MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Fe-C-Cu POWDER-FORGED CONNECTING ROD
Received date: 2015-09-16
Online published: 2015-10-29
Supported by
Supported by National Natural Science Foundation of China (No.51321003)
Powder-forged (P/F) connecting rods have been widely used due to their advantages of high strength, less machining, light weight, and consistency etc.. Currently, P/F connecting rods were only supplied by GKN in Britain and Metaldyne in US in commercial quantities. In this work, the microstructure and mechanical properties of the P/F Fe-C-Cu automobile engine connecting rods (H16) were designed and manufactured domestically, and the factors affecting the fatigue performance were systematically analyzed. The Measured results indicate that the density of the connecting rod is greater than 7.80 g/cm3. Microstructure observation showed that there were no oxide penetrations or network near or at rod surface and the surface decarburization layer is thinner than 70 mm. Anisotropy at different locations inside the P/F connecting rod was revealed. Furthermore, the bending of connecting rods was found to affect the fatigue performance significantly. The microstructure and the surface shot-peening condition had certain influence on the sites of fatigue crack initiation. Most importantly, the fatigue strength of H16 P/F connecting rod was found to be superior to that of the wrought steel-forged connecting rod (C70), and similar to that of P/F connecting rods designed and manufactured by entities.
Key words: powder-forging; connecting rod; tensile strength; fatigue limit; microstructure
Linna BAI , Fuping LIU , Sui WANG , Feng JIANG , Jun SUN , Liangbin CHEN , WANG , Fengyuan . MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Fe-C-Cu POWDER-FORGED CONNECTING ROD[J]. Acta Metall Sin, 2016 , 52(1) : 41 -50 . DOI: 10.11900/0412.1961.2015.00486
| [1] | Capus J. Met Powder Rep, 2014; 69: 31 |
| [2] | Ilia E, Tutton K O, Neill M. Met Powder Rep, 2005; 60: 38 |
| [3] | Guo B, Ge C C, Zhang S C, Zhang Y. Powder Metall Ind, 2011; 21(3): 45 |
| [3] | (郭 彪, 葛昌纯, 张随财, 张 宇. 粉末冶金工业, 2011; 21(3): 45) |
| [4] | Afzal A. Master Thesis, University of Toledo, USA, 2004 |
| [5] | Dinu D, Lapp M T. SAE Tech Paper, 2006; 01: 0894 |
| [6] | Hanke W, Buschbeck R, Letourneau S, Sinclair D, Skiadas A, Urabe M, Takiguchi M. SAE Tech Paper, 2009; 01: 1958 |
| [7] | Bao X P, Tan X Y, Liu S D, Le P. Light Vehicles, 2009; 236: 20 |
| [7] | (包雪鹏, 谭晓园, 刘善德, 乐 萍. 轻型汽车技术, 2009; 236: 20) |
| [8] | Ilia E, Lanni G, Xin J, Yan R, Zung E. Trans Csice, 2008; 26: 463 |
| [8] | (Ilia E, Lanni G, 辛 军, Yan R, Zung E. 内燃机学报, 2008; 26: 463) |
| [9] | Williams B. Met Powder Rep, 2004; 59: 14 |
| [10] | Guo B, Ge C C, Yan Y N, Zhang S C, Yu B J. Mater Rev, 2012; 26(7)B: 141 |
| [10] | (郭 彪, 葛昌纯, 颜永年, 张随财, 余本军. 材料导报, 2012; 26(7)B: 141) |
| [11] | Guo B, Ge C C, Yan Y N, Zhang S C, Yu B J. Hot Work Technol, 2012; 41(18): 64 |
| [11] | (郭 彪, 葛昌纯, 颜永年, 张随财, 余本军. 热加工工艺, 2012; 41(18): 64) |
| [12] | Wang J L, Chen Z, Chen H. J Changchun Univ Technol, 2005; 26(1): 61 |
| [12] | (王佳玲, 陈 卓, 陈 华. 长春工业大学学报, 2005; 26(1): 61) |
| [13] | Wang J X, Guo C M, Zhu Z Y, Yin Z M, Zhou K Z, Li Z Y. Mater Sci Eng Powder Metall, 2006; 11(1): 19 |
| [13] | (王继新, 郭昌明, 朱志远, 尹志民, 周科朝, 李智友. 粉末冶金材料科学与工程, 2006; 11(1): 19) |
| [14] | Zhou M Z, Li P, Xue K M. J Plast Eng, 2005; 12(6): 11 |
| [14] | (周明智, 李 萍, 薛克敏. 塑性工程学报, 2005; 12(6): 11) |
| [15] | Tu T S, Lin D W. Met Forming Technol, 2001; 19(2): 4 |
| [15] | (屠挺生, 林大为. 金属成形工艺, 2001; 19(2): 4) |
| [16] | Zhao W B. PhD Dissertation, South China University of Technology, Guangzhou, 2005 |
| [16] | (赵伟斌. 华南理工大学博士学位论文, 广州, 2005) |
| [17] | Wang C L. In: PM Branch of SCS Ed., The 20th Anniversary Corpus of PM Branch of SCS, Beijing: CMPMA, 2010: 104 |
| [17] | (王崇琳. 中国钢结构协会粉末冶金分会 编. 粉末冶金产业技术创新战略联盟论坛暨中国钢协机协粉末冶金协会二十周年纪念文集, 北京: 中国机械通用零部件工业协会粉末冶金专业协会, 2010: 104) |
| [18] | Guo B. PhD Dissertation, Southwest Jiaotong University, Chengdu, 2008 |
| [18] | (郭 彪. 西南交通大学博士学位论文, 成都, 2008) |
| [19] | Li P. Auto Technol Mater, 2010; (1): 42 |
| [19] | (李 鹏. 汽车工艺与材料, 2010; (1): 42) |
| [20] | Han F L. Adv Mater Ind, 2005; (11): 55 |
| [20] | (韩凤麟. 新材料产业, 2005; (11): 55) |
| [21] | Hong S Z. J Netshape Forming Eng, 2011; (3): 47 |
| [21] | (洪慎章. 精密成形工程, 2011; (3): 47) |
| [22] | Wang Y K, Peng M G. Met Mater Metall Eng, 2007; 35(5): 57 |
| [22] | (王云坤, 彭茂公. 金属材料与冶金工程, 2007; 35(5): 57) |
| [23] | Han F L. Powder Metall Ind, 2011; 21(4): 1 |
| [23] | (韩凤麟. 粉末冶金工业, 2011; 21(4): 1) |
| [24] | Engstrom U. Int J Powder Metall, 2003; 39: 29 |
| [25] | Han F L. Powder Metall Ind, 2014; 24(4): 1 |
| [25] | (韩凤麟. 粉末冶金工业, 2014; 24(4): 1) |
| [26] | Haerian A H, Khaki J V, Mashhadi H A. IJE Trans, 2004; 6B: 81 |
| [27] | Tang R Z,Tian R Z. Binary Alloy Phase Diagrams and Crystal Structure of Intermediate Phase. Changsha: Central South University Press, 2009: 126 |
| [27] | (唐仁政,田荣璋. 二元合金相图及中间相晶体结构. 长沙: 中南大学出版社, 2009: 126) |
| [28] | Jang X D, Liu Z L, Zou D H, Liu B L. Mater Mech Eng, 2012; 36(4): 46 |
| [28] | (蒋晓冬, 刘子利, 邹德华, 刘伯路. 机械工程材料, 2012; 36(4): 46) |
/
| 〈 |
|
〉 |