INVESTIGATION OF HIGH PERFORMANCE DISC ALLOY GH4065 AND ASSOCIATED ADVANCED PROCESSING TECHNIQUES

  • Beijiang ZHANG ,
  • Guangpu ZHAO ,
  • Wenyun ZHANG ,
  • Shuo HUANG ,
  • Shifu CHEN
Expand
  • High Temperature Materials Research Division, Central Iron & Steel Research Institute, Beijing 100081

Online published: 2015-08-25

Supported by

Supported by High Technology Research and Development Program of China (No.2012AA03A510) and National Basic Research Program of China (No.2010CB631203)

Abstract

Much attention has been paid to the development of more advanced materials for high-pressure compressor and turbine discs of gas turbine engines. A high performance wrought superalloy GH4065 for disc applications has been recently developed based on the comprehensive evaluation of a series of model alloys with characteristic chemical composition, lattice parameter, particularly γ’ volume fraction. The concentration of major alloying elements of GH4065 is closely similar with René 88 DT and specifically optimized considering the demands of ingot metallurgy technologies. Therefore, GH4065 can be considered as an ingot metallurgy version of powder metallurgy René 88 DT. Large scale vacuum arc remelting (VAR) ingots of GH4065 alloy with diameter up to 508 mm have been produced via standard triple melting techniques. Micro-scale segregation of alloying elements on large VAR ingot has been effectively suppressed due both to optimized alloying elements concentration and to improved melting techniques. Ultra-low carbon content (less than 0.02% in mass fraction) significantly decreases the dendritic segregation tendency of certain alloying elements and promotes the uniformity of microstructures. VAR ingot of GH4065 exhibits extraordinary hot plasticity, ingot conversion can be accomplished using conventional open die forging procedure. Fine and uniform γ+γ’ duplex structures can be obtained on billets and disc forgings via a newly developed multi-cycle thermomechanical processing method. The flow stress data show that the formation of γ+γ’ microduplex results in a significant decrease of flow stress in comparison with γ’ dispersion structures under exactly the same deformation conditions. The distribution of strain rate sensitivity m in relationship with temperature and strain rate accurately identifies a specific domain within which γ+γ’ microduplex exhibits superplasticity. Full-scale turbine discs of GH4065 alloy with diameter of 630 mm achieve an optimal combination of creep resistance, fatigue lifetime and ductility. GH4065 discs exhibit extraordinary microstructural and property stability during prolonged thermal exposure, which means that dendritic segregation has been successfully restricted to an acceptable level. The results reveal that highly alloyed disc alloys produced via ingot metallurgy techniques exhibit lower costs and higher productivity, and can still meet the ever increasing demand of high performance gas turbine engines.

Cite this article

Beijiang ZHANG , Guangpu ZHAO , Wenyun ZHANG , Shuo HUANG , Shifu CHEN . INVESTIGATION OF HIGH PERFORMANCE DISC ALLOY GH4065 AND ASSOCIATED ADVANCED PROCESSING TECHNIQUES[J]. Acta Metall Sin, 2015 , 51(10) : 1227 -1234 . DOI: 10.11900/0412.1961.2015.00368

References

[1] Williams J C, Starke E A. Acta Mater, 2003; 51: 5775
[2] Decker R F. JOM, 2006; 58(9): 32
[3] Sims C T, Stoloff N S, Hagel W C. Superalloys II—High Temperature Materials for Aerospace and Industrial Power. New York: John wiley & Sons, 1987: 32
[4] Donachie M J, Donachie S J. Superalloys: A Technical Guide. Ohio: ASM International, 2002: 120
[5] Shi C X, Zhong Z Y. Acta Matall Sin, 1997; 33: 1 (师昌绪, 仲增墉. 金属学报, 1997; 33: 1)
[6] Heaney J A, Lasonde M L, Powell A M, Bond B J, O'Brien C M. In: Ott E, Banik A, Liu X B, Dempster I, Heck K, Andersson J, Groh J, Gabb T, Helmink R, Sarnek A W eds., 8th Int Symp on Superalloy 718 and Derivatives, Pittsburgh: TMS, 2014: 67
[7] Devaux A, Picqué B, Gervais M F, Georges E, Poulain T, Héritier P. In: Huron E S, Reed R C, Hardy M C, Mills M J, Montero R E, Telesman J eds., Superalloy 2012: 12th Int Symp on Superalloys, Pittsburgh: TMS, 2012: 911
[8] Monajati H, Jahazi M, Yue S, Taheri A K. Metall Mater Trans, 2005; 36A: 895
[9] Bond B J, O'Brien C M, Russell J L, Heane J A, Lasonde M L. In: Ott E, Banik A, Liu X B, Dempster I, Heck K, Andersson J, Groh J, Gabb T, Helmink R, Sarnek A W eds., 8th Int Symp on Superalloy 718 and Derivatives, Pittsburgh: TMS, 2014: 107
[10] Long Z D, Zhuang J Y, Deng B, Zhong Z Y. Acta Metall Sin, 1999; 35: 1211 (龙正东, 庄景云, 邓 波, 仲增墉. 金属学报, 1999; 35: 1211)
[11] Zhang B J, Zhao G P, Jiao L Y, Xu G H, Qin H Y, Feng D. Acta Metall Sin, 2005; 41: 351 (张北江, 赵光普, 焦兰英, 胥国华, 秦鹤勇, 冯 涤. 金属学报, 2005; 41: 351)
[12] Zhang B J, Zhao G P, Xu G H, Feng D. Acta Metall Sin, 2005; 41: 1207 (张北江, 赵光普, 胥国华, 冯 涤. 金属学报, 2005; 41: 1207)
[13] Carter W T, Jones R M F. JOM, 2005; 57(4): 52
[14] Cantwell P R, Tang M, Dillon S J, Luo J, Rohrer G S, Harmer M P. Acta Mater, 2014; 62: 1
[15] Robson J D. Acta Mater, 2013; 61: 7781
[16] Fang B, Ji Z, Liu M, Tian G, Jia C, Zeng T T, Hu B F, Wang C C. Mater Sci Eng, 2014; A590: 255
[17] Larrouy B, Villechaise P, Cormie J, Berteaux O. In: Ott E, Banik A, Liu X B, Dempster I, Heck K, Andersson J, Groh J, Gabb T, Helmink R, Sarnek A W eds., 8th Int Symp on Superalloy 718 and Derivatives, Pittsburgh: TMS, 2014: 713
[18] Valitov V A. In: Ott E, Banik A, Liu X B, Dempster I, Heck K, Andersson J, Groh J, Gabb T, Helmink R, Sarnek A W eds., 8th Int Symp on Superalloy 718 and Derivatives, Pittsburgh: TMS, 2014: 665
[19] Wlodek S T, Kelly M, Alden D A. In: Kissinger R D, Deye D J, Anton D L, Cetel A D, Nathal M V, Pollock T M, Woodford D A eds., Proc 8th Int Symp on Superalloy, Pennsylvania: TMS, 1996: 129
[20] Carter J L W, Kuper M W, Uchic M D, Mills M J. Mater Sci Eng, 2014; A605: 127
[21] Findley K O, Saxena A. Metall Mater Trans, 2005; 37A: 1469
[22] Tiley J, Viswanathan G B, Srinivasan R, Banerjee R, dimiduk D M, Fraser H L. Acta Mater, 2009; 57: 2538
[23] MacSleyne J, Uchic M D, Simmons J P, Graef M D. Acta Mater, 2009; 57: 6251
[24] Radis R, Schaffer M, Albu M, Kothleitner G, Polt P, Kozeschnik E. Acta Mater, 2009; 57: 5739
[25] Reed R C. The Superalloys: Fundamentals and Applications. Cambridge: Cambridge University Press, 2006: 236
[26] Viswanathan G B, Sarosi P M, Henry M F, Whitis D D, Milligan W W, Mills M J. Acta Mater, 2005; 53: 3041
[27] Hayes R W, Unocic R R, Nasrollahzadeh M. Metall Mater Trans, 2015; 46A: 218
Outlines

/

〈 〉