EFFECT OF HYBRID SURFACE NANOCRYSTALLI-ZATION ON THE ELECTROCHEMICAL CORROSION BEHAVIOR IN 2A14 ALUMINUM ALLOY
Received date: 2016-03-23
Online published: 2016-08-17
Supported by
Supported by National Natural Science Foundation of China (No.51275517) and Special Project of Xi'an University of Technology (No.2014TS002)
In recent years, the surface nanocrystallization (SNC) technology has received extensive attentions in the field of metal material. The shot peening and surface mechanical rolling processing technology can form the gradient nanostructured (GNS) layer on the surface of metal. The material surface roughness is large generally. Therefore, the problem how to form the thick, smooth, flawless GNS layer is need to solve urgently. By means of the hybrid surface nanocrystallization (HSNC) method of both supersonic fine particles bombarding (SFPB) and surface mechanical rolling treatment (SMRT), a gradient nanostructured surface layer was formed on 2A14 aluminum alloy plate. The electrochemical corrosion behavior of the HSNC sample at the air of room temperature and low temperature liquid nitrogen was compared with that of the original sample in aqueous solution of 3.5%NaCl. The results showed that grain size increases from about 30 nm at the surface layer gradually to coarse grain size of the matrix when the sample was processed by HSNC. The total thickness of the plastic deformation layer is about 130 μm. The surface roughness Ra is about 0.6 μm with the surface microcrack disappeared. Compared to the original sample, the pitting corrosion resistance of the SFPB samples was not improved and the pitting corrosion resistance of the HSNC samples was improved. The self-corrosion potential and pitting corrosion potential increase respectively from -1.01228 and -0.29666 V in the original sample to -0.67445 and 0.026760 V at the air room temperature of the HSNC sample. The pitting corrosion resistance of the HSNC sample at the air of room temperature was the biggest. The analysis showed that the surface GNS grain, significant increase of the nanocrystal boundaries, the introduction of compressive residual stress and the decrease of surface roughness were beneficial to improve the pitting corrosion resistance.
Key words: aluminum; alloy,; hybrid; surface; nanocrystallization,; gradient; nanostructure,; pitting; corrosion; resistance
Jianhai YANG , Yuxiang ZHANG , Liling GE , Jiazhao CHEN , Xin ZHANG . EFFECT OF HYBRID SURFACE NANOCRYSTALLI-ZATION ON THE ELECTROCHEMICAL CORROSION BEHAVIOR IN 2A14 ALUMINUM ALLOY[J]. Acta Metall Sin, 2016 , 52(11) : 1413 -1422 . DOI: 10.11900/0412.1961.2016.00102
| [1] | Lu K, Lu J.J Mater Sci Technol, 1999; 15: 193 |
| [2] | Lu L, Sui M L, Lu K.Science, 2000; 287: 1463 |
| [3] | Lu K, Lu J.Mater Sci Eng, 2004; A375: 38 |
| [4] | Chen T, John H, Xu J, Lu Q, Hawk J, Liu X.Corros Sci, 2013; 77: 230 |
| [5] | Hajizadeh K, Maleki G H, Arabi A, Behnamian Y, Aghaie E, Farrokhi A, Hosseini M G, Fathi M H.Surf Interface Anal, 2015; 47: 978 |
| [6] | Huang R, Han Y.Mater Sci Eng, 2013; C33: 2353 |
| [7] | Jelliti S, Richard C, Retraint D, Roland T, Chemkhi M, Demangel C.Surf Coat Technol, 2013; 224: 82 |
| [8] | Ye W, Li Y, Wang F.Electrochim Acta, 2006; 51: 4426 |
| [9] | Raja K S, Namjoshi S A, Misra M.Mater Lett, 2005; 59: 570 |
| [10] | Ahmed A A, Mhaede M, Wollmann M, Wagner L.Appl Surf Sci, 2016; 363: 50 |
| [11] | Ma S N, Wang X, Wang X M.China Surf Eng, 2010; 24(5): 22 |
| [11] | (马世宁, 王翔, 王晓明. 中国表面工程, 2010; 24(5): 22) |
| [12] | Balusamy T, Sankara Narayanan T S N, Ravichandran K, Park I S, Lee M H.Corros Sci, 2013; 74: 332 |
| [13] | Bai T.PhD Dissertation, East China University of Science and Technology, Shanghai, 2013(白涛. 华东理工大学博士学位论文, 上海, 2013) |
| [14] | Klug H P, Alexander L E.X-ray Diffraction Procedures for Polycrystalline and Amorphous Materials. New York: John Wiley & Sons Wiley, 1974: 491 |
| [15] | Tao N R, Wang Z B, Tong W P, Sui M L, Lu J, Lu K.Acta Mater, 2002; 50: 4603 |
| [16] | Cheng M, Zhang D, Chen H, Qin W, Li J.Int J Adv Technol, 2016; 83: 123 |
| [17] | De A K, Murdock D C, Mataya M C, Speer J G, Matlock D K.Scr Mater, 2004; 50: 1445 |
| [18] | Kumar S A, Raman S G S, Narayanan T S N S.Surf Coat Technol, 2012; 206: 4425 |
| [19] | Liu L, Li Y, Wang F H.Acta Metall Sin, 2014; 50: 212 |
| [19] | (刘莉, 李瑛, 王福会. 金属学报, 2014; 50: 212) |
| [20] | Tong W P, Tao N R, Wang Z B, Lu J, Lu K.Science, 2003; 289: 686 |
| [21] | Ge L L, Lu Z X, Jing X T, Liu Z L, Tian N.Acta Metall Sin, 2009; 45: 566 |
| [21] | (葛利玲, 卢正欣, 井晓天, 刘忠良, 田娜. 金属学报, 2009; 45: 566) |
| [22] | Wang A X, Liu G, Zhou L, Wang K, Yang X H, Li Y.Acta Metall Sin, 2005; 41: 577 |
| [22] | (王爱香, 刘刚, 周蕾, 王科, 杨晓华, 李瑛. 金属学报, 2005; 41: 577) |
| [23] | Cao C N.Principles of Electrochemistry of Corrosion. 3rd Ed., Beijing: Chemical Industry Press, 2008: 216 |
| [23] | (曹楚南. 腐蚀电化学原理. 第三版, 北京: 化学工业出版社, 2008: 216) |
| [24] | Tong W P, Han Z, Wang L M, Lu J, Lu K.Surf Coat Technol, 2008; 202: 4957 |
| [25] | Sun Y, Bailey R.Surf Coat Technol, 2014; 253: 284 |
| [26] | Huang H W, Wang Z B, Liu L, Yong X P, Lu K.Acta Metall Sin, 2015; 51: 513 |
| [26] | (黄海威, 王镇波, 刘莉, 雍兴平, 卢柯. 金属学报, 2015; 51: 513) |
/
| 〈 |
|
〉 |