Orginal Article

EFFECT OF DISSOLVED OXYGEN IN STEAM ON THE CORROSION BEHAVIORS OF ZIRCONIUM ALLOYS

  • Tianguo WEI ,
  • Jiankang LIN ,
  • Chongsheng LONG ,
  • Hongsheng CHEN
Expand
  • 1 Science and Technology on Reactor Fuel and Materials Laboratory, Nuclear Power Institute of China, Chengdu 610213, China
    2 Fujian Fuqing Nuclear Power Co. Ltd., Fuqing 350318, China

Received date: 2015-04-14

  Online published: 2015-11-24

Supported by

Supported by National Natural Science Foundation of China (No.51171175)

Abstract

Advanced boiling water reactors (ABWRS) show optimistic application prospect in the future. However, in these reactors, influence of dissolved oxygen (DO) on the corrosion rate of zirconium fuel claddings should be seriously considered. In this work, the effect of the dissolved oxygen (DO) on the corrosion behaviors of Zr-4, N18 (Zr-1.0Sn-0.3Nb -0.3Fe-0.1Cr) and N36 (Zr-1.0Sn-1.0Nb-0.3Fe) alloys in 400 ℃ and 10.3 MPa steam was investigated. A recirculation loop was used to control the DO level at about 0.1×10-6 and 1.0×10-6, respectively. The results showed that, under the two DO level conditions, N18 had almost the same weight gain as Zr-4 after exposure for 90 d, and N36 had the highest weight gain. In the initial period of the corrosion test, the three alloys had lower weight gain under higher DO level condition. With the increase of exposure time, the weight gain under 1.0×10-6 DO level exceeded gradually the weight gain under 0.1×10-6 level for each alloy, and the time needed for exceeding was significantly shorter for the alloy with higher Nb content.

Cite this article

Tianguo WEI , Jiankang LIN , Chongsheng LONG , Hongsheng CHEN . EFFECT OF DISSOLVED OXYGEN IN STEAM ON THE CORROSION BEHAVIORS OF ZIRCONIUM ALLOYS[J]. Acta Metall Sin, 2016 , 52(2) : 209 -216 . DOI: 10.11900/0412.1961.2015.00219

References

[1] Cox B.J Nucl Mater, 2005; 336: 331
[2] Zhou B X, Yao M Y, Li Z K, Wang X M, Zhou J, Long C S, Liu Q, Luan B F.J Mater Sci Technol, 2012; 28: 606
[3] Bojinov M, Karastoyanov V, Kinnunen P, Saario T.Corros Sci, 2010; 52: 54
[4] Kumar M K, Aggarwal S, Kain V, Saario T, Bojinov M.Nucl Eng Des, 2010; 240: 985
[5] Cox B, Garzarolli F, Rudling P.Corrosion of Zr-Nb Alloys, Zirat-9 Specialtopics Report, Advanced Nuclear Technology International, Ekbaken 33, SE-735, 35, SURAHAMMAR, Sweden, September, 2004
[6] Kumar M K, Aggarwal S, Beniwal D, Dey A K, Singh H, Kain V.Mater Corros, 2014; 65: 244
[7] Allen T R, Konings R J M, Motta A T.Compr Nucl Mater, 2012; 5: 49
[8] Yan Y H, Gao Z Y.Nucl Power Eng, 1997; 18(1): 12
[8] (严育华, 高祖瑛. 核动力工程, 1997; 18(1): 12)
[9] Liu X R, Chen Z Q, Hou Z S.Shangdong Elec Power, 1996; (5): 46
[9] (刘信荣, 陈志奇, 侯忠松. 山东电力技术, 1996; (5): 46)
[10] Zhang H X.PhD Dissertation, Xi'an Jiaotong University, 2009
[10] (章海霞. 西安交通大学博士学位论文, 2009)
[11] Yao M Y, Zhou B X, Li Q, Xia S, Liu W Q.Shanghai Met, 2008; 30(6): 1
[11] (姚美意, 周邦新, 李强, 夏爽, 刘文庆. 上海金属, 2008; 30(6): 1)
[12] Yao M Y, Li S L, Zhang X, Peng J C, Zhou B X, Zhao X S, Shen J Y.Acta Metall Sin, 2011; 47: 865
[12] (姚美意, 李士炉, 张欣, 彭剑超, 周邦新, 赵旭山, 沈剑韵. 金属学报, 2011; 47: 865)
[13] Zhang H X, Fruchart D, Hlil E K, Ortega L, Li Z K, Zhang J J, Sun J, Zhou L.J Nucl Mater, 2010; 396: 65
[14] Ni N, Lozano-Perez S, Sykes J, Grovenor C.Ultramicroscopy, 2011; 111: 123
[15] Ni N, Hudson D, Wei J, Wang P, Lozano-Perez S, Smith G D W, Sykes J M, Yardley S S, Moore K L, Lyon S, Cottis R, Preuss M, Grovenor C R M.Acta Mater, 2012; 60: 7132
[16] Li Z K, Zhou L, Li P Z, Zhang J J, Xue X Y, Song Q Z.Rare Met Mater Eng, 1999; 28: 380
[16] (李中奎, 周廉, 李佩志, 张建军, 薛祥义, 宋启忠. 稀有金属材料与工程, 1999; 28: 380)
[17] Zhao W J, Miao Z, Jiang Y R, Jiang H M, Zhou B X.Rare Met, 2000; 24: 150
[17] (赵文金, 苗志, 蒋有荣, 蒋宏曼, 周邦新. 稀有金属, 2000; 24: 150)
[18] Parise M, Sicardy O, Cailletaud G.J Nucl Mater, 1998; 256: 35
[19] Tejland P, Andren H O.J Nucl Mater, 2012; 430: 64
[20] Baek J H, Jeong Y H, Kim I S.J Nucl Mater, 2000; 280: 235
[21] Jeong Y H, Kim H G, Kim T H.J Nucl Mater, 2003; 317: 1
[22] Kim H G, Park J Y, Jeong Y H.J Nucl Mater, 2005; 347: 140
[23] Proff C, Abolhassania S, Lemaignan C.J Nucl Mater, 2013; 432: 222
Outlines

/

〈 〉