RESEARCH ON MORPHOLOGY EVOLUTION OF PRIMARY PHASE IN SEMISOLID A356 ALLOY UNDER CHAOTIC ADVECTION
Received date: 2015-04-20
Online published: 2015-10-16
Supported by
Supported by National Natural Science Foundation of China (Nos.51144009 and 51361012), Natural Science Foundation of Jiangxi Province (No.20142bab206012) and Science and Technology Program of the Education Department of Jiangxi Province (NoGJJ14407)
Chaotic advection could be strengthened mix, mass transfer and heat transfer in the viscous fluid, the melt flow forming was affected by electromagnetic field in the metal solidification process, so were the macro and microstructure of materials. So it was necessary to study chaotic characteristics of semisolid Al alloy in the electromagnetic field. The characterization of chaotic convention and morphology of primary phase were mainly researched in semisolid A356 alloy under the electromagnetic field. The trajectories of the particle in semisolid A356 alloy melt was simulated by the computational fluid dynamics software Fluent, the Kolmogorov entropy and fractal dimension of the flow trajectories of semisolid A356 alloy melt were judged and analyzed. The results showed that chaotic advection may happen in semisolid alloy melt under electromagnetic field. Combined with experiment, the results of process parameters and different current frequencies were compared. The results showed that the primary phase with 59.86 μm in average equal-area circle diameter, 0.71 in average shape factor, 6829.5 nat/s of Kolmogorov entropy and 2.2439 of fractal dimension can be obtained in semisolid A356 alloy with pouring 650 ℃, stirring for 15 s at 30 Hz, and holding at 590 ℃ for 10 min. Meanwhile, the morphology of primary phase can be observed with the best parameters.
Zheng LIU , Jiayi ZHANG , Haolin LUO , Keyue DENG . RESEARCH ON MORPHOLOGY EVOLUTION OF PRIMARY PHASE IN SEMISOLID A356 ALLOY UNDER CHAOTIC ADVECTION[J]. Acta Metall Sin, 2016 , 52(2) : 177 -183 . DOI: 10.11900/0412.1961.2015.00228
| [1] | Lin X, Tong L L, Zhao L N, Wang L N, Wang M, Huang W D.Trans Nonferrous Met Soc China, 2010; 20: 826 |
| [2] | Zhao L N, Lin X, Huang W D.Acta Metall Sin, 2011; 47: 403 |
| [2] | (赵力宁, 林鑫, 黄卫东. 金属学报, 2011; 47: 403) |
| [3] | Xu J F, Wei B B.Acta Phys Sin, 2004; 53: 1909 |
| [3] | (徐锦峰, 魏炳波. 物理学报, 2004; 53: 1909) |
| [4] | Nikrityuk P A, Eckert K, Grundmann R.Int J Heat Mass Trans, 2006; 49: 1501 |
| [5] | Nikrityuk P A, Ungarish M, Eckert K, Grundmann R.Phys Fluids, 2005; 17: 101 |
| [6] | Pan Y, Zhang C Y.Acta Metall Sin, 2001; 37: 1035 |
| [6] | (潘冶, 张春燕. 金属学报, 2001; 37: 1035) |
| [7] | Campanella T, Charbon C, Rappaz M.Metall Mater Trans, 2004; 35A: 3201 |
| [8] | Zhao J Z, Li H L, Zhao L.Acta Metall Sin, 2009; 45: 1435 |
| [8] | (赵九洲, 李海丽, 赵雷. 金属学报, 2009; 45: 1435) |
| [9] | Gao S Y, Le Q C, Zhang Z Q, Cui J Z.Bull Mater Sci, 2012; 35: 651 |
| [10] | Eckert S, Nikrityuk P A, Willers B, Räbiger D, Shevchenko N, Neumann H H.Eur Phys J Spec Topics, 2013; 220: 123 |
| [11] | Poole G M, Heyen M, Nastac L, El-Kaddah N.Metall Mater Trans, 2014; 45B: 1834 |
| [12] | Aref H.J Fluid Mech, 1984; 143: 21 |
| [13] | Arratic P E, Muzzio F J.Ind End Chem Res, 2004; 43: 6557 |
| [14] | Bresler L, Shinbrot T, Metcalfe G, Ottino J M.Chem Eng Sci, 1997; 52: 1623 |
| [15] | Lu G M, Zhao D Z, Wang P, Cui J Z.J Northeastern Univ (Nat Sci), 2007; 28: 353 |
| [15] | (路贵民, 赵大志, 王平, 崔建忠. 东北大学学报(自然科学版), 2007; 28: 353) |
| [16] | Tao W Y, Zhao S D, Lin W J.J Mech Eng, 2012; 48(14): 50 |
| [16] | (陶文毓, 赵升吨, 林文捷. 机械工程学报, 2012; 48(14): 50) |
| [17] | Sun K H, He S B, He Y, Yin L Z.Acta Phys Sin, 2013; 62: 1 |
| [17] | (孙克辉, 贺少波, 何毅, 尹林子. 物理学报, 2013; 62: 1) |
| [18] | Zhu Y Z, Yi S H, Kong X P.Acta Phys Sin, 2015; 64: 701 |
| [18] | (朱杨柱, 易仕和, 孔小平. 物理学报, 2015; 64: 701) |
| [19] | Zheng G B, Jin N D.Acta Phys Sin, 2009; 58: 4485 |
| [19] | (郑桂波, 金宁德. 物理学报, 2009; 58: 4485) |
| [20] | Schouten J C, Takens F, van den Bleek C M.Phys Rev, 1994; 49E: 126 |
| [21] | Wang Z F, Wang Z H.Chin J Comput, 2012; 35: 364 |
| [21] | (王中锋, 王志海. 计算机学报, 2012; 35: 364) |
| [22] | Falconer K J.Math Proc Camb Phil Soc, 1988; 103: 339 |
| [23] | Li S G.Fractals. Beijing: Higher Education Press, 2004: 55 |
| [23] | (李水根. 分形. 北京:高等教育出版社, 2004: 55) |
| [24] | Liu Z H, Sun R X, Wang Y D.Ciesc J, 2014; 65: 3340 |
| [25] | Fan Z, Chen J Y.Mater Sci Technol, 2002; 18: 258 |
| [26] | Liu F F, Yang C J, Su Q, Wang D H, Zhang Y Z.J Mech Eng, 2010; 46(19): 24 |
| [27] | Yang X W, Zhu J C, He D.Trans Nonferrous Met Soc China, 2013; 23: 1442 |
/
| 〈 |
|
〉 |