MICROSTRUCTURE OF DIRECTLY EXTRUDED Mg-1Zn-1Ca ALLOY AND ITS CORROSION BEHAVIOR IN SBF SOLUTION

  • Zhongming ZHANG ,
  • Kai YU ,
  • Weiwei REN ,
  • Ying MA ,
  • Chunjie XU ,
  • Zengzhe XI
Expand
  • 1 Key Laboratory of Electrical Materials and Infiltration Technology of Shaanxi Province, School of Materials Science and Engineering, Xi'an University of Technology, Xi'an 710048
    2 Shaanxi Key Laboratory of Optoelectronic Functional Materials and Devices, School of Materials and Chemical Engineering, Xi'an Technological University, Xi'an 710032

Accepted date: 2015-03-27

  Online published: 2015-08-27

Supported by

Supported by Shaanxi Provincial Science and Technology Plan Project (No.2010K10-08), Scientific Research Project of Education Department of Shaanxi Province (No.2013JK0906) and Research Project of Key Laboratory of Electrical Materials and Infiltration Technology of Shaanxi Province (No.ZSKJ201302)

Abstract

The as-extruded Mg-1Zn-1Ca (mass fraction, %) alloys was fabricated successively by alloying, homogenization treatment and hot extrusion. The corrosion behavior of the alloy in simulated body fluid (SBF) solution was evaluated by electrochemical test and immersion test. The microstructure and morphology of corrosion product were observed by OM and SEM. Compositions of corrosion layer and different phases were investigated by EDS analysis. Fourier Transform infrared spectroscopy was also conducted to identify the functional groups in the corrosion products and XRD was also used to determine the phase constitutes of the corrosion products. The results show that Mg-1Zn-1Ca alloy consists of three phases, i.e. a-Mg, Mg2Ca and Ca2Mg6Zn3. After immersion in SBF solution for 72 h, the corrosion products is composed of HA (Ca10(OH)2(PO4)6), CaCO3, MgCl2 and Mg(OH)2. During the stage of immersion, the high active Mg2Ca phases act as the anode and corrode first, so they protect the around a-Mg substrate; the Ca2Mg6Zn3 phases are the lowest active, so they accelerate the corrosion of around α-Mg substrate. The corrosion resistance of as-cast Mg-1Zn-1Ca alloy are better than as-extruded alloy.

Cite this article

Zhongming ZHANG , Kai YU , Weiwei REN , Ying MA , Chunjie XU , Zengzhe XI . MICROSTRUCTURE OF DIRECTLY EXTRUDED Mg-1Zn-1Ca ALLOY AND ITS CORROSION BEHAVIOR IN SBF SOLUTION[J]. Acta Metall Sin, 2015 , 51(8) : 985 -992 . DOI: 10.11900/0412.1961.2014.00652

References

[1] Mark P S, Alexis M P. Biomaterials, 2006; 27: 1728
[2] Li K K, Wang B, Yan B. Corros Sci Protect Technol, 2012; 24: 181 (李锴锴, 王 冰, 严 彪. 腐蚀科学与防护技术, 2012; 24: 181)
[3] Moravej M, Mantovani D. Int J Mol Sci, 2011; 12: 4250
[4] Wen Z, Wu C, Dai C. J Alloys Compd, 2009; 488: 392
[5] Xin Y C, Huo K F, Tao H, Tang G Y, Chu P K. Acta Biomater, 2008; 4: 2008
[6] Hradilova M, Montheillet F, Frackiewicz A, Desrayaud C, Lejcek P. Mater Sci Eng, 2013; A580: 217
[7] Zhang X, Yuan G, Mao L, Niu J, Fu P, Ding W. Biomaterials, 2012; 7: 77
[8] Yin D S, Zhang E L, Zeng S Y. Trans Mater Heat Treat, 2009: 114: 118 (尹冬松, 张二林, 曾松岩. 材料热处理学报, 2009; 114: 118)
[9] Somekawa H, Mukai T. Mater Sci Eng, 2007; A459: 366
[10] Song W W, Martin H J, Hicks A, Seely D, Walton C A, Lawrimore II W B, Wang P T, Horstemeyer M F. Corros Sci, 2014; 78: 353
[11] Bakhsheshi-Rad H R, Abdul-kadir M R, Idris M H, Farahany S. Corros Sci, 2012; 64: 184
[12] Kokubo T, Takadama H. Biomaterials, 2006; 27: 2907
[13] Mao P L, Yu J C, Liu Z. Chin Trans Nonferrous Met Soc, 2013; 23: 889 (毛萍莉, 于金程, 刘 正. 中国有色金属学报, 2013; 23: 889)
[14] Wang Q, Wang J F, Huang S. J Mater Eng Perform, 2013; (11): 57 (汪 清, 王敬丰, 黄 崧. 材料工程, 2013; (11): 57)
[15] Liu C M,Zhu X R,Zhou H T. Phase Diagrams for Magnesium Alloys. Changsha: Central South University Press, 2006: 1 (刘楚明,朱秀荣,周海涛. 镁合金相图集. 长沙: 中南大学出版社, 2006: 1)
[16] Wasiur-Rahman S, Medraj M. Intermetallics, 2009; 17: 847
[17] Farahany S, Bakhsheshi-Rad H R, Idris M H, Abdul-kadir M R, Lotfabadi A F, Ourdjini A. Thermochim Acta, 2012; 527: 180
[18] Meng E C, Guan S K, Wang H X, Wang L G, Zhu S J, Hu J H, Ren C X, Gao J H, Feng Y S. Appl Surf Sci, 2011; 257: 4811
[19] Zhang X, Liang M J, Liao H H, Bai P K, Huang S. Hot Working Technol, 2014; 43(8): 9 (张 晓, 梁敏洁, 廖海洪, 白培康, 黄 莎. 热加工工艺, 2014; 43(8): 9)
[20] Fang S J, Liu Y H, Dong G D. Corros Sci Protect Technol, 2008; 20: 100 (方世杰, 刘耀辉, 佟国栋. 腐蚀科学与防护技术, 2008; 20: 100)
[21] Li Z J, Gu X A, Lou S Q. Biomaterials, 2008; 29: 1329
[22] Zhang S X, Zhang X N, Zhao C L, Li J N, Song Y, Xie C Y, Tao H R, Zhang Y, He Y H, Jiang Y, Bian Y J. Acta Biomater, 2010; 6: 626
[23] Du H, Wei Z J, Liu X W, Zhang E. Mater Chem Phys, 2011; 125: 568
[24] Bakhsheshi-Rad H R, Idris M H, Abdul-Kadir M R, Ourdjini A, Medraj M, Daroonparvar M, Hamzah E. Mater Des, 2014; 53: 283
[25] Kirkland N T, Birbilis N, Walker J, Woodfield T, Dias G J, Staiger M P. Biomed Mater Res, 2010; 95B: 91
Outlines

/

〈 〉