SIZE EFFECTS ON THE DEFORMATION AND DAMAGEOF Cu-BASED METALLIC NANOLAYEREDMICRO-PILLARS
Received date: 2016-07-19
Online published: 2016-08-25
Supported by
Supported by National Basic Research Program of China (No.2010CB631003), National Natural Science Foundation of China (Nos.51571157, 51321003, 51322104 and 51201123), Program of Introducing Talents of Discipline to Universities of China (No.B06025) and Natural Science Basic Research Plan in Shaanxi Province of China (No.2015JM5158)
The nanostructured metallic multilayers (NMMs) are widely used as essential components of high performance microelectronics and interconnect structures. The deformation and damage of NMMs is the essential factor leading to the structural failure of these systems. In this paper, based on these experimental results achieved by the authors, as well as the state-of-the-art and progress at home and abroad in the plastic deformation behavior of micropillars of Cu-based NMMs, the correlation of microstructure-size constraint-mechanical performance in the Cu-based nanolayered micropillars is illustrated. The universality of their deformation modes and internal damage mechanisms are revealed, and the work hardening /softening behaviors of two types of nanolaminates, including crystalline/crystalline and crystalline/amorphous NMMs, are summarized. Finally, a brief prospect on the studies of NMMs in future is suggested.
Jun SUN , Jinyu ZHANG , Kai WU , Gang LIU . SIZE EFFECTS ON THE DEFORMATION AND DAMAGEOF Cu-BASED METALLIC NANOLAYEREDMICRO-PILLARS[J]. Acta Metall Sin, 2016 , 52(10) : 1249 -1258 . DOI: 10.11900/0412.1961.2016.00315
| [1] | Was G S, Foecke T.Thin Solid Films, 1996; 286: 1 |
| [2] | Li Y P, Zhang G P.Acta Mater, 2010; 58: 3877 |
| [3] | Zhang J Y, Zhang X, Wang R H, Lei S Y, Zhang P, Niu J J, Liu G, Zhang G J, Sun J.Acta Mater, 2011; 59: 7368 |
| [4] | Romig Jr A D, Dugger M T, McWhorter P J.Acta Mater, 2003; 51: 5837 |
| [5] | Fullwood D T, Niezgoda S R, Adams B L, Kalidindi S R.Prog Mater Sci, 2010; 55: 477 |
| [6] | Beyerlein I J, Demkowicz M J, Misra A, Uberuaga B P.Prog Mater Sci, 2015; 74: 125 |
| [7] | Greer J R, de Hosson J T M.Prog Mater Sci, 2011; 56: 654 |
| [8] | Zhu T, Li J.Prog Mater Sci, 2010; 55: 710 |
| [9] | Uchic M D, Shade P A, Dimiduk D M.Annu Rev Mater Res, 2009; 39: 361 |
| [10] | Nan C W.Heterogeneous Materials Physics: Microstructure and Performance. Beijing: Science Press, 2005: 1 |
| [10] | (南策文. 非均质材料物理-显微结构-性能关联. 北京: 科学出版社, 2005: 1) |
| [11] | Cammarata R C.Prog Surf Sci, 1994; 46: 1 |
| [12] | Hoagland R G, Kurtz R J, Henager C H.Scr Mater, 2004; 50: 775 |
| [13] | Hoagland R G, Mitchell T E, Hirth J P, Kung H.Phil Mag, 2002; 82: 643 |
| [14] | Wang J, Hoagland R G, Hirth J P, Misra A.Acta Mater, 2008; 56: 5685 |
| [15] | Wang J, Misra A, Hoagland R G, Hirth J P.Acta Mater, 2012; 60: 1503 |
| [16] | Wang Y M, Li J, Hamza A V, Barbee J T W.Proc Natl Acad Sci USA, 2007; 104: 11155 |
| [17] | Zhang J Y, Zhang X, Liu G, Zhang G J, Sun J.Scr Mater, 2010; 63: 101 |
| [18] | Zhang J Y, Niu J J, Zhang X, Zhang P, Liu G, Zhang G J, Sun J.Mater Sci Eng, 2012; A543: 139 |
| [19] | Zhang J Y, Zhang P, Zhang X, Wang R H, Liu G, Zhang G J, Sun J.Mater Sci Eng, 2012; A545: 118 |
| [20] | Zhang J Y, Liu Y, Chen J, Chen Y, Liu G, Zhang X, Sun J.Mater Sci Eng, 2012; A552: 392 |
| [21] | Wu K, Zhang J Y, Liu G, Zhang P, Cheng P M, Zhang G J, Sun J.Acta Mater, 2013; 61: 7889 |
| [22] | Wu K, Zhang J Y, Zhang P, Wang Y Q, Liu G, Zhang G J, Sun J.Mater Sci Eng, 2014; A613: 130 |
| [23] | Wu K, Zhang J Y, Li J, Wang Y Q, Liu G, Sun J.Acta Mater, 2015; 100: 344 |
| [24] | Li Y P, Zhang G P, Wang W, Tan J, Zhu S J.Scr Mater, 2007; 57: 117 |
| [25] | Li Y P, Zhu X F, Tan J, Wu B, Wang W, Zhang G P.J Mater Res, 2009; 24: 728 |
| [26] | Wen S P, Zong R L, Zeng F, Gao Y, Pan F.Acta Mater, 2007; 55: 345 |
| [27] | Zhu X Y, Liu X J, Zong R L, Zeng F, Pan F.Mater Sci Eng, 2010; A527: 1243 |
| [28] | Liu Y, Bufford D, Wang H, Sun C, Zhang X.Acta Mater, 2011; 59: 1924 |
| [29] | Liu Y, Bufford D, Rios S, Wang H, Chen J, Zhang J Y, Zhang X.J Appl Phys, 2012; 111: 073526 |
| [30] | Lai W S, Yang M J.Appl Phys Lett, 2007; 90: 181917 |
| [31] | Zhang J Y, Liu G, Zhang X, Zhang G J, Sun J, Ma E.Scr Mater, 2010; 62: 333 |
| [32] | Wang Y Q, Zhang J Y, Liang X Q, Wu K, Liu G, Sun J.Acta Mater, 2015; 95: 132 |
| [33] | Zhang J Y, Liu G, Sun J.Mater China, 2016; 35: 31 |
| [33] | (张金钰, 刘刚, 孙军. 中国材料进展, 2016; 35: 31) |
| [34] | Mara N A, Bhattacharyya D, Dickerson P, Hoagland R G, Misra A.Appl Phys Lett, 2008; 92: 231903 |
| [35] | Mara N A, Bhattacharyya D, Hirth J P, Dickerson P, Misra A.Appl Phys Lett, 2010; 97: 021909 |
| [36] | Zhang J Y, Lei S Y, Liu Y, Niu J J, Chen Y, Liu G, Zhang X, Sun J.Acta Mater, 2012; 60: 1610 |
| [37] | Zhang J Y, Liu G, Lei S Y, Niu J J, Sun J.Acta Mater, 2012; 60: 4054 |
| [38] | Zhang J Y, Li J, Liang X Q, Liu G, Sun J.Sci Rep, 2014; 4: 4205 |
| [39] | Zhang J Y, Zhang X, Wang R H, Lei S Y, Zhang P, Niu J J, Liu G, Zhang G J, Sun J.Acta Mater, 2012; 60: 7183 |
| [40] | Zhang J Y, Liu G, Sun J.Sci Rep, 2013; 3: 2324 |
| [41] | Kim Y B, Budiman A S, Baldwin J K, Mara N A, Misra A.J Mater Res, 2012; 27: 592 |
| [42] | Han S M, Phillips M A, Nix W D.Acta Mater, 2009; 57: 4473 |
| [43] | Wang J, Yang C, Hodgson P D.Scr Mater, 2013; 69: 626 |
| [44] | Zhang J Y, Cui J C, Liu G, Sun J.Scr Mater, 2013; 68: 639 |
| [45] | Zhang J Y, Liang X Q, Zhang P, Wu K, Liu G, Sun J.Acta Mater, 2014; 66: 302 |
| [46] | Dayal P, Quadir M Z, Kong C, Savvides N, Hoffman M.Thin Solid Films, 2011; 519: 3213 |
| [47] | Wei Q.J Mater Sci, 2007; 42: 1709 |
| [48] | Zhang J Y, Liu G, Sun J.Int J Plast, 2013; 50: 1 |
| [49] | Zhang J Y, Liu G, Sun J.Acta Mater, 2013; 61: 6868 |
| [50] | Zhang J Y, Wang Y Q, Wu K, Zhang P, Liu G, Zhang G J, Sun J.Mater Sci Eng, 2014; A612: 28 |
| [51] | Niu J J, Zhang J Y, Liu G, Zhang P, Lei S Y, Zhang G J, Sun J.Acta Mater, 2012; 60: 3677 |
| [52] | Zhang J Y, Wang Y Q, Liu G, Sun J.Appl Surf Sci, 2014; 321: 19 |
| [53] | Carlton C E, Ferreira P J.Acta Mater, 2007; 55: 3749 |
| [54] | Kocks U F, Mecking H.Prog Mater Sci, 2003; 48: 171 |
| [55] | Misra A, Zhang X, Hammon D, Hoagland R G.Acta Mater, 2005; 53: 221 |
| [56] | Yan J W, Zhu X F, Yang B, Zhang G P.Phys Rev Lett, 2013; 110: 155502 |
| [57] | Gruber P A, B?hm J, Onuseit F, Wanner A, Spolenak R, Arzt E.Acta Mater, 2008; 56: 2318 |
| [58] | Lei S Y, Zhang J Y, Niu J J, Liu G, Zhang X, Sun J.Scr Mater, 2012; 66: 706 |
| [59] | Lu L, Chen X, Huang X, Lu K.Science, 2009; 323: 607 |
| [60] | Bhattacharyya D, Mara N A, Dickerson P, Hoagland R G, Misra A.Acta Mater, 2011; 59: 3804 |
| [61] | Huang X, Hansen N, Tsuji N.Science, 2006; 312: 249 |
| [62] | Knorr I, Cordero N M, Lilleodden E T, Volkert C A.Acta Mater, 2013; 61: 4984 |
| [63] | Li N, Mara N A, Wang Y Q, Nastasi M, Misra A.Scr Mater, 2011; 64: 974 |
| [64] | Anderson P M, Foecke T, Hazzledine P M.Mater Res Soc Bull, 1999; 24: 27 |
| [65] | Misra A, Verdier M, Kung H, Embury J D, Hirth J P.Scr Mater, 1999; 41: 973 |
| [66] | Zhu X F, Li Y P, Zhang G P, Tan J, Liu Y.Appl Phys Lett, 2008; 92: 161905 |
| [67] | Zhang J, Zhang J Y, Liu G, Zhao Y, Sun J.Thin Solid Films, 2009; 517: 2936 |
| [68] | Donohue A, Spaepen F, Hoagland R G, Misra A.Appl Phys Lett, 2007; 91: 241905 |
| [69] | Chen C Q, Pei Y T, De Hosson J T M.Acta Mater, 2010; 58: 189 |
| [70] | Zhang J Y, Liu G, Sun J.Acta Mater, 2014; 66: 22 |
| [71] | Kim J Y, Jang D C, Greer J R.Adv Funct Mater, 2011; 21: 4550 |
| [72] | Kuzmin O V, Pei Y T, Chen C Q, De Hosson J T M.Acta Mater, 2012; 60: 889 |
| [73] | Jang D, Greer J R.Nat Mater, 2010; 9: 215 |
| [74] | Kiener D, Minor A M.Acta Mater, 2011; 59: 1328 |
| [75] | Beyerlein I J, Caro A, Demkowicz M J, Mara N A, Misra A, Uberuaga B P.Mater Today, 2013; 16: 443 |
| [76] | Yu K Y, Liu Y, Fu E G, Wang Y Q, Myers M T, Wang H, Shao L, Zhang X.J Nucl Mater, 2013; 440: 310 |
| [77] | Zhang P, Zhang J Y, Li J, Liu G, Wu K, Wang Y Q, Sun J.Acta Mater, 2014; 76: 221 |
| [78] | Zhang P, Zhang J Y, Li J, Liu G, Wu K, Wang Y Q, Sun J.J Mater Sci, 2015; 50: 1901 |
| [79] | Wang Y Q, Hou Z Q, Zhang J Y, Liang X Q, Liu G, Zhang G J, Sun J.Acta Metall Sin (Engl Lett), 2016; 29: 156 |
| [80] | Zhang J Y, Wang Y Q, Liang X Q, Zeng F L, Liu G, Sun J.Acta Mater, 2015; 92: 140 |
| [81] | Liang X Q, Zhang J Y, Wang Y Q, Wu S H, Zeng F L, Wu K, Liu G, Zhang G J, Sun J.Mater Sci Eng, 2016; A672: 153 |
/
| 〈 |
|
〉 |