新新. 高电压技术, 2009; 35(1): 1)
[21] Yang X P, Dai L Y, Zeng M Q, Ouyang L Z.Mater Rev, 2010; 24: 320
[21] (杨小平, 戴乐阳, 曾美琴, 欧阳柳章. 材料导报, 2010; 24: 320)
[22] Sun Q D.Master Thesis, Tianjin University, 2013
[22] (孙启迪. 天津大学硕士学位论文, 2013)
[23] Dai L Y, Lin S F, Chen Q L, Yang X P.Mod Manuf Eng, 2010; 5(5): 48
[23] (戴乐阳, 林少芬, 陈清林, 杨小平. 现代制造工程, 2010; 5(5): 48)
[24] Dai L Y.PhD Dissertation, South China University of Technology, Guangzhou, 2006
[24] (戴乐阳, 华南理工大学博士学位论文, 广州, 2006)
[25] Zhu M, Dai L Y, Gu N S, Cao B, Ouyang L Z.J Alloys Compd, 2009; 478: 624
[26] Dai L Y.Acta Metall Sin (Engl Lett), 2013; 26: 63
[27] Dai L Y, Cao B, Zhu M.Acta Metall Sin (Engl Lett), 2006; 19: 411
[28] Conrad H, Yang D.Acta Mater, 2002; 50: 2851
[29] Chen Z H.Master Thesis, South China University of Technology, Guangzhou, 2015
[29] (陈志鸿. 华南理工大学硕士学位论文, 广州, 2015)
[30] Jia C X, Chen P, Wang Q, Wang J, Ren R.Chin J Mater Res, 2015; 29: 10
[30] (贾彩霞, 陈平, 王乾, 王静, 任荣. 材料研究学报, 2015; 29: 10)
[31] Meng R G.Master Thesis, Jimei University, Xiamen, 2013
[31] (孟荣刚. 集美大学硕士学位论文, 厦门, 2013)
[32] Yang X P.Master Thesis, South China University of Technology, Guangzhou, 2010
[32] (杨小平. 华南理工大学硕士学位论文, 广州, 2010)
[33] Dai L Y, Lin S F, Chen J F, Zeng M Q, Zhu M.Int J Refract Met Hard Mater, 2012; 30: 48
[34] Zhu M, Bao X Y, Yang X P, Gu N S, Wang H, Zeng M Q, Dai L Y.Metall Mater Trans, 2011; 42: 2930
[35] Wang W, Lu Z C, Chen Z H, Zeng M Q, Wang H, Zhu M.J Rare Earth (Engl Lett), DOI: 10.1007/S12598-016-0769-5
[36] Hu R Z, Yang L C, Zhu M.Chin Sci Bull (Chin Ver), 2013; 58: 3140
[36] (胡仁宗, 杨黎春, 朱敏. 科学通报(中文版), 2013; 58: 3140)
[37] Hu R Z.PhD Dissertation, South China University of Technology, Guangzhou, 2011
[37] (胡仁宗. 华南理工大学博士学位论文, 广州, 2011)
[38] Liu H, Hu R, Zeng M, Liu J W, Zhu M.J Mater Chem, 2012; 22A: 8022
[39] Hui L, Hu R Z, Sun W, Zeng M Q, Yang L C, Liu J W, Zhu M,J Power Sources, 2013; 242: 114
[40] Zhang H Y, Hu R Z, Liu H, Sun W, Lu Z C, Liu J W, Yang L C, Zhang Y, Zhu M.J Mater Chem, 2016; 4A: 10321
[41] W. Sun, R.Z.Hu, H. Liu, M. Q. Zeng, M. Zhu.J Power Sources, 2014; 268:610
[42] Ouyang L Z, Guo L N, Cai W H, Ye J S, Hu R Z, Liu J W, Yang LC, Zhu M.J Mater Chem A, 2014; 2A: 11280
[43] Wang Y K, Yang L C, Hu R Z, Sun W, Liu J W, Ouyang L Z, Yuan B, Wang H, Zhu M.J Power Sources, 2015; 288: 314
[44] Zaluska A, Zaluski L, Str?m-Olsen J O.J Alloys Compd, 1999; 288: 217
[45] Huot J, Tremblay M L, Schulz R.J Alloys Compd, 2003; 356: 603
[46] Lu Y S, Zhu M, Wang H, Li Z M, Ouyang L Z, Liu J W.Int J Hydrogen Energy, 2014; 39: 14033
[47] Ouyang L Z, Cao Z J, Wang H, Liu J W, Sun D L, Zhang Q A, Zhu M.J Alloys Compd, 2014; 586: 113
[48] Cao Z J, Ouyang L Z, Wu Y, Wang H, Liu J W, Fang F, Sun D L, Zhang Q A, Zhu M.Dual-tuning effects of In, Al, and Ti on the thermodynamics and kinetics of Mg85In5Al5Ti5 alloy synthesized by plasma milling.J Alloys Compd, 2015; 623: 354
[49] Ouyang L Z, Cao Z J, Li L L, Wang H, Liu J W, Min D, Chen Y W, Xiao F M, Tang R H, Zhu M.Int J Hydrogen Energy, 2014; 39: 12765
[50] Dai L Y, Zhang B J, Lin S F, Liu Z J, Wang W C.Chin J Nonferrous Met, 2015; 1: 171
[50] (戴乐阳, 张宝剑, 林少芬, 刘志杰, 王文春. 中国有色金属学报, 2015; 1: 171)
Outlines

/