Orginal Article

MICROSTRUCTURE, HARDNESS AND ELECTRICAL RESISTIVITY OF DIRECTIONALLY SOLIDIFIEDCu-6%Ag ALLOY UNDER A TRANSVERSE MAGNETIC FIELD

  • Xiaowei ZUO ,
  • Rui GUO ,
  • Bailing AN ,
  • Lin ZHANG ,
  • Engang WANG
Expand
  • Key Laboratory of Electromagnetic Processing of Materials (Ministry of Education), Northeastern University, Shenyang 110819, China

Received date: 2015-05-26

  Online published: 2015-12-02

Supported by

Supported by National Natural Science Foundation of China (Nos.51474066 and 51004038), National High Technology Research and Development Program of China (No2007AA03Z519), Special Research Fund for Doctoral Disciplines Program of Chinese Higher Education (No.2012004211008) and Programme of Introducing Talents of Discipline to Universities of China (NoB07015)

Abstract

Cu-Ag material with excellent combination of high strength and high conductivity is an important conductor for both direct current resistive and pulsed high-field magnets. The strength and electrical conductivity of Cu-Ag microcomposite are closely related to the microstructure of proeutectic Cu because of its high volume fraction. The morphology of proeutectic Cu, Ag precipitation and concentration of Ag in Cu can be controlled by application of external field and the addition of the third elements. In this work, the microstructural evolution, concentration contributions, the resulting microhardness and electrical resistivity of Cu-6%Ag alloy, which was directionally solidified under a transverse magnetic field were studied. The effect of the magnetic field on the microstructure was analyzed by OM, SEM, TEM and EDS. The results demonstrate that in macro scales, the growth direction of columnar grains is gradually deflected along the axial and heating flow directions with increasing magnetic field intensity. In micro scales, the increasing magnetic field increases both the primary dendrite arm spacing and volume fraction of proeutectic Cu, and traps more supersaturated Ag in proeutectic Cu. No obvious effect on the secondary dendrite arm spacing of proeutectic Cu is observed. In nano scales, SAED pattern in TEM indicates a small quantity of fine nanostructured Ag precipitations in proeutectic Cu. A relationship among the primary dendrite arm spacing, external magnetic field intensity and the initial diffusion coefficient in liquid was established from the viewpoint of suppressed convection by the magnetic field. The increased supersaturated Ag in proeutectic Cu is thought to be caused by the influence of magnetic field on the solute redistribution coefficient. The changes of microstructure induced by magnetic field result in the increases of the microhardness and electrical resistivity in Cu-6%Ag alloy. A model was proposed to clarify the changes of electrical resistivity in terms of the resistivity of Cu matrix, the impurity-scattering resistivity from dissolved Ag in Cu and the scattering resistivity from vacancy, where the interface-scattering resistivity from precipitation of Ag is assumed to be ruled out. The result shows that the impurity-scattering resistivity from dissolved Ag in Cu, which is increased by the application of external magnetic field, plays an important role in determining the overall resistivity of the alloy.

Cite this article

Xiaowei ZUO , Rui GUO , Bailing AN , Lin ZHANG , Engang WANG . MICROSTRUCTURE, HARDNESS AND ELECTRICAL RESISTIVITY OF DIRECTIONALLY SOLIDIFIEDCu-6%Ag ALLOY UNDER A TRANSVERSE MAGNETIC FIELD[J]. Acta Metall Sin, 2016 , 52(2) : 143 -150 . DOI: 10.11900/0412.1961.2015.00279

References

[1] Davy C A, Ke H, Kalu P N, Bole S T.IEEE Trans Appl Supercond, 2008; 18: 560
[2] Han K, Toplosky V, Goddard R, Lu J, Niu R, Chen J.IEEE Trans Appl Supercond, 2011; 22: 6900204
[3] Sakai Y, Schneider-Muntau H J.Acta Mater, 1997; 45: 1017
[4] Sakai Y, Inoue K, Asano T, Wada H, Maeda H.Appl Phys Lett, 1991; 59: 2965
[5] Han K, Vasquez A A, Xin Y, Kalu P N.Acta Mater, 2003; 51: 767
[6] Han K, Embury J D, Sims J R, Campbell L J, Schneider-Muntau H J, Pantsyrnyi V I, Shikov A, Nikulin A,Vorobieva A.Mater Sci Eng, 1999; A267: 99
[7] Morris D G, Benghalem A, Morris-Munoz M A.Scr Mater, 1999; 41: 1123
[8] Zuo X W, Han K, Zhao C C, Niu R M, Wang E G.Mater Sci Eng, 2014; A619: 319
[9] Zuo X W, Zhao C C, Wang E G, Zhang L, Han K, He J C.J Low Temp Phys, 2013; 170: 409
[10] Zuo X W, Zhao C C, Niu R M, Wang E G, Han K.J Mater Process Technol, 2015; 224: 208
[11] Liu J B, Zhang L, Meng L.Acta Metall Sin, 2006; 42: 937
[11] (刘嘉斌, 张雷, 孟亮. 金属学报, 2006; 42: 937)
[12] Liu J B, Meng L.Acta Metall Sin, 2006; 42: 931
[12] (刘嘉斌, 孟亮. 金属学报, 2006; 42: 931)
[13] Piyawit W, Xu W Z, Mathaudhu S N, Freudenberger J, Rigsbee J M, Zhu Y T.Mater Sci Eng, 2014; A610: 85
[14] Bittner F, Yin S, Kauffmann A, Freudenberger J, Klauss H, Korpala G, Kawalla R, Schillinger W, Schultz L.Mater Sci Eng, 2014; A597: 139
[15] Tian Y Z, Freudenberger J, Pippan R, Zhang Z F.Mater Sci Eng, 2013; A568: 184
[16] Lehmann P, Moreau R, Camel D, Bolcato R.J Cryst Growth, 1998; 183: 690
[17] Zuo X W, Wang E G, Han H, Zhang L, He J C.Acta Metall Sin, 2008; 44: 1219
[17] (左小伟, 王恩刚, 韩欢, 张林, 赫冀成. 金属学报, 2008; 44: 1219)
[18] Wang C J, Wang Q, Wang Y Q, Huang J, He J C.Acta Phys Sin, 2006; 55: 648
[18] (王春江, 王强, 王亚勤, 黄剑, 赫冀成. 物理学报, 2006; 55: 648)
[19] Li X, Fautrelle Y, Ren Z M.Acta Mater, 2007; 55: 3803
[20] Li X, Fautrelle Y, Ren Z M.Acta Mater, 2008; 56: 3146
[21] Li X, Fautrelle Y, Ren Z M, Gagnoud A, Moreau R, Zhang Y D, Esling C.Acta Mater, 2009; 57: 1689
[22] Li G M, Wang E G, Zhang L, Zuo X W, He J C.Acta Metall Sin, 2010; 46: 1128
[22] (李贵茂, 王恩刚, 张林, 左小伟, 赫冀成. 金属学报, 2010; 46: 1128)
[23] Li G M, Liu Y, Su Y, Wang E G, Han K.China Foundry, 2013; 10: 162
[24] Li G M, Wang E G, Zhang L, Zuo X W, He J C.Rare Met Mater Eng, 2012; 41: 701
[24] (李贵茂, 王恩刚, 张林, 左小伟, 赫冀成. 稀有金属材料与工程, 2012; 41: 701)
[25] Hunt J R.Solidification and Casting of Metals. London: The Metal Society, 1979: 3
[26] Kurz W, Fisher D J.Acta Metall, 1981; 29: 11
[27] Trivedi R.Metall Trans, 1984; 15A: 977
[28] Hu H Q.Solidification Principle of Metal. 2nd Ed., Beijing: China Machine Press, 2000: 112
[28] (胡汉起. 金属凝固原理. 第2版, 北京: 机械工业出版社, 2000: 112)
[29] Botton V, Lehmann P, Bolcato R, Moreau R, Haettel R.Int J Heat Mass Transf, 2001; 44: 3345
[30] Gaganov A, Freudenberger J, Botcharova E, Schultz L.Mater Sci Eng, 2006; A437: 313
Outlines

/

〈 〉