EFFECT OF MARTENSITE DISTRIBUTION ON MICROSCOPIC DEFORMATION BEHAVIOR AND MECHANICAL PROPERTIES OF DUAL PHASE STEELS

  • Jie DENG ,
  • Jiawei MA ,
  • Yiyang XU ,
  • Yao SHEN
Expand
  • State Key Laboratory of Metal Matrix Composites, Shanghai Jiao Tong University, Shanghai 200240

Online published: 2015-06-16

Supported by

Supported by National Basic Research Program of China (No.2012CB619600 ) and National Natural Science Foundation of China (No.51471107 )

Abstract

Investigation of the relationship between microstructure and microscopic deformation behavior of dual phase steel is very important for high property dual phase steel development. In this work, step quenching (SQ) and intercritical annealing (IA) heat treatments were optimized to produce dual phase steels of similar martensite volume fraction, but with respectively isolated and continuous martensite distribution. The tensile and dynamic fracture properties of dual phase steels were investigated. Strain distribution of steels was measured by digital image correlation (DIC) method. Combined with observations of microcracks/microvoids, different deformation and fracture mechanisms were revealed. Compared to IA steel, SQ steel has lower strength, but longer elongation and higher fracture toughness, and the latter were attributed to larger deformation in ferrites that results in more stress relaxation of martensite during deformation. While in IA steel, the deformation in ferrites is blocked by adjacent martensites, so that a relatively small strain of ferrite cannot effectively relax the stress in martensites, which resulted in higher plastic deformation in martensite than in SQ steel; therefore, cracks preferentially initiate in martensite, and IA steel exhibits higher strength and lower plasticity.

Cite this article

Jie DENG , Jiawei MA , Yiyang XU , Yao SHEN . EFFECT OF MARTENSITE DISTRIBUTION ON MICROSCOPIC DEFORMATION BEHAVIOR AND MECHANICAL PROPERTIES OF DUAL PHASE STEELS[J]. Acta Metall Sin, 2015 , 51(9) : 1092 -1100 . DOI: 10.11900/0412.1961.2015.00083

References

[1] Rashid M. Annu Rev Mater Sci, 1981; 11(1): 245
[2] Ma M T,Wu B R. Dual Phase Steel-Physics & Mechanical Metallurgy. 2nd Ed., Beijing: Metallurgical Industry Press, 2009: 1 (马鸣图,吴宝榕. 双相钢-物理和力学冶金. 第二版 , 北京: 冶金工业出版社, 2009: 1)
[3] Tian Z Q, Tang D, Jiang H T, Ma X L, Xu H X. Mater Mech Eng, 2009; 33(4): 1 (田志强, 唐 荻, 江海涛, 马小亮, 许洪汛. 机械工程材料, 2009; 33(4): 1)
[4] Gao L,Zhou Y M,Liu J L,Shen X D,Ren Z M. In: The Chinese Society for Metals ed., Proceeding 7th China Steel Conference, Beijing: Metallurgical Industry Press, 2009: 96 (高 丽,周月明,刘俊亮,沈小丹,任忠鸣. 见: 中国金属学会主编, 第七届中国钢铁年会论文集, 北京: 冶金工业出版社, 2009: 96)
[5] Tasan C, Hoefnagels J, Geers M. Scr Mater, 2010; 62: 835
[6] Byun T S, Kim I S. J Mater Sci, 1993; 28: 2923
[7] Gerbase J, Embury J D, Hobbs R M. In: Kot R A, Morris J W eds., Structure and Properties of Dual-Phase Steels, New York: TMS-AIME, 1979: 118
[8] Calcagnotto M, Adachi Y, Ponge D, Raabe D. Acta Mater, 2011; 59: 658
[9] Pierman A P, Bouaziz O, Pardoen T, Jacques P J, Brassart L. Acta Mater, 2014; 73: 298
[10] Park K, Nishiyama M, Nakada N, Tsuchiyama T, Takaki S. Mater Sci Eng, 2014; A604: 135
[11] Das D, Chattopadhyay P P. J Mater Sci, 2009; 44: 2957
[12] Ahmad E, Manzoor T, Ziai M, Hussain N. J Mater Eng Perform, 2012; 21: 382
[13] Su Y, Gurland J. Mater Sci Eng, 1987; 95: 151
[14] Han Q, Kang Y, Hodgson P D, Stanford N. Scr Mater, 2013; 69: 13
[15] Kim N, Thomas G. Metall Trans, 1981; 12A: 483
[16] Xu Y Y, Deng J, Ge H Q, Shen Y. Mater Mech Eng, 2015; 39(6): 40 (许以阳, 邓 洁, 葛涵清, 沈 耀. 机械工程材料, 2015; 39(6): 40)
[17] Sutton M A, Orteu J J, Schreier H. Image Correlation for Shape, Motion and Deformation Measurements: Basic Concepts, Theory and Applications. New York: Springer-Verlag US, 2009: 119
[18] Pan B, Qian K, Xie H, Asundi A. Meas Sci Technol, 2009; 20(6): 1
[19] Kang J, Ososkov Y, Embury J D, Wilkinson D S. Scr Mater, 2007; 56: 999
[20] Kang J, Jain M, Wilkinson D S, Embury J D. J Strain Anal Eng Des, 2005; 40: 559
[21] Joo S H, Lee J K, Koo J M, Lee S, Suh D W, Kim H S. Scr Mater, 2013; 68: 245
[22] Heat Treatment Manual Editorial Committee in Heat Treatment Institute of Chinese Mechanical Engineering Society. Heat Treatment Manual (Vol.1). 3rd Ed., Beijing: China Machine Press, 2001: 131 (中国机械工程学会热处理专业学会《热处理手册》编委会.热处理手册(第一卷)工业基础. 第三版, 北京: 机械工业出版社, 2001: 131
[23] Bag A, Ray K K, Dwarakadasa E S. Metall Mater Trans, 1999; 30A: 1193
[24] Ghadbeigi H, Pinna C, Celotto S, Yates J. Mater Sci Eng, 2010; A527: 5026
[25] Shen H, Lei T, Liu J. Mater Sci Technol, 1986; 2(1): 28
[26] Woo W, Em V, Kim E Y, Han S, Han Y, Choi S H. Acta Mater, 2012; 60: 6972
Outlines

/

〈 〉