EFFECTS OF B ON HIGH TEMPERATURE MECHA-NICAL PROPERTIES AND THERMAL FATIGUE BEHAVIOR OF COPPER DIE-CASTING DIE STEEL
Received date: 2014-10-30
Online published: 2015-07-23
Supported by
National Natural Science Foundation of China (No.50974080)
Copper die-casting die steel is usually used in severe rugged environment. Liquid metal flows with high temperature and high pressure during injection and provides rapid filling of the die cavity. The copper die-casting steel should has excellent combination of the properties of high toughness, wear resistance, hardness, thermal fatigue resistance, oxidation resistance and corrosion resistance at high temperature for the cavity surface of die-casting die suffers high pressure, scour, erosion and thermal shock. A new kind of copper alloy die-casting die steel with pure austenitic matrix was conducted in this work, wherein the boride with high thermal stability and high hardness distributes in the austenitic matrix. The mechanical properties of copper alloy die-casting die steel at high temperature of 850 ℃ were studied using dynamic thermal-mechanical simulation testing machine. The thermal fatigue behavior of die steel at room temperature to 800 ℃ was performed using self-restraint Uddeholm thermal fatigue test method, and the depth extension status of surface thermal fatigue cracks and cross-sectional cracks in die steel thermal fatigue specimens was measured using stereo microscope and SEM. The effects of B content on the mechanical properties at room temperature and high temperature and on the thermal fatigue resistance were evaluated. The experimental results showed that boride distributes in austenitic matrix in the form of M2B-type boride (M represents Fe, Cr or Mn) after adding B in the tested steels, and the comprehensive performances of steel at high temperatures were effectively improved, the hardness of the steel at room temperature increased from 200 HV to 302 HV, the tensile yield strength at 850 ℃ increased from 144.3 MPa to 190.3 MPa, and the compressive yield strength increased from 139.7 MPa to 167.9 MPa. Evaluation of the degree of heat checking on 300 cyc of thermal fatigue testing at room temperature to 800 ℃ showed that the die steel containing B was rating 2~3, much better than rating 7~8 of electroslag remelting ESR-H13 steel for comparison, which mainly because the thermal fatigue cracks were blunted or deflected by boride, and then the cracks spread as scattering shapes was avoided.
Key words: B; die-casting die steel; thermal fatigue property; copper alloy; die-casting
Zhisheng WANG , Xiang CHEN , Yanxiang LI , Huawei ZHANG , Yuan LIU . EFFECTS OF B ON HIGH TEMPERATURE MECHA-NICAL PROPERTIES AND THERMAL FATIGUE BEHAVIOR OF COPPER DIE-CASTING DIE STEEL[J]. Acta Metall Sin, 2015 , 51(5) : 519 -526 . DOI: 10.11900/0412.1961.2014.00591
| [1] | Cui K. Heat Treat Met, 2007; 32(1): 1 (崔 崑. 金属热处理, 2007; 32(1): 1) |
| [2] | Klobcar D, Tusek J, Taliat B. Mater Sci Eng, 2008; A472: 198 |
| [3] | Wallace F J, Schwam D. Die Cast Eng, 2000; 44(3): 50 |
| [4] | Zhu Y L, Schwan D, Wallace J F, Birceanu S. Mater Sci Eng, 2004; A379: 420 |
| [5] | Mesquita R A, Kestenbach H J. Mater Sci Eng, 2011; A528: 4856 |
| [6] | Medvedeva A, Bergstrom J, Gunnarsson S, Andersson J. Mater Sci Eng, 2009; A523: 39 |
| [7] | Li G B, Li X Z, Wu J J. J Mater Process Technol, 1998; 74: 23 |
| [8] | Persson A, Hogmark S, Bergstr?m J. J Mater Process Technol, 2004; 152: 228 |
| [9] | Kang J W, You R, Nie G, Hao X K, Long H M, Wang T J, Huang T Y. J Mech Eng, 2012; 48(12): 63 (康进武, 游 锐, 聂 刚, 郝小坤, 龙海敏, 王天骄, 黄天佑. 机械工程学报, 2012; 48(12): 63) |
| [10] | Persson A, Hogmark S, Bergstr M J. J Mater Process Technol, 2004; 148: 108 |
| [11] | Khader I, Renz A, Kailer A, Haas D. J Eur Ceram Soc, 2013; 33: 593 |
| [12] | Norstrom L. Scand J Metall, 1982; 11: 33 |
| [13] | Kariofillis G K, Kiourtsidis G E, Tsipas D N. Surf Coat Technol, 2006; 201: 19 |
| [14] | Chen Y W, Wu X C. J Iron Steel Res, 2010; 22(7): 42 (陈英伟, 吴晓春. 钢铁研究学报, 2010; 22(7): 42) |
| [15] | Cui K. Mater Mech Eng, 2001; 25(1): 1 (崔 崑. 机械工程材料, 2001; 25(1): 1) |
| [16] | Jiang Q C, Sui H L, Guan Q F. ISIJ Int, 2004; 44: 1103 |
| [17] | Sui H L. PhD Dissertation, Jilin University, Changchun, 2006 (隋鹤龙. 吉林大学博士学位论文, 长春, 2006) |
| [18] | Chen X, Zheng S, Yuan J Y. Procedia Eng, 2012; 27: 1780 |
| [19] | Chen X, Li Y X, Zhang H M. J Mater Sci, 2011; 46: 957 |
| [20] | Chen X, Li Y X. Mater Sci Eng, 2010; A528: 770 |
| [21] | Liu Z L, Li Y X, Chen X, Hu K H. Acta Metall Sin, 2007; 43: 477 (刘仲礼, 李言祥, 陈 祥, 胡开华. 金属学报, 2007; 43: 477) |
| [22] | Liu Z L, Li Y X, Chen X. China Foundry, 2012; 9: 313 |
| [23] | Chen X, Li Y X. Mater Sci Eng, 2007; A444: 298 |
| [24] | Li Y X, Liu Z L, Chen X. Int J Cast Met Res, 2008; 21: 67 |
| [25] | Liu Z L, Chen X, Li Y X. J Iron Steel Res Int, 2009; 16(3): 37 |
| [26] | Liu Z L, Li Y X, Chen X. Mater Sci Eng, 2008; A486: 112 |
| [27] | Liu Z L. PhD Dissertation, Tsinghua University, Beijing, 2007 (刘仲礼. 清华大学博士学位论文, 北京, 2007) |
| [28] | Chen X, Li Y X. China Foundry, 2013; 10: 155 |
| [29] | Benxi 1st Steelworks enxi 1st Steelworks. Boron Steel. Beijing: Metallurgical Industry Press, 1977: 39 (本溪钢铁公司第一炼钢厂. 硼钢. 北京: 冶金工业出版社, 1977: 39) |
| [30] | Guo C, Kelly P M. Mater Sci Eng, 2003; A352: 40 |
| [31] | Ma S Q, Xing J D, Liu G F, Yi D W, Fu H G, Zhang J J, Li Y F. Mater Sci Eng, 2010; A527: 6800 |
| [32] | Guo C Q. PhD Dissertation, The University of Queensland, Brisbane, 2002 |
| [33] | Chu Y Y, He X L, Tang L, Xu T D, Ke J. Acta Metall Sin, 1987; 23: 169 (褚幼义, 贺信莱, 唐 立, 徐庭栋, 柯 俊. 金属学报, 1987; 23: 169) |
| [34] | He X L, Chu Y Y, Ke J. Acta Metall Sin, 1983; 19: 459 (贺信莱, 褚幼义, 柯 俊. 金属学报, 1983; 19: 459) |
| [35] | Jahazi M, Jonas J J. Mater Sci Eng, 2002; A335: 49 |
| [36] | He X L, Chu Y Y, Tang L, Zhou Z X, Ke J. Acta Metall Sin, 1987; 23: 291 (贺信莱, 褚幼义, 唐 立, 周振新, 柯 俊. 金属学报, 1987; 23: 291) |
| [37] | Persson A, Hogmark S, Bergstr?m J. Int J Fatigue, 2004; 26: 1095 |
/
| 〈 |
|
〉 |