Orginal Article

MICROSTRUCTURES AND MECHANICAL PROPERTIES OF DUAL-BEAM LASER KEYHOLE WELDED JOINTS OF ALUMINUM ALLOYS TO STAINLESS STEELS

  • Feng PAN ,
  • Li CUI ,
  • Wei QIAN ,
  • Dingyong HE ,
  • Shizhong WEI
Expand
  • School of Materials Science and Engineering, Beijing University of Technology, Beijing 100124, China

Received date: 2016-03-09

  Online published: 2016-06-21

Supported by

Supported by National Natural Science Foundation of China (No.51475006) and Key Program of Research Foundation of Education Bureau of Beijing and Beijing Natural Science Foundation of B Category (No.KZ201610005004)

Abstract

Aluminum alloy and steel thin sheets have been mostly used in the automotive industry to get a lightweight car body. Nowadays several studies are focused on the joining of aluminum alloy to steel by new welding methods especially by laser welding. In this work dual-beam fiber laser keyhole welding was introduced to joining of 1.5 mm-thick aluminum alloys to 1.8 mm-thick 304 stainless steels in an overlap joint configure. The influences of different laser focusing positions on the weld appearance, interface microstructures and tensile mechanical resistance of the welded joints were studied. As a result, the good weld appearance of the aluminum alloy to stainless steel joints were obtained by dual-beam fiber laser keyhole welding process without any filler materials. The thickness of the intermetallic compound layer of the joint interface is comparatively thin when the laser beam with low energy is focusing on the front. The nano-hardness testing results show that the average hardness of intermetallic compound layer is 9.61 GPa, which is significantly higher than that of the parent stainless steel of 4.12 GPa and aluminum alloy of 1.09 GPa. The fracture of the welded joints occurs on the aluminum alloy/stainless steel interface layer. The highest mechanical resistance of 131 N/mm can be obtained by the low energy laser beam focused on the front.

Cite this article

Feng PAN , Li CUI , Wei QIAN , Dingyong HE , Shizhong WEI . MICROSTRUCTURES AND MECHANICAL PROPERTIES OF DUAL-BEAM LASER KEYHOLE WELDED JOINTS OF ALUMINUM ALLOYS TO STAINLESS STEELS[J]. Acta Metall Sin, 2016 , 52(11) : 1388 -1394 . DOI: 10.11900/0412.1961.2016.00077

References

[1] Liu B, Peng C Q, Wang R C, Wang X F, Li T T.Chin J Nonferrous Met, 2010; 20: 1705
[1] (刘兵, 彭超群, 王日初, 王小锋, 李婷婷. 中国有色金属学报, 2010; 20: 1705)
[2] Wang Z T, Zhang X H.Light Alloy Fabrication Technol, 2011; 39(2): 1
[2] (王祝堂, 张新华. 轻合金加工技术, 2011; 39(2): 1)
[3] Zhang W Z.Master Thesis, Dalian University of Technology, 2009
[3] (张维哲. 大连理工大学硕士学位论文, 2009)
[4] Ma K, Chen S H, Huang J H, Xia J, Zhang H, Zhao X K.Appl Laser, 2010; 30: 493
[4] (马柯, 陈树海, 黄继华, 夏军, 张华, 赵兴科. 应用激光, 2010; 30: 493)
[5] Lu J X, Yang W X, Wu S K, Zhao X D, Xiao R S.Acta Metall Sin (Engl Lett), 2014; 27: 670
[6] Zhou D W, Peng Y, Xu S H, Liu J S.Acta Metall Sin, 2013; 49: 959
[6] (周惦武, 彭艳, 徐少华, 刘金水. 金属学报, 2013; 49: 959)
[7] Zhou D W, Wu P, Peng L, Zhang Y, Chen G Y.Chin J Nonferrous Met, 2012; 22: 1738
[7] (周惦武, 吴平, 彭利, 张屹, 陈根余. 中国有色金属学报, 2012; 22: 1738)
[8] Ma J J, Masoud H, Carlson B, Kovacevic R.Mater Des, 2014; 58: 390
[9] Chen S H, Huang J H, Yang D D, Ma K, Zhang H.Trans China Weld, 2012; 33(8): 9
[9] (陈树海, 黄继华, 杨冬冬, 马柯, 张华. 焊接学报, 2012; 33(8): 9)
[10] Zhang S Z.Master Thesis, Lanzhou University of Technology, 2012
[10] (张诗正. 兰州理工大学硕士学位论文, 2012)
[11] Zhang D W.Master Thesis, Harbin Institute of Technology, 2010
[11] (张东卫. 哈尔滨工业大学硕士学位论文, 2010)
[12] Xiao R S, Dong P, Zhao X D.Chin J Lasers, 2011; 38(6): 28
[12] (肖荣诗, 董鹏, 赵旭东. 中国激光, 2011; 38(6): 28)
[13] Torkamany M J, Tahamtan S, Sabbaghzadeh J.Mater Des, 2010; 31: 458
[14] David A K, Team P.Mater Des, 2014; 54: 184
[15] Sierra G, Peyre P, Deschaux-Beaume F, Stuart D, Fras D.Mater Sci Eng, 2007; 447: 197
[16] Li L Q, Chen Y B, Tao W.Chin J Lasers, 2008; 35: 1783
[16] (李俐群, 陈彦宾, 陶汪. 中国激光, 2008; 35: 1783)
[17] Huang Y, Wang C M, Duan Z C, Hu L J, Hu X Y.Machinery, 2006; 44(5): 19
[17] (黄禹, 王春明, 段正澄, 胡伦骥, 胡席远. 机械制造, 2006; 44(5): 19)
[18] Yang J, Li X Y, Chen L, Gong S L, Li Q Y.Rare Met Mater Eng, 2011; 40: 871
[18] (杨璟, 李晓延, 陈俐, 巩水利, 李巧艳. 稀有金属材料与工程, 2011; 40: 871)
[19] Harooni M, Carlson B, Kovacevic R.Opt Laser Technol, 2014; 56: 247
[20] Harooni M, Ma J J, Carlson B, Kovacevic R.J Mater Process Technol, 2015; 216: 114
[21] Laukant H, Wallmann C, Korte M, Glatzel U. Adv Mater Res#/magtechI #, 2005; 6-8: 163
[22] Li L Q, Tan C W, Chen Y B, Guo W, Mei C X.J Mater Process Technol, 2013; 213: 361
[23] Tan C W, Mei C X, Li L Q, Dai J M, Guo W.Chin J Nonferrous Met, 2012; 22: 1577
[23] (檀财旺, 梅长兴, 李俐群, 戴景民, 郭伟. 中国有色金属学报, 2012; 22: 1577)
[24] Shi Y, Zhang H, Watanabe T, Tang J G.Opt Lasers Eng, 2010; 48: 732
[25] Qin G L, Lin S Y.Trans China Weld, 2006; 27(1): 81(秦国梁, 林尚扬. 焊接学报, 2006; 27(1): 81)
Outlines

/