CORROSION BEHAVIOR OF PURE Mg BASED ON GENERATION/COLLECTION AND FEEDBACK MODES OF SCANNING ELECTROCHEMICAL MICROSCOPY

  • Xinyin WANG ,
  • Yan XIA ,
  • Yaru ZHOU ,
  • Linlin NIE ,
  • Fahe CAO ,
  • Jianqing ZHANG ,
  • Chunan CAO
Expand
  • Department of Chemistry, Zhejiang University, Hangzhou 310027

Received date: 2014-10-31

  Online published: 2015-07-23

Supported by

National Natural Science Foundation of China (Nos.51171172 and 51131005) and Fundamental Research Funds for the Central Universities (No.2015QNA3011)

Abstract

Since electrochemical impedance spectroscopy, polarization curve and hydrogen collection were the main technologies for corrosion research of Mg and its alloy. However, those methods only provide the mean information of entire surface of corrosion electrode. In this work, H2 evolution and active sites of pure Mg from localized sites (point, line and surface) in NaCl and Na2SO4 solution based on generation/collection and feedback modes of scanning electrochemical microscopy (SECM) were studied. The results indicate that both cathodic and anodic polarization are in favor of H2 evolution in NaCl and Na2SO4 solution, which is well in line with the negative difference effect by the classical H2 collection, but the SECM results show that the H2 evolution in localized sites is not uniform and stable. The H2 evolution rate increases with NaCl concentration increasing, which is opposite in Na2SO4 solution. The higher NaCl concentration, anodic polarization and lower pH value accelerate the formation of active sites on pure Mg surface.

Cite this article

Xinyin WANG , Yan XIA , Yaru ZHOU , Linlin NIE , Fahe CAO , Jianqing ZHANG , Chunan CAO . CORROSION BEHAVIOR OF PURE Mg BASED ON GENERATION/COLLECTION AND FEEDBACK MODES OF SCANNING ELECTROCHEMICAL MICROSCOPY[J]. Acta Metall Sin, 2015 , 51(5) : 631 -640 . DOI: 10.11900/0412.1961.2014.00602

References

[1] Cao C N. Principles of Electrochemistry of Corrosion. 3rd Ed., Beijing: Chemical Industry Press, 2008: 258 (曹楚南. 腐蚀电化学原理. 第三版, 北京: 化学工业出版社, 2008: 258)
[2] Song G, Atrens A, Stjohn D, Nairn J, Li Y. Corros Sci, 1997; 39: 855
[3] Baril G, Pébère N. Corros Sci, 2001; 43: 471
[4] Song G L. Corrosion and Protection of Magnesium Alloy. Beijing: Chemical Industry Press, 2006: 30 (宋光铃. 镁合金腐蚀与防护. 北京: 化学工业出版社, 2006: 30)
[5] Hampel C A. The Encyclypedia of Electrochemistry. New York: Reinhold, 1964: 341
[6] Petty R L, Davidson A W, Kleinberg J. J Am Chem Soc, 1954; 76: 363
[7] Makar G L, Kruger J. J Electrochem Soc, 1990; 137: 414
[8] Tunold R, Holtan H, Berge M B H, Lasson A, Steen-Hansen R. Corros Sci, 1977; 17: 353
[9] Bender S, Goellner J, Heyn A, Schmigalla S. Mater Corros, 2012; 63: 707
[10] Frankel G S, Samaniego A, Birbilis N. Corros Sci, 2013; 70: 104
[11] Kirkland N T, Birbilis N, Staiger M P. Acta Biomater, 2012; 8: 925
[12] Dra?i? D, Popi? J. J Appl Electrochem, 1999; 29: 43
[13] Liu W, Cao F, Xia Y, Chang L, Zhang J. Electrochim Acta, 2014; 132: 377
[14] Williams G, McMurray H N. J Electrochem Soc, 2008; 155: C340
[15] Taheri M, Kish J R, Birbilis N, Danaie M, McNally E A, McDermid J R. Electrochim Acta, 2014; 116: 396
[16] Taub I A, Roberts W, LaGambina S, Kustin K. J Phys Chem, 2002; 106A: 8070
[17] Straumanis M E, Bhatia B K. J Electrochem Soc, 1963; 110: 357
[18] King A, Birbilis N, Scully J. Electrochim Acta, 2014; 121: 394
[19] Tian Y, Yang L J, Li Y F, Wei Y H, Hou L F, Li Y G, Murakami R I. Trans Nonferrous Met Soc China, 2011; 21: 912
[20] Song G, Atrens A, John D S, Wu X, Nairn J. Corros Sci, 1997; 39: 1981
[21] Wang L, Shinohara T, Zhang B-P. J Alloys Compd, 2010; 496: 500
[22] Souto R M, González-Garc??a Y, González S. Corros Sci, 2005; 47: 3312
[23] El-Taib Heakal F, Shehata O S, Tantawy N S, Fekry A M. Int J Hydrogen Energy, 2012; 37: 84
[24] Curioni M. Electrochim Acta, 2014; 120: 284
[25] Winzer N, Atrens A, Dietzel W, Raja V S, Song G, Kainer K U. Mater Sci Eng, 2008; A488: 339
[26] Chen J, Wang J Q, Han E H, Ke W. Mater Sci Eng, 2008; A488: 428
[27] Chen J, Wang J Q, Han E H, Dong J H, Ke W. Corros Sci, 2008; 50: 1292
[28] Zhang T, Shao Y W, Meng G Z, Li Y, Wang F H. Electrochim Acta, 2006; 52: 1323
[29] Song R G, Blawert C, Dietzel W, Atrens A. Mater Sci Eng, 2005; A399: 308
[30] Carter T J, Cornish L A. Eng Fail Anal, 2001; 8: 113
[31] Song G, Atrens A. Adv Eng Mater, 2003; 5: 837
Outlines

/

〈 〉