STUDY ON REJUVENATION HEAT TREATMENT OF A DIRECTIONALLY-SOLIDIFIED SUPERALLOYDZ125 DAMAGED BY CREEP
Received date: 2015-09-26
Online published: 2016-03-11
The degradation of microstructure and property in turbine blades of aircraft engines is inevitable during their service. Usually, rejuvenation heat treatment is applied to regenerate the original microstructure for extending the service life of blades and improve economic returns. To date, systematic investigations about rejuvenation heat treatment of the directionally-solidified superalloys are limited. In this work, the effect of rejuvenation heat treatment on the degraded microstructure and property of DZ125 superalloy damaged by creep was investigated. The interrupted creep test was first conducted on DZ125 superalloy to simulate the damage of turbine blades during their service. Three rejuvenation heat treatments with the solution temperature at 1230, 1240 and 1250 ℃ were applied to the interrupted creep specimen. Then, the rejuvenated specimens were retested, and their microstructures as well as creep properties were compared with those of the initial interrupted creep tests. The results showed that no recrystallization occurred after the interrupted creep tests at 1.0% and 3.5% strain followed by rejuvenation heat treatment, and the critical strain for the formation of the recrystallization was between 3.5%~10.0%. The solution treatment at 1230 ℃ partially dissolved the coarse γ' phase caused by creep deformation, caused a nonuniform microstructure of γ /γ' matrix after aging treatments, and resulting in partially recovering the baseline creep property. However, the solution treatment at 1240 and 1250 ℃ could not only dissolve the coarse γ' phase but also reduce the fraction of residual γ' eutectic significantly, and then regain a uniform microstructure of γ /γ' matrix after aging treatments. Hence, the effect of rejuvenation was further improved, maintaining or exceeding the baseline creep property.
Jing ZHANG , Yunrong ZHENG , Qiang FENG . STUDY ON REJUVENATION HEAT TREATMENT OF A DIRECTIONALLY-SOLIDIFIED SUPERALLOYDZ125 DAMAGED BY CREEP[J]. Acta Metall Sin, 2016 , 52(6) : 717 -726 . DOI: 10.11900/0412.1961.2015.00505
| [1] | Feng Q, Tong J Y, Zheng Y R, Wang M L, Wei W J, Zhao H L, Yuan X F, Ding X F.Mater China, 2012; 31(12): 31 |
| [1] | (冯强, 童锦艳, 郑运荣, 王美玲, 魏文娟, 赵海龙, 袁晓飞, 丁贤飞. 中国材料进展, 2012; 31(12): 31) |
| [2] | Li W.Gas Turbine Experiment Res, 2002; 15(2): 28 |
| [2] | (李伟. 燃气涡轮试验与研究, 2002; 15(2): 28) |
| [3] | Tao C H, Zhang W F, Li Y J, Shi H J.Failure Anal Prevention, 2006; 1(4): 1 |
| [3] | (陶春虎, 张卫方, 李运菊, 施惠基. 失效分析与预防, 2006; 1(4): 1) |
| [4] | Liburdi J, Lowden P, Nagy D, De Priamus T R, Shawet S. In: Proc ASME Turbo Expo, Orlando: International GasTurbine Institute, 2009: 819 |
| [5] | Guo J T.Materials Science and Engineering for Superalloys. Vol. 2, Beijing: Science Press, 2008: 405 |
| [5] | (郭建亭. 高温合金材料学(中册). 北京: 科学出版社, 2008: 405) |
| [6] | Davies P W, Dennison J P, Evans H E.J Inst Met, 1966; 94(8): 270 |
| [7] | Steven R A, Flewitt P E J.J Mater Sci, 1978; 13: 367 |
| [8] | Dennison J P, Elliott I C, Evans H E.In: Tien J K, Wlodek S T, Morrow H, Gell M, Maurer G E eds., Superalloys 1980, Ohio: TMS, 1980: 671 |
| [9] | Dennison J P, Wilshire B.In: Taplin D M R ed., Fracture 1977, Proc 4th Int Conf on Fracture, Waterloo: University of Waterloo Press, 1977: 635 |
| [10] | Liburdi J, Stephens J O. ASME1980 International Gas Turbine Conference and Products Show, New Orleans: American Society of Mechanical Engineers, 1980: 80-GT-181 |
| [11] | Rettberg L H, Tsunekane M, Pollock T M.In: Huron E S, Reed R C, HardyM C, Mills M J, Montero R E, Portella P D, Telesman J eds., Superalloys 2012, Warrendale, Pennsylvania: TMS, 2012: 341 |
| [12] | Koul A K, Immarigeon J P, Castillo R, Lowden P, Liburdi J.In: Reichman S, Nuhl D N, Maurer G, Antolovich S, Lund C eds., Superalloys 1988, Warrendale, Pennsylvania: TMS, 1988: 755 |
| [13] | Davies P W, Dennison J P.Met Sci, 1975; 9: 319 |
| [14] | China Aeronautical Materials Handbook Editorial Committee. China Aeronautical Materials Handbook. Vol.2, Beijing: China Sandard Pess, 2002: 771 |
| [14] | (中国航空材料手册编辑委员会. 中国航空材料手册.第2卷, 北京: 中国标准出版社, 2002: 771) |
| [15] | Nathal M V, Mackay R A.Mater Sci Eng, 1987; A85: 127 |
| [16] | Davies P W, Dennison J P.Met Sci, 1975; 9: 319 |
| [17] | Koul A K, Castillo R.Metall Trans, 1988; 19A: 2049 |
| [18] | She L, Chen R Z, Wang T.Trans Mater Heat Treatment, 2002; (4): 13 |
| [18] | (佘力, 陈荣章, 王涛. 金属热处理学报, 2002; (4): 13) |
| [19] | She L, Chen R Z. Rare Met, 1998; 22(4): 19(佘力, 陈荣章. 稀有金属, 1998; 22(4): 19) |
| [20] | Chen R Z, Wang L B, Wang Y P.Acta Aeron Astronaut Sin, 1988; 7: 368 |
| [20] | (陈荣章, 王罗宝, 王玉屏. 航空学报, 1988; 7: 368) |
| [21] | Zheng Y R, Wang L B, Li C G.Chin J Met Sci Technol, 1989; 5(2): 90 |
| [22] | Tian S G, Tian N, Yu H C, Meng X L, Li Y.Mater Sci Eng, 2014; A615: 469 |
| [23] | Zheng Y R, Cai Y L, Wang L B.Acta Metall Sin, 1983; 19: 30 |
| [23] | (郑运荣, 蔡玉林, 王罗宝. 金属学报, 1983; 19: 30 |
| [24] | Xie G, Wang L, Zhang J, Lou L H.Metall Mater Trans, 2008; 39A: 206 |
| [25] | Koizumi Y, Kobayashi T, Harada H, Yamagata T.In: Strang A, Banks W M, Conroy R D, Goulette M J eds., Advances in Turbine Materials, Design and Manufacturing, Newcastle upon Tyne: Maney Materials Science, 1997: 679 |
| [26] | Decker R F, Dewitt R R.J Met, 1965; 17: 139 |
| [27] | Jackson J J, Donachie M J, Gell M, Henricks R J.Metall Trans, 1977; 8A: 1615 |
| [28] | Ross M D, Bennett G T, Stewart D C.Rejuvenation of Turbine Blade Material by Thermal Treatment. West Palm Beach, Florida: Pratt and Whitney Aircraft, 1979: 14 |
| [29] | Zheng Y R, Han Y F.Acta Metall Sin, 2002; 38: 1203 |
| [29] | (郑运荣, 韩雅芳. 金属学报, 2002; 38: 1203) |
/
| 〈 |
|
〉 |