Orginal Article

INVESTIGATION ON THE WELDING PROCESS AND MICROSTRUCTURE AND MECHANICAL PROPERTY OF BUTT JOINTS OF TA1/X65 CLAD PLATES

  • Zongyue BI ,
  • Jun YANG ,
  • Haizhang LIU ,
  • Wanpeng ZHANG ,
  • Yaobin YANG ,
  • Lei TIAN ,
  • Xiaojiang HUANG
Expand
  • 1 National Engineering Technology Research Center for Petroleum and Natural Gas Tubular Goods, Baoji 721008, China.
    2 Steel Pipe Research Institute of Baoji Petroleum Steel Pipe Co., Ltd., Baoji 721008, China

Received date: 2015-11-30

  Online published: 2016-04-21

Abstract

Titanium/steel clad material with excellent mechanical properties and corrosion resistance has important application in storage and transportation equipment of oil and gas. Due to the metallurgical incompatibility of titanium and steel, the mechanical properties of weld joint would completely lose when the brittle intermetallic phase TixFey and TiC appeared in the fusion welding process. Therefore, the gas tungsten arced welding (TIG), metal inert-gas welding (MIG) and metal active-gas welding (MAG) with V/Cu composite filler metals for butt joint in this study was carried out on TA1/X65 pipeline steel clad plates with thickness 16 mm ( titanium cladding with thickness 2 mm, X65 pipeline steel with thickness 14 mm). The microstructure, interface element distribution, main phase, microhardness distribution on cross section and mechanical properties of butt welds were investigated by using OM, XRD, EDS element mapping, microhardness and tensile test. The results indicate that the design of “U-type” circular groove advantageous to the MIG of Cu transition-metals, because of the “U-type” circular groove does not cause stress concentration and crack initiation. The deposited metal of Ti, V, Cu and Fe have obvious zoning, interdiffusion melting phenomenon is not severe, and by using solid solution phases to transit zonings of deposited metal. The microstructure of Ti and V transition interface was composed of Ti-based solid solution, the microstructure of V and Cu transition interface was composed of V-based solid solution, and the microstructure of Cu and Fe transition interface was composed of Cu-based solid solution. The high hardness region of butt weld cross section appeared in the Ti/V transition-interface and V/Cu transition-interface, the hardness value was respectively 326 HV10 and 336 HV10, and weakened the ductility of transition interfacial layer. A joint with a tensile strength of 546 MPa, mainly of that of the carbon steel was obtained.

Cite this article

Zongyue BI , Jun YANG , Haizhang LIU , Wanpeng ZHANG , Yaobin YANG , Lei TIAN , Xiaojiang HUANG . INVESTIGATION ON THE WELDING PROCESS AND MICROSTRUCTURE AND MECHANICAL PROPERTY OF BUTT JOINTS OF TA1/X65 CLAD PLATES[J]. Acta Metall Sin, 2016 , 52(8) : 1017 -1024 . DOI: 10.11900/0412.1961.2015.00615

References

[1] Zhang X Y, Zhao Y Q, Bai C G.Titanium Alloys and Their Applications .Beijing: Chemical Industry Press, 2005: 287
[1] (张喜燕, 赵永庆, 白晨光. 钛合金及应用. 北京: 化学工业出版社, 2005: 287)
[2] Yuan X J, Sheng G M, Qin B.Mater Charact, 2008; 59: 930
[3] Li G Q.Welded Pipe Tube, 2011; 34(11): 39
[3] (李国庆. 焊管, 2011; 34(11): 39)
[4] Xu G Z.Welded Pipe Tube, 2009; 32(11): 70
[4] (许贵芝. 焊管, 2009; 32(11): 70)
[5] Yang K, Wang Y J, Yun H T, Bai Y, Fu L.Welded Pipe Tube, 2015; 38(7): 6
[5] (杨凯, 王永军, 云海涛, 白颖, 傅莉. 焊管, 2015; 38(7): 6 )
[6] Sheng C C, Master Thesis Jiangsu University of Science and Technology, Zhenjiang, 2008
[6] (盛长城. 江苏科技大学硕士学位论文, 镇江, 2008)
[7] Li P, Li J L, Xiong J T, Zhang F S.J Aeronaut Mater, 2010; 30(5): 25
[7] (李鹏, 李京龙, 熊江涛, 张赋升. 航空材料学报, 2010; 30(5): 25)
[8] Liu P, Lu M, Ji X W, Huang Q, Dai R X.Ordnance Mater Sci Eng, 2011; 34(3): 14
[8] (刘鹏, 陆明, 冀鑫炜, 黄钦, 戴汝迅. 兵器材料科学与工程, 2011; 34(3): 14)
[9] Yan W, Master Thesis Northeastern University Shenyang, 2006
[9] (闫伟. 东北大学硕士学位论文, 沈阳, 2006)
Outlines

/