Orginal Article

RESEARCH ON THE PREPARATION AND PERFOR-MANCE OF TUNGSTEN-ALUMINUM TRANSMIS-SION TARGET FOR MICRO-COMPUTED TOMOGRAPHY BY MAGNETRONSPUTTERING

  • Yutian MA ,
  • Junbiao LIU ,
  • Rongling HUO ,
  • Li HAN ,
  • Geng NIU
Expand
  • Institute of Electrical Engineering, Chinese Academy of Sciences, Beijing 100190

Online published: 2015-08-10

Supported by

Supported by National Key Scientific Instrument and Equipment Development Projects (No.2011YQ030112)

Abstract

Micro-computed tomography is a new three-dimension high-resolution imaging device, which due to its X-ray brightness generated by a compact electron impact X-ray source. To achieve higher X-ray brightness, the size of the X-ray source should be as small as possible. However, the X-ray brightness is fundamentally limited by the maximum possible heat dissipation of the X-ray target. As an electron beam strikes a metallic target, the power density of target is increased with the decreasing of the spot size of electron beam, which results in the decrease of the X-ray brightness by significant temperature elevation of the target surface. A practical solution for these requirements is the use of a multi-film target consisting of a thin-film target on a thicker substrate film. The substrate should be composed of a light material with high thermal conductivity to prevent absorption of the signal X-rays and to elevate the target temperature. In such a multi-film target, several factors as following must be considered to choose the materials and thicknesses of the multiple films: the highest power density of the target can sustain without performance degradations or damage, and the efficiency of the X-ray generation in the target material including any self absorption effects. The present work designed a basic structure of tungsten-aluminum transmission target, according to the theoretical model of the end-window transmission target for Micro-CT. The thicknesses of tungsten target surface and aluminum substrate are determined by the Geant4 simulation results and the Müller calculation model of temperature rise, respectively. According to the structure parameter of tungsten-aluminum transmission target of YXLON, the tungsten film with the thickness of 2, 5 and 8 μm are prepared on the aluminum substrate by the magnetron sputtering method. The density and evenness of tungsten film both are well by the SEM analysis. The performance of three kinds of target with different thicknesses is carried out on the X-ray tube of YXLON. The results show that the optimal thickness of tungsten film is 5 μm, and the X-ray emitting efficiency of tungsten-aluminum transmission target is the biggest, which the corresponding production power of X-ray is the lowest. On this basis, the contrast experiments of X-ray emitting efficiency and X-ray imaging effect are carried out between the tungsten-aluminum transmission target of homemade and that of YXLON. The experimental results indicate that the X-ray emitting efficiency, the corresponding X-ray production power and the X-ray imaging effect of homemade target all are superior to that of YXLON, which could be satisfied the application requirements of high quality target for Micro-CT.

Cite this article

Yutian MA , Junbiao LIU , Rongling HUO , Li HAN , Geng NIU . RESEARCH ON THE PREPARATION AND PERFOR-MANCE OF TUNGSTEN-ALUMINUM TRANSMIS-SION TARGET FOR MICRO-COMPUTED TOMOGRAPHY BY MAGNETRONSPUTTERING[J]. Acta Metall Sin, 2015 , 51(11) : 1416 -1424 . DOI: 10.11900/0412.1961.2015.00147

References

[1] Rubin C, Turner A S, Müller R, Mittra E, McLeod K, Lin W, Qin Y.J Bone Miner Res, 2002; 17: 349
[2] Moreno-Atanasio R, Richard A W. Particuology, 2010; 8: 81
[3] Gui J B, Hu Z L, Zhou Y, Zheng H R. CT Theory Appl, 2009; 18:106 (桂建保, 胡战利, 周颖, 郑海荣. CT理论与应用研究, 2009; 18:106)
[4] Yan J, Jiang S E, Su M, Wu S C, Lin Z W. Acta Phys Sin, 2012; 61: 068703 (晏骥, 江少恩, 苏明, 巫顺超, 林稚伟. 物理学报, 2012; 61: 068703)
[5] Yan J, Zheng J H, Chen L, Lin Z W, Jiang S E. Acta Phys Sin, 2012; 61: 148701 (晏骥, 郑建华, 陈黎, 林稚伟, 江少恩. 物理学报, 2012; 61: 148701)
[6] Cnudde V, Boone M N. Earth-Sci Rev, 2013; 123: 1
[7] Wang Y D, Peng G Y, Tong Y J, Zhou G Z, Ren Y Q, Yang Q, Xiao T Q. Acta Phys Sin, 2012; 61: 054205 (王玉丹, 彭冠云, 佟亚军, 周光照, 任玉琦, 杨群, 肖体乔. 物理学报, 2012; 61: 054205)
[8] Qi J C, Ye L L, Chen R C, Xie H L, Ren Y Q, Du G H, Deng B, Xiao T Q. Acta Phys Sin, 2014; 63: 104202 (戚俊成, 叶琳琳, 陈荣昌, 谢红兰, 任玉琦, 杜国浩, 邓彪, 肖体乔. 物理学报, 2014; 63: 104202)
[9] Batemna J E, Moss G R, Roekett P, Webb S. Nucl Instru Meth, 1988; 273A: 767
[10] Pinies B R. translated by He L. Fine-Focus X-ray Tube and its Application in Structural Analysis. Beijing: Science Press, 1963: 40 (Pinies B R著, 何犖译. 细聚焦X射线管及其在结构分析中的应用. 北京: 科学出版社,1963: 40)
[11] Ihsan A, Heo S H, Cho S O. Nucl Instru Meth, 2009; 267B: 3566
[12] Wu Y, Wang G Y, Mu Q, Zhao Q. Chin Phys, 2014; 23B: 013401
[13] Mei C X, Zhang X A, Zhao Y T, Zhou X M, Ren J R, Wang X, Lei Y, Sun Y B, Cheng R, Wang Y Y, Liang C H, Li Y Z, Xiao G Q. Chin Phys, 2013; 22B: 103403
[14] Lei Y H, Liu X, Guo J C, Zhao Z G, Niu H B. Chin Phys, 2011; 20B: 042901
[15] Wang Y F, Que J M, Cao D Q, Sun C L, Zhao W, Wei C F, Shi R J, Wei L. Chin Phys, 2013; 37C: 078202
[16] Wang Y, Li Q, Jiang X G. Chin Phys, 2012; 36C: 861
[17] Dai Q S, Qi Y J. Acta Phys Sin, 2010; 59: 357 (代秋声, 漆玉金. 物理学报, 2010; 59: 357)
[18] Yoshioka A, Yamaguchi Y, Tamura K, Shimizu R. Surf Interface Anal, 2005; 37: 356
[19] Yoshioka A, Yamaguchi Y, Tamura K, Shimizu R. Surf Interface Anal, 2004; 36: 1417
[20] Gao L N, Chen W G. Chin J Rare Met, 2008; 32: 605 (高丽娜, 陈文革. 稀有金属, 2008; 32: 605)
[21] Gao L N. Electron Des Eng, 2012; 20(19): 168 (高丽娜. 电子设计工程, 2012; 20(19): 168)
[22] Lai D G, Zhang Y M, Li J X, Su Z F, Zhang Y Y, Ren S Q, Yang L, Yang S. High Power Laser Part Beams, 2012; 25: 1396 (来定国, 张永民, 李进玺, 苏兆峰, 张玉英, 任书庆, 杨莉, 杨实. 强激光与粒子束, 2012; 25: 1396)
[23] Park C K, Kim J P, Yun S J, Lee S H, Park J S. Thin Solid Films, 2007; 516: 304
[24] Jenneson P M, Luggar R D, Morton E. J Appl Phys, 2004; 96: 2889
[25] Senda S, Sakai Y, Mizuta Y, Kita S, Okuyama F. Appl Phys Lett, 2004; 85: 5679
[26] Ma Y H. The Characteristics of X-ray, X-ray Physics and Protection. Beijing: People's Medical Publishing House, 1996: 27 (马延洪. 特征X线、X线物理与防护. 北京: 人民卫生出版社, 1996: 27)
[27] Teterev U G, Belov A G. Atomic Energy, 2001; 91: 745
[28] Yoshioka A, Yamaguchi Y, Tamura K, Shimizu R. Surf Interface Anal, 2005; 37: 356
[29] Cao Q Q, Jin C, Ren X, Sha J T. Chin J Radiol Health, 2013; 22(1): 15 (曹琴琴, 金川, 任翔, 沙京田. 中国辐射卫生, 2013; 22(1): 15)
[30] Yang Q, Ge L Q, Gu Y, Hua Y T, Luo Y Y. Spectrosc Spectral Anal, 2013; 33: 1130 (杨强, 葛良全, 谷懿, 花永涛, 罗耀耀. 光谱学与光谱分析, 2013; 33: 1130)
Outlines

/

〈 〉