Orginal Article

CHARACTERISTIC TEMPERATURE AND PERFOR-MANCE OF THE Ge30Se70 CHALCOGENIDE GLASS

  • Tingting JIA ,
  • Zengyun JIAN ,
  • Junfeng XU ,
  • Man ZHU ,
  • Fang'e CHANG
Expand
  • School of Materials and Chemical Engineering, Xi'an Technological University, Xi'an 710021, China

Received date: 2015-09-25

  Online published: 2016-04-12

Supported by

Supported by National Basic Research Program of China (No.2013CB632904), National Natural Science Foundation of China (Nos.51371133, 51171136, 51301125 and 51401156), Natural Science Foundation of Shaanxi Province (Nos.2012JM6010 and 2014- JM6225) and Key Laboratory Research Project of Shaanxi Provincial Education Department (No.13JS041)

Abstract

Chalcogenide glass is an ideal infrared wave-transparent material, and it has the advantages of low cost, high production efficiency, high glass transition temperature and good mechanical properties, etc.. It is a candidate material for thermal imaging system. The block sample of Ge30Se70 chalcogenide glass was prepared by the method of the melt-quenched. In this work, XRD was used to determine whether the sample was amorphous material. With the DSC thermal analysis method, the glass transition temperature Tg and the initial crystallization temperature Tx of the sample were measured. The dynamics ideal glass transition temperature T0 of the specimen was fitted by VFT equation. The method of segmented step heating is used to analyze the calorific value for the glass and congruent crystal of Ge30Se70 sample in setting temperature range. Then from the calculated calorific values of the glass and crystalline samples, the specific heat capacity relationships were obtained, i.e., cp,l=0.0002T+0.3337 and cp,c=0.00006T+0.4594. The results show that Tg and T0 of Ge30Se70 sample is 590 and 581 K, respectively. And Tg will increase with the increasing of the heating rate R. The average value of the specific heat capacity of the Ge30Se70 glass sample is about 11.8 J/(molK) below the glass transition temperature. The infrared transmittance is about 60% indicating that the infrared performance is good. The glass reduced temperature Trg of Ge30Se70 sample is between 0.5~0.667, and the nucleation rate is very low, which indicates that the glass forming ability of Ge30Se70 glass is good.

Cite this article

Tingting JIA , Zengyun JIAN , Junfeng XU , Man ZHU , Fang'e CHANG . CHARACTERISTIC TEMPERATURE AND PERFOR-MANCE OF THE Ge30Se70 CHALCOGENIDE GLASS[J]. Acta Metall Sin, 2016 , 52(6) : 755 -760 . DOI: 10.11900/0412.1961.2015.00501

References

[1] Wei W H.PhD Dissertation, Chongqing University, 2014
[1] (魏文猴. 重庆大学博士学位论文, 2014)
[2] Song B A, Dai S X, Xu T F, Nie Q H, Shen X, Wang X S, Lin C G.Acta Phys Sin, 2011; 60: 084217-1
[2] (宋宝安, 戴世勋, 徐铁峰, 聂秋华, 沈祥, 王训四, 林常规. 物理学报, 2011; 60: 084217-1)
[3] Jian Z Y, Zheng C, Chang F E, Zhou J, Gao Y S, Lv S Y.J Xi'an Technol Univ, 2009; 29: 52
[3] (坚增运, 郑超, 常芳娥, 周晶, 高玉社, 吕士勇. 西安工业大学学报, 2009; 29: 52)
[4] Xue J Q, Xu M, Gong Y Q, Zhao X J.Optoelectron Technol Inf, 2003; 16(4): 28
[4] (薛建强, 徐曼, 龚跃球, 赵修建. 光电子技术与信息, 2003; 16(4): 28)
[5] Zhang X H.Laser Focus World, 2002; 38: 71
[6] Zhang X H, Guimond Y, Bellec Y.J Non-Cryst Solids, 2003; 326: 519
[7] Yin D M, Dai S X, Wang X S, Xu Y S, Zhang P Q, Lin C G, Shen X.Laser Optoelectron Progr, 2013; 50(2): 92
[7] (尹冬梅, 戴世勋, 王训四, 许银生, 张培晴, 林常规, 沈祥. 激光与光电子学进展, 2013; 50(2): 92)
[8] Burgess T, Ferry M.Mater Today, 2009; 12: 24
[9] Inoue A, Shen B L, Koshiba H, Kato H, Yavari A R.Acta Mater, 2004; 52: 1631
[10] Orava J, Greer A L, Gholipour B, Hewak D W, Smith C E.Nat Mater, 2012; 11: 279
[11] Giulia D F, Livio B.Acta Mater, 2013; 61: 2260
[12] Mukherjee S, Schroers J, Johnson W L, Rhim W K. Phys Rev Lett, 2005; 94: 245501
[13] Angell C A.Science, 1995; 267: 1924
[14] Fontana G D, Battezzati L.Acta Mater, 2013; 61: 2260
[15] Tournier R F. Intermetallics, 2012; 30: 104
[16] Turnbull D.Contemp Phys, 1969; 10: 473
[17] Mukherjee S, Schroers J, Johnson W L, Rhim W K.Phys Rev Lett, 2005; 94: 245501
[18] Stillinger F H.J Chem phys, 1988; 88: 7818
[19] Kauzmann W.Chem Rev, 1948; 43: 219
[20] Mei Q S, Lu K.Prog Mater Sci, 2007; 52: 1175
[21] Chen G R, Cheng J J.Bull Chin Ceram Soc, 1997; (4): 63
[21] (陈国荣, 程继健. 硅酸盐通报, 1997; (4): 63)
[22] Zallen R.The Physics of Amorphous Solids. New York: A Wiley-Interscience Publication, 1983: 53
[23] Jiang Q, Xu X Y, Zhao M.Acta Metall Sin, 1997; 33: 763
[23] (蒋青, 徐晓亚, 赵明. 金属学报, 1997; 33: 763)
[24] Turnbull D.Contemp Phys, 1969; 10: 473
[25] Inoue A.Acta Mater, 2000; 48: 279
[26] Vogel H.Physikalische Zeitschrift, 1921; 22: 645
[27] Fulcher G S.J Am Ceram Soc, 1925; 8: 339
[28] Tammann G, Hesse G Z.Anorg Allg Chem, 1926; 156: 245
[29] Flynn J H.Thermochim Acta, 1993; 217: 129
[30] Fan G J, L?ffler J F, Wunderlich R K, Fecht H J.Acta Mater, 2004; 52: 667
[31] Jia R, Bian X F, Wang Y Y.Chin Sci Bull, 2011; 56: 3912
Outlines

/

〈 〉