Online published: 2015-06-01
As one of the most promising next generation reactors, the molten salt breeder reactor (MSBR) with excellent inherence security has attracted more and more attentions in recent years due to energy shortage and the security problem of traditional nuclear reactor. The most significant service characteristic of the structural material used in MSBR is the existence of FLiNaK molten salt compared with other nuclear reactors. FLiNaK molten salt is very corrosive to the structural material in the reactor, and affects the safety operation of nuclear power plants. A polycrystalline Ni-Mo-Cr-Fe superalloy was developed and used as an important structural material in MSBR at Oak Ridge National Laboratory (ORNL), but the corrosion mechanism of the alloy in FLiNaK molten salt has not been determined since the study terminated in 1970' s as some politic reasons. Alloy served in harsh environments, often using protective coating to improve the corrosion properties. While few works about the coating corrosion resistance in FLiNaK molten salt were reported at present. Al2O3 and Cr2O3 coatings usually have excellent corrosion resistance in molten salt, such as sulphate, nitrate and halide molten salt. But, whether the oxide film has corrosion resistance in FLiNaK molten salt has not been determined. In this work, the corrosion mechanism of alloy in FLiNaK molten salt was studied by using immersion corrosion experiment through the method of SEM, EDS and XRD. The influence of Al2O3 coating on corrosion resistance in FLiNaK molten salt was also investigated. The results show that the Al2O3 coating does not affect the exsolution corrosion characteristics of Cr and Mo elements in FLiNaK molten salt at 700 ℃ for 400 h. The different is that naked alloy exhibits intergranular corrosion characteristic, and the alloy with Al2O3 coating exhibits spot corrosion characteristic. The Al2O3 coating cannot improve the corrosion resistance of the alloy in FLiNaK molten salt. The Al2O3 film dissolved in molten salt and resulted in the exposure of the alloy surface. The corrosion rate was increased since the formation of corrosion cell between oxide film and the exposed alloy surface.
Key words: GH3535 alloy; FLiNaK molten salt; Al2O3 coating; corrosion
Tao LIU , Jiasheng DONG , Guang XIE , Yisheng WANG , Hui LI , Zhijun LI , Xingtai ZHOU , Langhong LOU . CORROSION BEHAVIOR OF GH3535 SUPERALLOY IN FLiNaK MOLTEN SALT[J]. Acta Metall Sin, 2015 , 51(9) : 1059 -1066 . DOI: 10.11900/0412.1961.2015.00132
| [1] | Guerrieri C, Cammi A, Luzzi L. Prog Nucl Energ, 2013; 67: 56 |
| [2] | Zou S L, Zou Y. J Univ South China (Soc Sci Ed), 2011; 12(2): 1 (邹树梁, 邹 旸. 南华大学学报(社会科学版), 2011; 12(2): 1) |
| [3] | Zanetti M, Cammi A, Fiorina C, Luzzi L. Prog Nucl Energy, 2015; 83: 82 |
| [4] | Jér?me S, Michel A, Ondrej B, Sylvie D, Olga F, Véronique G, Daniel H, David H, Victor I, Jan L K, Lelio L, Elsa M L, Jan U, Ritsuo Y, Dai Z. Prog Nucl Energy, 2014; 77: 308 |
| [5] | Rosenthal M W, Kasten P R, Briggs R B. Nucl Appl Technol, 1970; 8: 107 |
| [6] | Manly W D, Coobs J H, De Van J H, Douglas D A, Inouye H, Patriarca P, Roche T K, Scott J L. Prog Nucl Energy, 1960; 4: 164 |
| [7] | Wang Y M. J Chin Soc Corros Prot, 1981; 1: 64 (罔毅民. 中国腐蚀与防护学报, 1981; 1: 64) |
| [8] | Nobuya I, Yukio M, Kazuo F, Yoshio K, Hiroshi K. Trans JWRI, 1980; 9: 117 |
| [9] | Kondo M, Nagasaka T, Xu Q, Muroga T, Sagara A, Noda N, Ninomiya D, Nagura M, Suzuki A, Terai T, Fujii N. Fusion Eng Des, 2009; 84: 1081 |
| [10] | Olson L C, Ambrosek J W, Sridharan K, Anderson M H, Allen T R. J Fluorine Chem, 2009; 130: 67 |
| [11] | Cho S H, Park S B, Kang D S, Jeong M S, Park H, Hur J M, Lee H S. J Nucl Mater, 2010; 399: 212 |
| [12] | Rahman A, Chawlab V, Jayaganthan R, Chandra R, Ambardar R. Mater Chem Phys, 2011; 126: 253 |
| [13] | Dutta R S, Yusufali C, Paul B, Majumdar S, Sengupta P, Mishra R K, Kaushik C P, Kshirsagar R J, Kulkarni U D, Dey G K. J Nucl Mater, 2013; 432: 72 |
| [14] | Ma J, Jiang S M, Gong J, Sun C. Corros Sci, 2012; 58: 251 |
| [15] | Firouzi A, Shirvani K. Corros Sci, 2010; 52: 3579 |
| [16] | Zheng D Y, Zhu S L, Wang F H. Surf Coat Technol, 2006; 200: 5931 |
| [17] | Phahle A M, Hill A E, Calderwood J H. Thin Solid Films, 1974; 22: 67 |
| [18] | Dasher B E, Farmer J, Ferreira J, Caro M S, Rubenchik A, Kimura A. J Nucl Mater, 2011; 419: 15 |
| [19] | Liu T, Dong J S, Wang L, Li Z J, Zhou X T, Lou L H, Zhang J. J Mater Sci Technol, 2015; 31: 269 |
| [20] | Ouyang F Y, Chang C H, You B C, Yeh T K, Kai J J. J Nucl Mater, 2013; 437: 201 |
| [21] | Tyreman C J. PhD Dissertation, University of Manchester, Manchester, UK, 1986 |
| [22] | Olson L C. PhD Dissertation, University of Wisconsin-Madison, Madison, USA, 2009 |
| [23] | Fu G F, Wang J, Kang J. Trans Nonferr Met Soc China, 2008; 18: 743 |
| [24] | Dreveton A. Procedia Eng, 2012; 46: 255 |
| [25] | Cao C N. Principles of Electrochemistry of Corrosion. Beijing: Chemical Industry Press, 2008: 104 (曹楚南. 腐蚀电化学原理. 北京: 化学工业出版社, 2008: 104) |
/
| 〈 |
|
〉 |