Abstract

The experimental alloy is designed and employed in high-performance industrial gas turbines as low-pressure turbine blades, working in temperature range of 750~900 ℃. The alloy contains high levels of refractory elements in order to increase the high-temperature mechanical properties. However, this can make the alloy prone to the formation of σ phase during service, which could deteriorate the properties further if the fraction of σ phase exceeds the safety allowances. In this study, the formation of σ phase during long-term thermal exposure, dissolution of the σ phase during rejuvenation process and their influence on stress-rupture properties of a hot-corrosion resistant nickel base superalloy have been investigated. During long-term thermal exposure at 800~900 ℃ for up to 1×104 h, the σ phase formation is mainly in dendrite cores with a few at interdendritic regions. As the aging temperature increases, the precipitation rate of σ phase increases and the incubation time for nucleation of σ phase decreases. From the kinetic analysis, the σ phase form firstly in the vicinity or on the M23C6 in dendrite cores with the strong segregation of W, Cr and Co. The calculated activation energies of σ formation show that the early stage is related to Co and Cr diffusions and the steady stage is related to Mo diffusion. During solid solution process at 1000~1170 ℃, the σ phase precipitated during long-term thermal exposure dissolves to γ matrix. As the solid solution temperature is higher, the dissolution of σ phase becomes faster. Moreover, the σ phase does not embrittle the alloy. The reheat treatment of the alloy leads to the dissolution of precipitated σ phase and further prolongs the stress-rupture life efficiently.

Cite this article

Jieshan HOU , Jianting GUO , Chao YUAN , Lanzhang ZHOU . STUDY ON THE PRECIPITATION AND DISSOLUTION OF σ PHASE IN A HOT CORROSION RESISTANCE CAST NICKLE BASE SUPERALLOY[J]. Acta Metall Sin, 2016 , 52(2) : 168 -176 . DOI: 10.11900/0412.1961.2015.00358

References

[1] Rettig R, Singer R F.In: Huron E S, Reed R C, Hardy M, Mills M J, Montero R E, Portella P D, Talesman J eds., Superalloys 2012, Pennsylvania: TMS, 2012: 205
[2] Pang H T, Edmonds I M, Jones C N, Stone H J, Rae C M F. In: Huron E S, Reed R C, Hardy M, Mills M J, Montero R E, Portella P D, Talesman J eds., Superalloys 2012, Pennsylvania: TMS, 2012: 301
[3] Han Y F, Ma W Y, Dong Z Q, Li S S, Gong S K.In: Reed R C, Green K A, Caron P, Gabb T P, Fahrmann M G, Huron E S, Woodard S A eds., Superalloys 2008, Pennsylvania: TMS, 2008: 91
[4] Pan Y M, Dung D S, Cragnolino G A.Metall Meter Trans, 2005; 36A: 1143
[5] Zhao S Q, Xie X S.Acta Metall Sin, 2003; 39: 399
[5] (赵双群, 谢锡善. 金属学报, 2003; 39: 399)
[6] Sun F, Zhang J X, Liu P, Feng Q, Han X D, Mao S C. J Alloys Compd, 2012; 536: 80
[7] Shi Z X, Li J R, Liu S Z.Prog Nat Sci: Mater Int, 2012; 22: 426
[8] El-Bagoury N, Mohsen Q.Phase Transitions, 2011; 84: 1108
[9] Hou J S, Guo J T, Zhou L Z, Ye H Q.Z Metallkund, 2006; 2: 174
[10] Hou J S, Zhou L Z, Yuan C, Guo J T, Wang W, Qin X Z, Liaw P K.Mater Charact, 2013; 77: 47
[11] Leclaire A D.In: Brandes E A, Brook E B eds., Smithells Metals Reference Book. Oxford: Butterworth-Heinemann, Linacre House, Jordan Hill, 1992: 131
[12] Zhou C, Gong W, Huang S, Wei H.J Min Metall, 2011; 47B: 171
[13] Cheng K Y, Jo C Y, Jin T, Hu Z Q.Mater Sci Eng, 2011; A528: 2704
[14] Mao P L, Xin Y, Han K, Wei G J.Acta Metall Sin (Engl Lett), 2009; 22: 365
[15] Cui T, Zhang Y S, Guo S, Wang L, Yang H C.Acta Metall Sin (Engl Lett), 2004; 17: 645
[16] Tian S G, Qian B J, Li T, Yu L L, Wang M G.Chin J Nonferrous Met, 2010; 20: 2154
[16] (田素贵, 钱本江, 李唐, 于莉丽, 王明罡. 中国有色金属学报, 2010; 20: 2154)
[17] Zhang B J, Wang L, Xu G H, Qin H Y, Zhao G P.J Mater Metall, 2012; 11: 136
[17] (张北江, 王磊, 胥国华, 秦鹤勇, 赵光普. 材料与冶金学报, 2012; 11: 136)
[18] Yokokawa T, Osawa M, Nishida K, Kobayashi T, Koizumi Y, Harada H.Scr Mater, 2003; 49: 1041
[19] Kobayashi T, Koizumi Y, Nakazawa S, Yamagata T, Harada H.In: Strang A, Banks W M, Conroy R D, Goulette M J eds., Proc 4th Int Charles Parsons Turbine Conference, Newcastle upon Tyne: Maney Publishing, 1997: 766
[20] Dong J X, Xie X S, Fujio Abe. J Mater Eng, 2000; (11): 15
[20] (董建新, 谢锡善, 阿部富士雄. 材料工程, 2000; (11): 15)
[21] Chen G S, Yao C C, Zhong Z Y.Acta Metall Sin, 1978; 14: 284
[21] (陈淦生, 姚常春, 仲增墉. 金属学报, 1978; 14: 284)
[22] Yeh A C, Rae C M F, Tin S. In: Green K A, Pollock T M, Harada H, Howson T E, Reed R C, Schirra J J, Walston S eds., Superalloys 2004, Warrendale: TMS, 2004: 677
[23] Divya V D, Balam S S K, Ramamurty U, Paul A.Scr Mater, 2010; 62: 621
[24] Acharya M V, Fuchs G E.Scr Mater, 2006; 54: 61
[25] Seiser B, Drautz R, Pettifor D G.Acta Mater, 2011; 59: 749
[26] Tin S, Pollock T M.Mater Sci Eng, 2003; A348: 111
[27] Monastyrskaia E V, Petrov E V, Beljaev V E, Dushkin A M.In: Green K A, Pollock T M, Harada H, Howson T E, Reed R C, Schirra J J, Walston S eds., Superalloys 2004, Warrendale: TMS, 2004: 779
[28] Karunaratne M S A, Cox D C, Carter P, Reed R C. In: Green K A, Pollock T M, Kissinger R D eds., Superalloys 2000, Warrendale: TMS, 2000: 263
[29] Darolia R, Lahrmann D F, Field R D.In: Reichman S, Dhul D N, Maurer G, Antolovich S, Lund C eds., Superalloys 1988, Warrendale: TMS, 1988: 255
[30] Erickson G L.In: Kissinger R D, Deye D J, Anton D L, Cetel A D, Nathal M V, Pollock T M, Woodford D A eds., Superalloys 1996, Warrendale: TMS, 1996: 35
[31] Walston W S, Schaeffer J C, Murphy W H.In: Kissinger R D, Deye D J, Anton D L, Cetel A D, Nathal M V, Pollock T M, Woodford D A eds., Superalloys 1996, Warrendale: TMS, 1996: 9
[32] Rae C M F, Karunaratne M S A, Small C J, Broomfield R W, Jones C N, Reed R C. In: Green K A, Pollock T M, Kissinger R D eds., Superalloys 2000, Warrendale: TMS, 2000: 767
[33] Flemings M C. Solidification Processing.New York: McGraw Hill Inc., 1974: 331
[34] Walston W S.In: Fuchs G E, Dannemann K A, Deragon T A eds., Long-Term Stability of High Temperature Materials. Warrendale, PA: TMS, 1999: 43
[35] Morinaga M, Yukawa N, Ezaki H.Philos Mag, 1995; 51A: 223
[36] Chen Q Z, Jones C N, Knowles D M.Acta Mater, 2002; 50: 1095
[37] Pyczak F, Mughrabi H.In: Morris D G, Naka S, Caron P eds., Intermetallics and Superalloys. Weinheim: Wiley-VCH, 2000: 47
[38] Keefe P W, Mancuso S O, Maurer G E.In: Antolovich S D, Stusrud R W, MacKay R A, Anton D L, Khan T, Kissinger R D, Klarstron D L eds., Superalloy 1992, Warrendale: TMS, 1992: 487
[39] Na Y S, Park N K, Reed R C.Scr Mater, 2000; 43: 585
[40] Li X, Miodownik A P, Saunders N.Mater Sci Technol, 1998; 18: 861
[41] Plati A. Master Thesis, University of Cambridge, 2003
[42] Burke J.The Kinetics of Phase Transformations in Metals. Oxford: Pergamon Press, 1965: 1
[43] Kim H T, Chun S S, Yao X X, Fang Y, Choi J.J Mater Sci, 1997; 32: 4917
[44] Moshtaghin R S, Asgari S.Mater Des, 2003; 24: 325
[45] Jackson M P, Reed R C.Mater Sci Eng, 1999; A259: 85
[46] Bryant D J, McIntosh Dr G. In: Kissinger R D, Deye D J, Anton D L, Cetel A D, Nathal M V, Pollock T M, Woodford D A eds., Superalloys 1996, Warrendale: TMS, 1996: 713
[47] Rae C M F, Reed R C.Acta Metall, 2001; 49: 4113
[48] Acharya M V, Fuchs G E.Mater Sci Eng, 2004; A381: 143
[49] Durand-Charre M.The Microstructure of Superalloys. Singapore: Gordon and Breach Science Publishers, 1997: 3
[50] Copley S M, Giamei A F, Johnson S M, Hornbeck M F.Metall Trans, 1970; 1: 2193
[51] Zhang J S, Hu Z Q, Murata Y, Morinaga M, Yukawa N.Metall Trans, 1993; 24A: 2443
Outlines

/