Orginal Article

MICROSTRUCTURE, MECHANICAL PROPERTIES AND SOLIDIFICATION BEHAVIOR OF AM50-x(Zn, Y) MAGNESIUM ALLOYS

  • Feng WANG ,
  • Dezhi MA ,
  • Zhi WANG ,
  • Pingli MAO ,
  • Zheng LIU
Expand
  • School of Materials Science and Engineering, Shenyang University of Technology, Shenyang 110870, China

Received date: 2016-01-29

  Online published: 2016-05-27

Supported by

Supported by National Natural Science Foundation of China (No.51504153), Natural Science Foundation of Liaoning Province (No.201602548) and Program for Liaoning Innovative Research Team in University (No.LT2013004)

Abstract

As the lightest metallic structural material, magnesium alloys were widely used in automotive, aerospace, electronic equipment and other fields. Among commercial magnesium alloys, AM series were commonly used due to excellent ductility and energy absorption. However, their relatively poor strength greatly restricted their extended use. In order to improve mechanical properties of AM50 alloy, the Zn and Y elements were added into the AM50 alloy in the form of atomic ratio of 6∶1 by the permanent mold casting. The microstructure, solidification behavior and mechanical properties of AM50-x(Zn, Y) (x=0, 2, 3, 4, 5, mass fraction, %) alloys were investigated by OM, SEM, EDS, XRD, thermal analysis and tensile tests. The results indicated that addition of Zn and Y elements with an atomic ratio of 6∶1 to AM50 alloy, the microstructures were obviously refined, and the quasicrystal I-phase(Mg3Zn6Y) cannot form. In addition, the granular Al6YMn6 phase and fine Al2Y phase were formed in the microstructure, and the size of Al6YMn6 phase increased with increasing the Zn and Y content. The Φ-Mg21(Zn, Al)17 phase with lamellar structure was formed around β phase when x≥3, and its amount increased with increasing the Zn and Y addition. Thermal analysis results show that the Φ-Mg21(Zn, Al)17 phase was formed at 354 ℃ by the peritectic reaction, in which the precipitation temperatures of α-Mg and β phase were decreased with the increase of x content. Due to the formation of Al6YMn6, Al2Y and Φ-Mg21(Zn, Al)17 phases, the size and amount of the β phase was decreased. For AM50-4(Zn, Y) alloy, the microstructure was greatly refined, and the ultimate tensile strength, yield strength and elongation of the alloy reached to the maximum, 206.63 MPa, 92.50 MPa and 10.04%, respectively.

Cite this article

Feng WANG , Dezhi MA , Zhi WANG , Pingli MAO , Zheng LIU . MICROSTRUCTURE, MECHANICAL PROPERTIES AND SOLIDIFICATION BEHAVIOR OF AM50-x(Zn, Y) MAGNESIUM ALLOYS[J]. Acta Metall Sin, 2016 , 52(9) : 1115 -1122 . DOI: 10.11900/0412.1961.2016.00048

References

[1] Agnew S R, Nie J F.Scr Mater, 2010; 63: 671
[2] Easton M, Beer A, Barnett M, Davies C, Dunlop G, Durandet Y, Blacket S, Hilditch T, Beggs P.JOM, 2008; 60(11): 57
[3] Fechner D, Hort N, Blawert C, Dieringa H, St?rmer M, Kainer K U. J Mater Sci, 2012; 47: 5461
[4] Kondori B, Mahmudi R.Mater Sci Eng, 2010; A527: 2014
[5] ünal M.Int J Cast Met Res, 2014; 27(2): 80
[6] Wang Q D, Lin J B, Liu M P, Ding W J.Int J Mater Res, 2008; 99: 761
[7] Wang J L, Yang J, Wu Y M, Zhang H J, Wang L M.Mater Sci Eng, 2008; A472: 332
[8] Singh L K, Srinivasan A, Pillai U T S, Joseph M A, Pai B C.Trans Ind Inst Met, 2015; 68: 331
[9] Kim J M, Park B K, Jun J H, Shin K, Kim K T, Jung W J. Mater Sci Eng, 2007; A449-451: 326
[10] Zhang J S, Pei L X, Du H W, Liang W, Xu C X, Lu B F.J Alloys Compd, 2008; 453: 309
[11] Bae D H, Lee M H, Kim K T, Kim W T, Kim D H.J Alloys Compd, 2002; 342: 445
[12] Zhang J S, Zhang Y Q, Zhang Y, Xu C X, Wang X M, Yan J.Trans Nonferrous Met Soc China, 2010; 20: 1199
[13] Teng X Y, Liu T, Zhou G R, Liu L Y. Adv Mater Res, 2011; 306-307: 582
[14] Wang X D, Du W B, Wang Z H, Liu K, Li S B.Mater Sci Eng, 2011; A530: 446
[15] Wang R M, Eliezer A, Gutman E M.Mater Sci Eng, 2003; A355: 201
[16] Zhang Z, Couture A, Luo A.Scr Mater, 1998; 39: 45
[17] Ohno M, Mirkovic D, Schmid-Fetzer R.Mater Sci Eng, 2006; A421: 328
[18] Wang J L, Peng Q M, Wu Y M, Wang L M.Trans Nonferrous Met Soc China, 2006; 16(s1): 703
[19] Zheng W C, Li S S, Tang B, Zeng D B.Acta Metall Sin, 2006; 42: 835
[19] (郑伟超, 李双寿, 汤彬, 曾大本. 金属学报, 2006; 42: 835)
[20] Pettersen G, Westengen H, H?ier R, Lohne O.Mater Sci Eng, 1996; A207: 115
[21] Wu G H, Fan Y, Zhai C Q, Ding W J.Acta Metall Sin, 2008; 44: 1247
[21] (吴国华, 樊昱, 翟春泉, 丁文江. 金属学报, 2008; 44: 1247)
[22] Wang J, Zhu X R, Xu Y D, Wang R, Nie J J, Zhang L J.Chin J Nonferrous Met, 2014; 24: 25
[22] (王军, 朱秀荣, 徐永东, 王荣, 聂景江, 张立君. 中国有色金属学报, 2014; 24: 25)
[23] Ohno M, Mirkovic D, Schmid-Fetzer R.Acta Mater, 2006; 54: 3883
[24] Wang Y S, Wang Q D, Ma C J, Ding W J, Zhu Y P.Mater Sci Eng, 2003; A342: 178
[25] Lü Y Z, Wang Q D, Ding W J, Zeng X Q, Zhu Y P.Mater Lett, 2000; 44(5): 265
[26] Maxwell I, Hellawell A.Acta Metall, 1975; 23: 229
[27] Becerra A, Pekguleryuz M.J Mater Res, 2009; 24: 1722
[28] Hou D H, Liang S M, Chen R S, Dong C.Acta Metall Sin, 2014; 50: 601
[28] (侯丹辉, 梁松茂, 陈荣石, 董闯. 金属学报, 2014; 50: 601)
[29] Zhao Z D, Chen Q, Wang Y B, Shu D Y. Mater Sci Eng, 2009; A515: 152
[30] Yuan W, Panigrahi S K, Su J Q, Mishra R S.Scr Mater, 2011; 65: 994
Outlines

/

〈 〉