INFLUENCE OF Re ON MICROSTRUCTURESOF A DIRECTIONALLY SOLIDIFIEDNi-BASED SUPERALLOY

  • Siqian ZHANG ,
  • Dong WANG ,
  • Di WANG ,
  • Jianqiang PENG
Expand
  • 1 School of Materials Science and Engineering, Shenyang University of Technology, Shenyang 110870, China.
    2 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China.
    3 Harbin Turbine Co. Ltd., Harbin 150046, China.

Received date: 2015-11-19

  Online published: 2016-03-21

Supported by

Supported by National Natural Science Foundation of China (Nos.51101160 and 51501117), National Key Foundation for Exploring Scientific Instrument (No.2012YQ22023304) and Liaoning Provincial Department of Education Project (No.L2014050)

Abstract

Up to now, considerable effort has been expended in attempts to investigate the influences of Re on Ni-based single crystal superalloys. However, few study had elucidated the influences of Re on carbide, boride and grain boundary. Therefore, the influence of a 2%Re (mass fraction) addition on the as-cast and heat-treated microstructures of a Ni-based directionally solidified superalloy was investigated by comparison with Re-free alloy using SEM, EPMA and TEM. The results show that Re accelerates the precipitation of μ phase in the periphery of eutectic and at grain boundary for as-cast microstructure. After heat treatment, Re also accelerates the precipitation of phase in the vicinity of primary MC carbide and at grain boundary. For 0Re alloy, there are small number of M6C carbide in the vicinity of primary MC carbide and M23(C, B)6 boro-carbide at grain boundary. For 2Re alloy, a large amount of blocky μ phase enveloped by thick γ′-film is found in the vicinity of primary MC carbide and at grain boundary. Enrichment of B along the grain boundary is observed in 0Re alloy. On the contrary, relatively uniform distribution of B is found in 2Re alloy. The precipitation mechanism of μ phase during the process of heat treatment is also analyzed.

Cite this article

Siqian ZHANG , Dong WANG , Di WANG , Jianqiang PENG . INFLUENCE OF Re ON MICROSTRUCTURESOF A DIRECTIONALLY SOLIDIFIEDNi-BASED SUPERALLOY[J]. Acta Metall Sin, 2016 , 52(7) : 851 -858 . DOI: 10.11900/0412.1961.2015.00600

References

[1] Koizumi Y, Kobayashi T, Yokokawa T, Zhang J X, Osawa M, Harada H, Aoki Y, Arai M.In: Green K A, Pollock T M, Harada H, Howson T E, Reed R C, Schirra J J, Walston S eds., Superalloys 2004, Warrendale, PA: The Minerals, Materials and Metals Society, 2004: 35
[2] Harris K, Erickson G L, Sikkenga S L, Brentnall W D, Aurrecoechea J M, Kubarych K G.J Mater Eng Perform, 1993; 2: 481
[3] Ross E W, O'Hara K S. In: Antolovich S D, Stusrud R W, MacKay R A, Anton D L, Khan T, Kissinger R D, Klarstrom D L eds., Superalloys 1992, Warrendale, PA: The Minerals, Materials and Metals Society, 1992: 257
[4] Cetel A D, Duhl D N.In: Antolovich S D, Stusrud R W, MacKay R A, Anton D L, Khan T, Kissinger R D, Klarstrom D L eds., Superalloys 1992, Warrendale, PA: The Minerals, Materials and Metals Society, 1992: 287
[5] Bürgel R, Grossmann J, Lüseberink O, Mughrabi H, Pyczak F, Singer R F, Volek A.In: Green K A, Pollock T M, Harada H, Howson T E, Reed R C, Schirra J J, Walston S eds., Superalloys 2004, Warrendale, PA: The Minerals, Materials and Metals Society, 2004: 25
[6] Harris K, Erickson G L, Schwer R E.In: Gell M, Kortovich C S, Bricknell R H, Kent W B, Radovich J F eds., Superalloys 1984, Warrendale, PA: The Minerals, Materials and Metals Society, 1984: 221
[7] Harris K, Erickon G L, Sikkenga S L, Kubarych K G.In: Antolovich S D, Stusrud R W, MacKay R A, Anton D L, Khan T, Kissinger R D, Klarstrom D L eds., Superalloys 1992, Warrendale, PA: The Minerals, Materials and Metals Society, 1992: 297
[8] Chen R Z. J Aero Mater, 1993; (1): 47
[8] (陈荣章. 航空材料学报, 1993; (1): 47)
[9] Blavette D, Caron P, Khan T.Scr Mater, 1986; 20: 1395
[10] Warren P J, Cerezo A, Smith G D W.Mater Sci Eng, 1998; A250: 88
[11] Mottura A, Warnken N, Miller M K, Finnis M W, Reed R C.Acta Mater, 2010; 58: 931
[12] Wanderka N, Glatzel U.Mater Sci Eng, 1995; A203: 69
[13] Rüsing J, Wanderka N, Czubayko U, Naundorf V, Mukherji D, R?sler J.Scr Mater, 2002; 46: 235
[14] Epishin A, Bruckner U, Portella P D, Link T.Scr Mater, 2003; 48: 455
[15] Fu C L, Reed R, Janotti A, Krcmar M.In: Green K A, Pollock T M, Harada H, Howson T E, Reed R C, Schirra J J, Walston S eds., Superalloys 2004, Warrendale, PA: The Minerals, Materials and Metals Society, 2004: 867
[16] Luo Y S, Li J R, Liu S Z, Sun F L, Han X M, Cao C X.Chin J Nonferrous Met, 2005; 15: 1655
[16] (骆宇时, 李嘉荣, 刘世忠, 孙凤礼, 韩秀梅, 曹春晓. 中国有色金属学报, 2005; 15: 1655)
[17] Li P, Li Q Q, Jin T, Zhou Y Z, Li J G, Sun X F, Zhang Z F.Mater Sci Eng, 2014; A603: 84
[18] Zhang Y D, Yang Z G, Zhang C, Lan H.Chin J Aero, 2010; 23: 370
[19] Wang M G, Tian S G, Yu H C, Yu X F, Qian B J.J Aero Mater, 2009; 29(4): 98
[19] (王明罡, 田素贵, 于慧臣, 于兴福, 钱本江. 航空材料学报, 2009; 29(4): 98)
[20] Li J R, Tang D Z, Chen R Z.J Mater Eng, 1997; (8): 3
[20] (李嘉荣, 唐定中, 陈荣章. 材料工程, 1997; (8): 3)
[21] Darolia R, Lahrman D F, Field R D.In: Reichman S, Duhl D N, Maurer S, Antolovich S, Lund C eds., Superalloys 1988, Warrendale, PA: The Minerals, Materials and Metals Society, 1988: 255
[22] Walston W S, Schaeffer J C, Murphy W H.In: Kissinger R D, Deye D J, Anton D L, Cetel A D, Nathal M V, Pollock T M, Woodford D A eds., Superalloys 1996, Warrendale, PA: The Minerals, Materials and Metals Society, 1996: 9
[23] Walston W S, O'Hara K S, Ross E W, Pollock T M, Murphy W H. In: Kissinger R D, Deye D J, Anton D L, Cetel A D, Nathal M V, Pollock T M, Woodford D A eds., Superalloys 1996, Warrendale, PA: The Minerals, Materials and Metals Society, 1996: 27
[24] Pollock T M, Murphy W H, Goldman E H, Uram D L, Tu J S.In: Antolovich S D, Stusrud R W, MacKay R A, Anton D L, Khan T, Kissinger R D, Klarstrom D L eds., Superalloys 1992, Warrendale, PA: The Minerals, Materials and Metals Society, 1992: 125
[25] Kong Y H, Chen Q Z.Mater Sci Eng, 2004; A366: 135
Outlines

/