FRICTION STIR WELDING AND LOW-TEMPERATURE SUPERPLASTICITY OF 7B04 Al SHEET

  • Chao YANG ,
  • Jijie WANG ,
  • Zongyi MA ,
  • Dingrui NI ,
  • Mingjie FU ,
  • Xiaohua LI ,
  • Yuansong ZENG
Expand
  • 1 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
    2 College of Materials Science and Engineering, Shenyang Aerospace University, Shenyang 110036
    3 Metal Forming Technology Department, Beijing Aeronautical Manufacturing Technology Research Institute, Beijing 100024

Online published: 2016-02-22

Supported by

Supported by National Natural Science Foundation of China (No.51331008)

Abstract

Annealed 7B04 Al sheets in thickness of 2 mm were subjected to friction stir welding (FSW) under three rotation rate and welding speed parameters of 1600 r/min, 200 mm/min; 800 r/min, 200 mm/min and 400 r/min, 400 mm/min, respectively. The effect of welding parameters on the tensile property and microstructure of the FSW joints were investigated, with more efforts focusing on the low-temperature superplasticity of the nugget zones (NZs). The results showed that FSW joints with high quality could be produced by controlling welding parameters, with a joint strength coefficient of 100% being obtained. Dynamic recrystallization took place in the NZs with fine and equiaxed grains generated. The grain size of the base material was about 300 μm, while it was significantly decreased in the NZs with decreasing the rotation rate: about 2, 1 and 0.6 μm for the above three samples, respectively. The fine grain structure of the NZs could facilitate their superplastic deformation. The NZs exhibited superplastic elongations ranged from 160% to 590% at 300 ℃ at strain rates of 1×10-3 and 3×10-4 s-1. The maximum superplasticity of 790% was obtained at 350 ℃ at the strain rate of 1×10-3 s-1. The ability to superplastic deformation disappeared in the NZs at 400 ℃.

Cite this article

Chao YANG , Jijie WANG , Zongyi MA , Dingrui NI , Mingjie FU , Xiaohua LI , Yuansong ZENG . FRICTION STIR WELDING AND LOW-TEMPERATURE SUPERPLASTICITY OF 7B04 Al SHEET[J]. Acta Metall Sin, 2015 , 51(12) : 1449 -1456 . DOI: 10.11900/0412.1961.2015.00154

References

[1] Thomas W M, Nicholas E D, Needham J C, Murch M G, Temple-Smith P, Dawes C J. Great Britain Pat, 9125978.8, 1991
[2] Thomas W M, Nicholas E D, Needham J C, Murch M G, Temple-Smith P, Dawes C J. US Pat, 5460317, EPS 0616490, 1991
[3] Mishra R S, Mahoney M W. Mater Sci, 2001; 507: 357
[4] Luan G H, Guo D L, Zhang T C, Sun C B. Weld Technol, 2003; 32: 1
[4] (栾国红, 郭德伦, 张田仓, 孙成彬. 焊接技术, 2003; 32: 1)
[5] Mishra R S, Mahoney M W, McFadden S X, Mara N A, Mukherjee A K. Scr Mater, 2002; 42: 163
[6] Ma Z Y, Mishra R S, Mahoney M W. Acta Mater, 2002; 50: 4419
[7] Ma Z Y, Mishra R S, Mahoney M W, Grimes R. Mater Sci Eng, 2003; A351: 148
[8] Ma Z Y, Mishra R S. Acta Mater, 2003; 51: 3551
[9] Ma Z Y, Liu F C, Mishra R S. Acta Mater, 2010; 58: 4693
[10] Xue P, Xiao B L, Ma Z Y. Acta Mater, 2014; 50: 245
[10] (薛 鹏, 肖伯律, 马宗义. 金属学报, 2014; 50: 245)
[11] Flores O V, Kennedy C, Murr L E, Brown D, Pappu S, Nowak B M, McClure J C. Scr Mater, 1998; 38: 703
[12] Jata K V, Semiatin S L. Scr Mater, 1998; 38: 703
[13] Su J Q, Nelson T W, Mishra R S, Mahoney M. Acta Mater, 2003; 51: 713
[14] Salem H G. Scr Mater, 2003; 49: 1103
[15] Mishra R S, Mahoney M W, McFadden S X, Mara N A, Mukherjee A K. Scr Mater, 1999; 42: 163
[16] Liu F C, Ma Z Y. Scr Mater, 2008; 58: 667
[17] Mishra R S, Ma Z Y. Mater Sci Eng, 2005; R50: 1
[18] Motohashi Y, Sakuma T, Goloborodko A, Ito T, Itoh G. Mater Wissenschaft Werkstofftechnik, 2008; 39: 4
[19] Jian H G, Jiang F, Xu Z Y, Guan D K. Hot Work Technol, 2006; 35(6): 66
[19] (蹇海根, 姜 锋, 徐忠艳, 官迪凯. 热加工工艺, 2006; 35(6): 66)
[20] Liu X T, Cui J Z. Mater Rev, 2005; 19(3): 47
[20] (刘晓涛, 崔建忠. 材料导报, 2005; 19(3): 47)
[21] Wang M, Zhang H J, Zhang J B, Zhang X, Yang L. Mater Eng Perform, 2014; 23: 1881
[22] Wang Y H, Chen Y H, Huang C P, Ke L M. Hot Work Technol, 2012; 41(15): 161
[22] (王运会, 陈玉华, 黄春平, 柯黎明. 热加工工艺, 2012; 41(15): 161)
[23] Charit I, Mishra R S. Acta Mater, 2005; 53: 4211
[24] Ren S R, Ma Z Y, Chen L Q, Zhang Y Z. Acta Metall Sin, 2007; 43: 225
[24] (任淑荣, 马宗义, 陈礼清, 张玉政. 金属学报, 2007; 43: 225)
[25] Liu F C, Ma Z Y. Acta Metall Sin, 2008; 44: 319
[25] (刘峰超, 马宗义. 金属学报, 2008; 44: 319)
[26] Pu H P, Liu F C, Huang J C. Metall Mater Trans, 1995; 26: 1153
[27] Ma Z Y, Mishra R S. Friction Stir Superplasticity for Unitized Structures. Chapter 4, Netherlands: Elsevier, 2014: 19
Outlines

/

〈 〉