ADVANCES IN SOLIDIFICATION CHARACTERISTICS AND TYPICAL CASTING DEFECTS IN NICKEL-BASED SINGLE CRYSTAL SUPERALLOYS

  • Jun ZHANG ,
  • Taiwen HUANG ,
  • Lin LIU ,
  • Hengzhi FU
Expand
  • State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072

Online published: 2015-09-07

Supported by

Supported by National High Technology Research and Development Program of China (No.2012AA03A511), National Natural Science Foundation of China (Nos.51331005 and 50931004), National Basic Research Program of China (No.2011CB610406) and NPU Foundation for Fundamental Research (No.2014JM62270)

Abstract

Single crystal (SC) superalloy is a kind of complex structure and multi phase materials. With the increase of the degree of alloying and the content of refractory elements, or the more complicated structure and larger size of the casting made of SC superalloy, it is essential important to suppress the formation of solidification defects to improve the quality and performance of the blades. The microstructure and solidification defects of single crystal alloy are not only related to the composition of the alloy, but also depend on its solidification characteristics and technological conditions. The paper first summarizes the research progress of the solidification characteristics for advanced SC superalloys, focusing on analysis of the effects of solidification characteristics and processing parameters on the formation and its mechanics for two typical directional solidification defects, crystallographic orientation deviation and stray grains. Then some methods and approaches to suppress such defect formation for complex single crystal blade have been reviewed.

Cite this article

Jun ZHANG , Taiwen HUANG , Lin LIU , Hengzhi FU . ADVANCES IN SOLIDIFICATION CHARACTERISTICS AND TYPICAL CASTING DEFECTS IN NICKEL-BASED SINGLE CRYSTAL SUPERALLOYS[J]. Acta Metall Sin, 2015 , 51(10) : 1163 -1178 . DOI: 10.11900/0412.1961.2015.00448

References

[1] Reed R C, Tao T, Warnken N. Acta Mater, 2009; 57: 5898
[2] Biavette D, Caron P, Khan T. Scr Metall, 1986; 20: 1395
[3] Mottura A, Wu R T, Finnis M W, Reed R C. Acta Mater, 2008; 56: 2669
[4] Tin S, Pollock T M. J Propul Power, 2006; 22: 361
[5] Tryon B, Feng Q, Pollock T M. Intermetallics, 2004; 12: 957
[6] Feng Q, Nandy T K, Pollock T M. Scr Mater, 2004; 50: 849
[7] D'Souza N, Dong H B. Scr Mater, 2007; 56: 41
[8] Zheng Y R. Acta Metall Sin, 1986; 22: 119 (郑运荣. 金属学报, 1986; 22: 119)
[9] Reed R C. The Superalloys: Fundamentals and Applications. New York: Cambridge University Press, 2006: 1
[10] Murakami H, Honma T, Koizumi Y, Harada H. In: Pollock T M, Kissinger R D, Bowman R R eds., Superalloy 2000, Warrendale: TMS, 2000: 747
[11] Kearsey R M, Beddoes J C, Jones P, Au P. Intermetallics, 2004; 12: 903
[12] Feng Q, Nandy T K, Tin S, Pollock T M. Acta Mater, 2003; 51: 269
[13] Heckl A, Rettig R, Singer R F. Metall Mater Trans, 2010; 41A: 202
[14] Hobbs R A, Tin S, Rae C M F, Broomfield R W, Humphreys C J. In: Green K A, Pollock T M, Harada H eds., Superalloys 2004, Warrendale: TMS, 2004: 819
[15] Liu G, Liu L, Zhao X B, Ge B M, Zhang J, Fu H Z. Metall Mater Trans, 2011; 42A: 2733
[16] Caldwell E C, Fela F J, Fuchs G E. In: Green K A, Pollock T M, Harada H eds., Superalloys 2004, Warrendale: TMS, 2004: 811
[17] Liu L R, Jin T, Zhao N R, Wang Z H. Mater Lett, 2004; 58: 2290
[18] Al-Jarba K A. PhD Dissertation, University of Florida, USA, 2003
[19] Hu Q, Liu L, Zhao X B, Gao S F, Zhang J, Fu H Z. Trans Nonferrous Met Soc China, 2013; 23: 3257
[20] Kearsey R M. PhD Dissertation, Carleton University, Canada, 2004
[21] Hobbs R A, Tin S, Rae C M F. Metall Mater Trans, 2005; 36A: 2761
[22] Tin S, Pollock T M. Mater Sci Eng, 2003; A348: 111
[23] Zheng L, Li S S, Xiao C B, Tang D Z, Gu C Q. Key Eng Mater, 2007; 353-358: 507
[24] Zhang J, Lou L H. J Mater Sci Technol, 2007; 23: 289
[25] Jiao S, Zhang J, Jin T, Wang C S, Wang H F, Liu L, Fu H Z. Rare Met Mater Eng, 2013; 42: 1028 (焦 莎, 张 军, 金 涛, 王常帅, 王海峰, 刘 林, 傅恒志. 稀有金属材料与工程, 2013; 42: 1028)
[26] Seth Brij B. In: Pollock T M, Kissrnger R D, Bowman R R, Gree K A, McLean M, Olson S, Schirra J J eds., Superalloys 2000, Warrendale: TMS, 2000: 3
[27] Gao S F, Liu L, Wang N, Zhao X B, Zhang J, Fu H Z. Metall Mater Trans, 2012; 43A: 3767
[28] Gao S F, Liu L, Wang N, Zhao X B, Zhang J, Fu H Z. Mater Sci Technol, 2011; 27: 1783
[29] Dai H J, Dong H B, D'Souza N. Metall Mater Trans, 2011; 42A: 3439
[30] Esaka H, Shinozuka K, Tamura M. Mater Sci Eng, 2005; A413-414: 151
[31] Zhang X Y. Master Thesis, Northwestern Polytechnical University, Xi'an, 2013 (张晓越. 西北工业大学硕士学位论文, 西安, 2013)
[32] Zhou Y Z, Volek A, Green N R. Acta Mater, 2008; 56: 2631
[33] Zhang X L, Zhou Y Z, Jin T, Sun X F, Liu L. J Mater Sci Technol, 2013; 29: 879
[34] Jiao J J. Master Thesis, Northwestern Polytechnical University, Xi'an, 2015 (焦娟娟. 西北工业大学硕士学位论文, 西安, 2015)
[35] Stanford N, Djakovic A, Shollock B A, McLean M, Souza N D, Jennings P. In: Green K A, Pollock T M, Harada H eds., Superalloys 2004, Warrendale: TMS, 2004: 719
[36] Stanford N, Djakovic A, Shollock B A, McLean M. Scr Mater, 2004; 50: 159
[37] Chen X Z. Master Thesis, Northwestern Polytechnical University, Xi'an, 2014 (陈先州. 西北工业大学硕士学位论文, 西安, 2014)
[38] de Bussac A, Gandin C A. Mater Sci Eng, 1997; A237: 35
[39] Rappaz M, Gandin C A, Desbiolles J L. Metall Mater Trans, 1996; 27A: 695
[40] Napolitano R E, Schaefer R J. Mater Sci, 2000; 35: 1641
[41] Meyer T V, Dedecke D, Paul U, Sahm P R. In: Kissinger R D, Deye D J, Anton D L, Cetel A D, Nathal M V, Pollock T M, Woodford D A eds., Superalloys 1996, Warrendale: TMS, 1996: 471
[42] Zhang X L, Zhou Y Z, Jin T, Sun X F. Acta Metall Sin, 2012; 48: 1229 (张小丽, 周亦胄, 金 涛, 孙晓峰. 金属学报, 2012; 48: 1229)
[43] Meng X B, LI J G, Chen Z Q. Metall Mater Trans, 2013; 44A: 1955
[44] Yang X L, Ness D, Lee P D, Souza N D. Mater Sci Eng, 2005; A413: 571
[45] Tin S, Pollock T M. Metall Mater Trans, 2003; 34A: 1953
[46] Gu J P, Beckermann C, Giamei A F. Metall Mater Trans, 1997; 28A: 1533
[47] Lu Y Z, Wang D W, Zhang J, Lou L H. Foundry, 2009; 58: 245 (卢玉章, 王大伟, 张 健, 楼琅洪. 铸造, 2009; 58: 245)
[48] Gao S F. PhD Dissertation, Northwestern Polytechnical University, Xi'an, 2012 (高斯峰. 西北工业大学博士学位论文, 西安, 2012)
[49] Chen C. Master Thesis, Northwestern Polytechnical University, Xi'an, 2013 (陈 纯. 西北工业大学硕士学位论文, 西安, 2013)
[50] Huang T W, Liu L, Zhang W G, Zhang J, Fu H Z. Acta Metall Sin, 2009; 45: 1225 (黄太文, 刘 林, 张卫国, 张 军, 傅恒志. 金属学报, 2009; 45: 1225)
[51] Ma D X, Bührig-Polaczek A. Metall Mater Trans, 2009; 40B: 738
[52] Ma D X, Zhou B, Bührig-Polaczek A. Adv Mater Res, 2011; 278: 306
[53] Xuan W D, Ren Z M, Ren W L, Yu J B, Chen C. J Iron Steel Res, 2011; 23: 369 (玄伟东, 任忠鸣, 任维丽, 余建波, 陈 超. 钢铁研究学报, 2011; 23: 369)
[54] Yang X L, Ness D, Lee P D. Mater Sci Eng, 2005; A413: 571
[55] D'Souza N, Jennings P A, Yang X L, Dong H B, Lee P D, McLean M. Metall Mater Trans, 2005; 36B: 657
[56] Yang C B, Liu L, Zhao X B, Sun D J, Zhang J, Fu H Z. Appl Phys, 2014; 114A: 979
[57] Zhou Y Z. Scr Mater, 2011; 65: 281
Outlines

/

〈 〉