MICROSTRUCTURAL DEGRADATION AND MECHANI- CAL PROPERTIES OF GH4033 ALLOY AFTER OVERHEATING FOR SHORT TIME

  • Jinyan TONG ,
  • Wei FENG ,
  • Chao FU ,
  • Yunrong ZHENG ,
  • Qiang FENG
Expand
  • 1 National Centre for Materials Service Safety, University of Science and Technology Beijing, Beijing 100083
    2 State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083
    3 Casting Center, Beijing Institute of Aeronautical Materials, Beijing 100095

Online published: 2015-08-26

Supported by

Supported by National High Technology Research and Development Program of China (No.2012-AA03A513) and Key Project of Chinese Ministry of Education (No.625010337)

Abstract

Service safety of turbine blades in aircraft engines are threatened by microstructural and property degradation instantly caused by overheating during service. Systematic investigations about microstructural degradation during overheating exposures and its influence on mechanical properties of turbine blades during service are limitedly reported. In this work, microstructure and mechanical properties of GH4033 alloy, which was sectioned from the shank of a serviced 2nd stage turbine blade in an aircraft engine, were studied after overheating at 900~1100 ℃ for 3 min. Microstructural degradation during overheating exposures as well as its influence on room temperature hardness and stress rupture life at 700 ℃, 430 MPa were analyzed. The results of microstructural characterization indicated that the coarsening and dissolution of γ’ precipitates were introduced by overheating exposures, and all of the γ’ precipitates dissolved at 980 ℃ for 3 min. Gradual dissolution of grain boundary (GB) carbides was observed with the increase of overheating temperature. Complete dissolution of GB carbides at 1100 ℃ resulted in grain growth. The room temperature hardness after overheating exposures decreased grossly with the dissolution of γ’ phase. Due to the dissolution and re-precipitation of γ’ phase as well as the dissolution of GB carbides, the stress rupture life under 700 ℃, 430 MPa of GH4033 alloy was initially increased and then decreased significantly.

Cite this article

Jinyan TONG , Wei FENG , Chao FU , Yunrong ZHENG , Qiang FENG . MICROSTRUCTURAL DEGRADATION AND MECHANI- CAL PROPERTIES OF GH4033 ALLOY AFTER OVERHEATING FOR SHORT TIME[J]. Acta Metall Sin, 2015 , 51(10) : 1242 -1252 . DOI: 10.11900/0412.1961.2015.00265

References

[1] Reed R C. The Superalloys Fundamentals and Applications. Cambridge, UK: Cambridge University Press, 2006: 18
[2] Guo J T. Materials Science and Engineering for Superalloys. Vol.3, Beijing: Science Press, 2010: 508 (郭建亭. 高温合金材料学(下册). 北京: 科学出版社, 2010: 508)
[3] Feng Q, Tong J Y, Zheng Y R, Wang M L, Wei W J, Zhao H L, Yuan X F, Ding X F. Mater China, 2012; 31(12): 21 (冯 强, 童锦艳, 郑运荣, 王美玲, 魏文娟, 赵海龙, 袁晓飞, 丁贤飞. 中国材料进展, 2012; 31(12): 21)
[4] Koul A, Wallace W. Met Mater Trans, 1983; 14A: 183
[5] Liburdi J, Lowden P, Nagy D, De Priamus T R, Shaw S. Proc ASME Turbo Expo, Orlando: International Gas Turbine Institute,2009: 819
[6] Yoo K B, Lee H S. Mater Sci Forum, 2010; 654-656: 2523
[7] Liu Q Q. Manufacture Technologies and Failure Analyses of Blades in Aircraft Engines. Beijing: Aviation Industry Press, 2011: 98 (刘庆瑔. 航空发动机叶片制造技术及失效分析. 北京: 航空工业出版社, 2011: 98)
[8] Tao C H. Faiture Analysis and Prevention for Rotor in Aero-Engine. Beijing: National Defense Industry Press, 2008: 1 (陶春虎. 航空发动机转动部件的失效与预防. 北京: 国防工业出版社, 2008: 1)
[9] Zhao W X, Li Y, Fan Y W, Zheng Y R. J Mater Eng, 2012; (8): 39 (赵文侠, 李 莹, 范映伟, 郑运荣. 材料工程, 2012; (8): 39)
[10] Tawancy H M, Al-Hdhrami L. Eng Fail Anal, 2008; 15: 1027
[11] Cai Y L,Zheng Y R. Metallographic Research of Superalloys. Beijing: National Defense Industry Press, 1986: 228 (蔡玉林,郑运荣. 高温合金的金相研究. 北京: 国防工业出版社, 1986: 228)
[12] Sun S Z, Li S Y, Zheng Y R. J Mater Eng, 1990; (3): 45 (孙淑珍, 李淑媛, 郑运荣. 材料工程, 1990; (3): 45)
[13] Li Y, Hou X Q, Tao C H, Jiang T. J Iron Steel Res, 2011; 23(suppl 2): 452 (李 莹, 候学勤, 陶春虎, 姜 涛. 钢铁研究学报, 2011; 23(增刊2): 452)
[14] Liu D L, Zhang W F, Li C G, Miao H B. Heat Treat Met, 2007; 32(1): 71 (刘德林, 张卫方, 李春光, 缪宏博. 金属热处理, 2007; 32(1): 71)
[15] Gao Y. New Manufacture Technologies, Metallograph Atlas and Manual for Data of Superalloys. Beijing: Science and Technology of China Press, 2006: 57 (高 原. 高温合金生产新工艺新技术与金相图谱及常用数据速用速查手册. 北京: 中国科技文化出版社, 2006: 57)
[16] Tong J Y, Ding X F, Wang M L, Zheng Y R, Yagi K, Feng Q. Mater Sci Eng, 2014; A618: 605
[17] Xu Y L, Jin Q M, Xiao X S, Cao X L, Jia G Q, Zhu Y M, Yin H J. Mater Sci Eng, 2011; A528: 4600
[18] Zhao Y, Gai X Y, Song G H. Phys Test Chem Anal: Phys Test, 2007; 43A: 498 (赵 越, 盖秀颖, 宋贵宏. 理化检验: 物理分册, 2007; 43A: 498)
[19] Bridges P J, White C H, Durber G L R. The Nimonic Alloys. Bristol: Edward Arnold Ltd, 1974: 33
[20] Richards E. J Inst Met, 1968; 96: 365
[21] Carter T J. Eng Fail Anal, 2005; 12: 237
[22] Zhang L H. Heat Treat, 2003; 18(3): 26 (张立红. 热处理, 2003; 18(3): 26)
[23] Ge T T. Master Thesis, University of Science and Technology Beijing, 2006 (葛婷婷. 北京科技大学硕士学位论文, 2006)
[24] Voice W E, Faulkner R G. Met Mater Trans, 1985; 16A: 511
[25] Furillo F T, Davidson J M, Tien J K, Jackman L A. Mater Sci Eng, 1979; A39: 267
[26] Iwashita C H. PhD Dissertation, Lehigh University, Bethlehem, 1998
[27] Bhowal P, Wright E, Raymond E. Met Trans, 1990; 21A: 1709
[28] Locq D, Caron P, Raujol S, Pettinari-Sturmel F, Coujou A, Clement N. In: Green K A, Pollock T M, Harada H, Howson T E, Reed R C, Schirra J J, Walston S eds., Superalloys 2004, Pennsylvania: TMS, 2004: 179
[29] Sun K J, Gai X Y, Li C X. Phys Test Chem Anal: Phys Test, 2009; 7A: 393 (孙克君, 盖秀颖, 李晨希. 理化检验: 物理分册, 2009; 7A: 393)
[30] Osada T, Nagashima N, Gu Y F, Yuan Y, Yokokawa T, Harada H. Scr Mater, 2011; 64: 892
Outlines

/

〈 〉