INTERFACIAL REACTION AND STRENGTHENING MECHANISM OF CERAMIC MATRIX COMPOSITE JOINTS USING LIQUID PHASE DIFFUSION BONDING WITH AUXILIARY PULSE CURRENT
Online published: 2015-07-07
Supported by
Supported by National Natural Science Foundation of China (No.51175239), Jiangsu Provincial Research Foundation for Basic Research (No.BK2011494) and College Natural Science Foundation of Jiangsu Province (No.11KJA430005)
Ceramic matrix composites (CMCs) is attracted in airspace and nuclear engineering due to their high temperature, corrosion and wearing resistance, but the usage is limited by the joining between CMC and other metals due to obvious incompatibility on physical and chemical aspects on them. The liquid phase-diffusion bonding (LPDB) on Ti(C, N)-Al2O3 CMC/Cu joint was studied using the Cu-Zr foil/Cu foil/Cu-Zr foil sanwich as an interlayer in this work. Auxiliary pulse current was also added to control the elemental diffusion and interfacial reaction during LPDB. The element diffusion and reacted products at the interface were analyzed with SEM, EPMA and EDS, and the joint strength was tested with four points bending method. The results show that with an auxiliary pulse current during LPDB, a higher joint strength is reached with a lower bonding temperature and a shorter holding time. The diffusion behavior of element Zr and Cu in CMC and the interfacial area is obviously changed, and the activity of Zr element and its chemical reaction with Al2O3 are depressed by the auxiliary pulse current during LPDB. The diffusion of ceramic partilces into the interface and the thickness of corresponding diffusion transition zone (DTZ) and Zr-Cu interfacial reaction zone (IRZ) at the interface are also depressed by the auxiliary pulse current, which strengthens the interface, and is always kept an higher joint strength.
Mingfang WU , Fei LIU , Fengjiang WANG , Yanxin QIAO . INTERFACIAL REACTION AND STRENGTHENING MECHANISM OF CERAMIC MATRIX COMPOSITE JOINTS USING LIQUID PHASE DIFFUSION BONDING WITH AUXILIARY PULSE CURRENT[J]. Acta Metall Sin, 2015 , 51(9) : 1129 -1135 . DOI: 10.11900/0412.1961.2015.00100
| [1] | Zhang D K, Wu A P, Zou G S. Trans China Weld Inst, 2005; 26(10): 59 (张德库, 吴爱萍, 邹贵生. 焊接学报, 2005; 26(10): 59) |
| [2] | Wang Q Z, Liu Y, Zhang Y Z, Guan D H, Bi J. Trans China Weld Inst, 2006; 27(8): 43 (王全兆, 刘 越, 张玉政, 关德慧, 毕 敬. 焊接学报, 2006; 27(8): 43) |
| [3] | Wu M F, Zhou X L, Ma C, Yang P. Trans China Weld Inst, 2006; 27(12): 1 (吴铭方, 周小丽, 马 骋, 杨 沛. 焊接学报, 2006; 27(12): 1) |
| [4] | Wang Y, Cao J, Geng J C. China Welding, 2009; 18(4): 39 |
| [5] | Passerone A, Muolo M L. Mater Manuf Process, 2000; 15: 631 |
| [6] | Chen Z, Cao M S, Zhao Q Z. Mater Sci Eng, 2004; A380: 394 |
| [7] | Li Z R, Cao J, Feng J C. Trans China Weld Inst, 2003; 24(2): 4 (李卓然, 曹 健, 冯吉才. 焊接学报, 2003; 24(2): 4) |
| [8] | Osendi M I, De Pablos A, Miranzo P. Mater Sci Eng, 2001; A308: 53 |
| [9] | Li S J, Liang X B, Duan H P. Key Eng Mater, 2002; 217: 101 |
| [10] | Rabin B H, Moore G A. In: Carin A H, Schwartz D S, Silberglitt R S, Loehman R E eds., Mater Res Soc Symp Proc, 1993; 314: 197 |
| [11] | He D H, Fu Z Y, Wang H, Zhang J Y. Trans China Weld Inst, 2002; 23(6): 33 (何代华, 傅正义, 王 皓, 张金咏. 焊接学报, 2002; 23(6): 33) |
| [12] | He D H, Fu Z Y, Wang H, Zhang J Y. Trans China Weld Inst, 2002; 23(1): 85 (何代华, 傅正义, 王 皓, 张金咏. 焊接学报, 2002; 23(1): 85) |
| [13] | Liu H J, Feng J C, Li G, Wang Y G. Welding Joining, 2000; (9): 7 (刘会杰, 冯吉才, 李 广, 王跃国. 焊接, 2000; (9): 7) |
| [14] | Wanger T, Kirchheim R, Rühle M. Acta Metall Mater, 1995; 43: 1053 |
| [15] | Zhang G, Zhang J, Pei Y, Li S, Chai D. Mater Sci Eng, 2008; A488: 146 |
| [16] | Yang W, Lin T, He P, Wei H, Xing L, Jia D. Ceram Int, 2014; 40: 7253 |
| [17] | Wu M F, Yu Z S, Jiang C Y, Qi K, Cheng X N. Rare Met Mater Eng, 2000; 29: 419 (吴铭方, 于治水, 蒋成禹, 祁 凯, 程晓农. 稀有金属材料与工程, 2000; 29: 419) |
| [18] | Wu M F, Wang F, Wang F J, Xu G X. Trans China Weld Inst, 2014; 35(6): 31 (吴铭方, 王 斐, 王凤江, 胥国祥. 焊接学报, 2014; 35(6): 31) |
| [19] | Loehman R E, Hosking F M, Gauntt B, Kotula P G, Lu P. J Mater Sci, 2005; 40: 2319 |
| [20] | Ye D L,Hu J H. Practical Handbook on the Thermodynamic Data of Inorganic Substances. 2nd Ed., Beijing: Metallurgical Industry Press, 2002: 57 (叶大伦,胡建华. 实用无机物热力学数据手册. 第二版, 北京: 冶金工业出版社, 2002: 57) |
| [21] | Ihsan B I,translated by Cheng N L,Niu S T,Xu G Y. Thermochemical Data of Pure Substances. Beijing: Science Press, 2003: 17 (Ihsan B I著,程乃良,牛四通,徐桂英译. 纯物质热化学数据手册. 北京: 科学出版社, 2003: 17) |
| [22] | Xu R,Jin T F.Thermodynamics and Kinetics of Materials. Harbin: Harbin Institute of Technology Press, 2003: 10 (徐 瑞,荆天辅.材料热力学与动力学. 哈尔滨: 哈尔滨工业大学出版社, 2003: 10) |
| [23] | Chen Z, Liu B, Wang Y X, Wei Q L. Rare Met Mater Eng, 2001; 30: 331 (陈 铮, 刘 兵, 王永欣, 魏齐龙. 稀有金属材料与工程, 2001; 30: 331) |
| [24] | Chang G W, Xue Q G. J Univ Sci Technol Beijing, 1999; 21: 175 (常国威, 薛庆国. 北京科技大学学报, 1999; 21: 175) |
| [25] | He S X, Wang J, Zhou Y H. Acta Metall Sin, 2002; 38: 479 (何树先, 王 俊, 周尧和. 金属学报, 2002; 38: 479) |
/
| 〈 |
|
〉 |