Orginal Article

STRESS CORROSION BEHAVIORS OF E690 HIGH-STRENGTH STEEL IN SO2-POLLUTED MARINE ATMOSPHERE

  • Hongchi MA ,
  • Cuiwei DU ,
  • Zhiyong LIU ,
  • Wenkui HAO ,
  • Xiaogang LI ,
  • Chao LIU
Expand
  • 1 Key Laboratory for Corrosion and Protection, Ministry of Education, Corrosion and Protection Center, University of Science and Technology Beijing, Beijing 100083, China
    2 Ningbo Institute of Material Technology & Engineering, Chinese Academy of Sciences, Ningbo 315201, China

Received date: 2015-07-09

  Online published: 2016-03-17

Supported by

Supported by National Basic Research Program of China (No.2014CB643300), National Natural Science Foundation of China (Nos.51471034, 51131005 and 51171025), National Environmental Corrosion Platform (NECP) and Beijing Higher Education Young Elite Teacher Project

Abstract

With the development of industry, the atmosphere in many cities along the coastal lines such as Qingdao in China has been polluted with SO2, and has been changed to coastal-industrial atmosphere with the co-existence of SO2 and Cl-. The corrosion and stress corrosion cracking (SCC) behavior and mechanism of steel in this environment is different from that in the coastal atmosphere containing only Cl- or the industrial atmosphere containing only SO2. Previous study have indicated that SO2 in the marine atmosphere can greatly promote the stress corrosion cracking of high-strength steel due to acidification of thin electrolyte layer and reproduction of H+ through FeSO4. E690 steel, as a newly-developed high strength steel, is very promising to be widely used in offshore platform in the near future for its excellent performance. However, there is few research about its SCC behavior in marine atmosphere, especially in SO2-polluted atmosphere. Therefore, it's of great importance to investigate the SCC behavior and mechanism of E690 steel in this environment. In this work, U-bend specimen corrosion test under dry/wet cyclic condition, electrochemical measurements, crack morphology observation and rust layer analysis, were conducted to investigate the effect of SO2 on SCC behavior of E690 steel in simulated SO2-polluted marine atmosphere. The results indicated that E690 steel has a high SCC susceptibility in SO2-polluted marine atmosphere with a combined mechanism of anodic dissolution (AD) and hydrogen embrittlement (HE). SO2 in the atmosphere can facilitate the densification of inner rust layer by promoting the formation of α-FeOOH and enrichment of Ni and Cr in the inner rust layer, leading to the concentration of Cl- under the rust layer, which may result in the initiation and propagation of SCC cracks significantly and therefore enhance the SCC susceptibility.

Cite this article

Hongchi MA , Cuiwei DU , Zhiyong LIU , Wenkui HAO , Xiaogang LI , Chao LIU . STRESS CORROSION BEHAVIORS OF E690 HIGH-STRENGTH STEEL IN SO2-POLLUTED MARINE ATMOSPHERE[J]. Acta Metall Sin, 2016 , 52(3) : 331 -340 . DOI: 10.11900/0412.1961.2015.00362

References

[1] Han E-H, Chen J M, Su Y J, Liu M.Mater China, 2014; 33(2): 65
[1] (韩恩厚, 陈建敏, 宿彦京, 刘敏. 中国材料进展, 2014; 33(2): 65)
[2] Nishikata A, Ichihara Y, Hayashi Y, Tsuru T.J Electrochem Soc, 1997; 144: 1244
[3] Zhong X K, Zhang G A, Qiu Y B, Chen Z Y, Guo X P, Fu C Y. Corros Sci, 2013; 66: 14
[4] Qiao L J, Luo J L, Mao X.Corrosion, 1998; 54: 115
[5] Dmytrakh I M, Smiyan O D, Syrotyuk A M, Bilyy O L.Int J Fatigue, 2013; 50: 26
[6] Gu B, Luo J, Mao X.Corrosion, 1999; 55: 96
[7] Li M C, Cheng Y F.Electrochim Acta, 2007; 52: 8111
[8] Chen W J, Hao L, Dong J H, Ke W, Wen H L.Acta Metall Sin, 2014; 50: 802
[8] (陈文娟, 郝龙, 董俊华, 柯伟, 文怀梁. 金属学报, 2014; 50: 802)
[9] Wang C, Wang Z Y, Ke W.Acta Metall Sin, 2008; 44: 729
[9] (汪川, 王振尧, 柯伟. 金属学报, 2008; 44: 729)
[10] Chen W J, Hao L, Dong J H, Ke W.Corros Sci, 2014; 83: 155
[11] Wang J H, Wei F I, Chang Y S, Shih H C.Mater Chem Phys, 1997; 47: 1
[12] Nishimura R, Shiraishi D, Maeda Y.Corros Sci, 2004; 46: 225
[13] Zheng C B, Huang Y L, Wang X, Sun G J, Pan L Z.Mater Prot, 2011; 44(5): 34
[13] (郑传波, 黄彦良, 王旭, 孙广杰, 潘立志. 材料保护, 2011; 44(5): 34)
[14] Zheng C B.PhD Dissertation, Institute of Oceanography, Chinese Academy of Sciences, Qingdao, 2008
[14] (郑传波. 中国科学院海洋研究所博士学位论文, 青岛, 2008)
[15] Xiong X Q, Xiong W M, Chen Y J, Sun X Z.Jiangxi Metall, 2012; 32(6): 21
[15] (熊小强, 熊文名, 陈英俊, 孙熙钟. 江西冶金, 2012; 32(6): 21)
[16] Zhang J, Cai Q W, Wu H B, Fan X H, Zhang M J.J Univ Sci Technol Beijing, 2012; 34: 657
[16] 张杰, 蔡庆伍, 武会宾, 樊学华, 张明洁. 北京科技大学学报, 2012; 34: 657)
[17] Wu B, Cai Q W, Zhang J, Wu H B.Heat Treat Met, 2011; 36(3): 26
[17] (武博, 蔡庆伍, 张杰, 武会宾. 金属热处理, 2011; 36(3): 26)
[18] Hao W K.PhD Dissertation, University of Science and Technology Beijing, 2015
[18] (郝文魁. 北京科技大学博士学位论文, 2015)
[19] Ma Y T, Li Y, Wang H F.Corros Sci, 2009; 51: 997
[20] Hao L, Zhang S X, Dong J H, Ke W.Corros Sci, 2012; 58: 175
[21] Collazo A, Novoa X R, Pérez C, Puga B.Electrochim Acta, 2008; 53: 7565
[22] Zhang Q C, Wu J S, Wang J J, Zheng W L, Chen J G, Li A B.Mater Chem Phys, 2003; 77: 603
[23] Castaño J G, Botero C A, Restrepo A H, Agudelo E A, Correa E, Echeverría F.Corros Sci, 2010; 52: 216
[24] Hao L, Zhang S X, Dong J H, Ke W. Corros Sci, 2012; 59: 270
[25] Akiyama E, Li S, Shinohara T, Zhang Z, Tsuzaki K.Electrochim Acta, 2011; 56: 1799
[26] Akiyama E, Matsukado K, Wang M, Tsuzaki K.Corros Sci, 2010; 52: 2758
[27] Tsuru T, Huang Y L, Ali M R, Nishikata A.Corros Sci, 2005; 47: 2431
[28] Antony H, Perrin S, Dillmann P, Legrand L, Chaussé A.Electrochim Acta, 2007; 52: 7754
[29] Zhou Y L, Chen J, Liu Z Y.J Iron Steel Res, 2013; 20: 66
[30] Tamura H.Corros Sci, 2008; 50: 1872
[31] Kamimura T, Hara S, Miyuki H, Yamashita M, Uchida H.Corros Sci, 2006; 48: 2799
[32] Dillmann P, Mazaudier F, Hoerle S.Corros Sci, 2004; 46: 1401
[33] Yamashita M, Miyuki H, Matsuda Y, Nagano H, Misawa T.Corros Sci, 1994; 36: 283
[34] Singh D D, Yadav S, Saha J K.Corros Sci, 2008; 50: 93
[35] Allam I M, Arlow J S, Saricimen H.Corros Sci, 1991; 32: 417
Outlines

/