EFFECT OF PEARLITIC LAMELLA ORIENTATION ON DEFORMATION OF PEARLITE STEEL WIRE DURING COLD DRAWING

  • Lichu ZHOU ,
  • Xianjun HU ,
  • Chi MA ,
  • Xuefeng ZHOU ,
  • Jianqing JIANG ,
  • Feng FANG
Expand
  • 1 School of Materials Science and Engineering, Southeast University, Nanjing 211189
    2 Sha-Steel Iron and Steel Research Institute of Jiangsu Province, Zhangjiagang 215625
    3 Sunnywell (China) New Material Technology Co. Ltd., Changzhou 213200

Accepted date: 2015-04-02

  Online published: 2015-05-22

Supported by

Supported by National Natural Science Foundation of China (Nos.51371050 and 51301038), Fund of Transformation of Scientific and Technological Achievements from Jiangsu Province (No.BA2014088) and Fund of Prospective Study and Research from Jiangsu Province (No.BY2014127-03)

Abstract

Cold drawing pearlitic steel wires with ultra-high strength have important applications such as the automobile tire, springs rope and bridge cables. There have been many investigations which are paid attention to the hardening mechanisms of pearlitic steel wire, covering evolution of microstructure, texture and dislocation. In this work, effects of pearlitic lamella orientation on mechanical properties and deformation of pearlite steel wire in cold drawing were investigated by combining TEM, SEM and nano-indentor. The experimental results showed that pearlitic lamellae having low angle with drawing direction would be turned to parallel the drawing direction through a combined rotating process of pearlite colonies. The <110> fiber texture in the ferrite phase formed and the distribution of dislocations in ferrite was almost uniform. The deformation between cementite and ferrite was coordinated. Pearlitic lamellae having large angle with drawing direction would be bent and turned to parallel the drawing direction. It was difficult for the bent pearlite to deform because of the fragmentation of cementite and formation of dislocation cell in ferrite. After cold drawing process, the micro-hardness of straight pearlite was higher than that of bent pearlite. The result indicated that pearlitic lamellae having low angle with drawing direction have higher working-hardening rate in drawing.

Cite this article

Lichu ZHOU , Xianjun HU , Chi MA , Xuefeng ZHOU , Jianqing JIANG , Feng FANG . EFFECT OF PEARLITIC LAMELLA ORIENTATION ON DEFORMATION OF PEARLITE STEEL WIRE DURING COLD DRAWING[J]. Acta Metall Sin, 2015 , 51(8) : 897 -903 . DOI: 10.11900/0412.1961.2014.00620

References

[1] Michael Z. Acta Mater, 2002; 50: 4431
[2] Li Y J, Choi P, Goto S, Borchers C, Raabe D, Kirchheim R. Acta Mater, 2012; 60: 4005
[3] Read H G, Reynolods J W T, Hono K, Tarui T. Scr Mater, 1997; 37: 1221
[4] Zhang X, Godfrey A, Huang X, Hansen N, Liu Q. Acta Mater, 2011; 59: 3422
[5] Li Y J, Raabe D, Herbig M, Choi P, Goto S, Kostka A, Yarita H, Borchers C, Kirchheim R. Phys Rev Lett, 2014; 113: 106104
[6] Zhang X, Godfrey A, Hansen N, Huang X. Acta Mater, 2013; 61: 4898
[7] Zhao T Z, Song H W, Zhang G L, Cheng M, Zhang S H. Acta Metall Sin, 2014; 50: 667 (赵天章, 宋鸿武, 张光亮, 程 明, 张士宏. 金属学报, 2014; 50: 667)
[8] Liu Y D, Jiang Q W, Zhao X, Zuo L, Liang Z D. Acta Metall Sin, 2002; 38: 1215 (刘沿东, 蒋奇武, 赵 骧, 左 良, 梁志德. 金属学报, 2002; 38: 1215)
[9] Fang F, Zhao Y F, Liu P P, Zhou L C, Hu X J, Zhou X F, Xie Z. Mater Sci Eng, 2014; A608: 11
[10] Wong J N, Chu M B, Sei J O, Soon-Ju K. Scr Mater, 1997; 37: 1221
[11] Fang F, Zhao Y F, Zhou L C, Hu X J, Xie Z, Jiang J Q. Mater Sci Eng, 2014; A618: 505
[12] Languillaume J, Kapelski G, Baudele B. Acta Mater, 2000; 42: 457
[13] Wang Y, Fang F, Wang L, Jiang J Q, Yang H. Trans Mater Heat Treat, 2010; 31(5): 92 (王 燕, 方 峰, 王 雷, 蒋建清, 杨 恒. 材料热处理学报, 2010; 31(5): 92)
[14] Fang F, Hu X J, Chen S H, Xie Z, Jiang J Q. Mater Sci Eng, 2012; A547: 51
[15] Guo N, Luan B F, Liu Q. Mater Des, 2013; 50: 285
[16] Zhang X, Godfrey A, Hansen N, Huang X, Liu W, Liu Q. Mater Charact, 2010; 61: 65
[17] Liu Y D, Jiang Q W, Wang G, Wang Y D, Liang T D. J Mater Sci Technol, 2005; 21: 357
[18] Hu X J,?Wang?L, Fang,?F,?Ma Z Q,?Xie Z H,?Jiang J Q. J Mater Sci,?2013;?48:?5528
[19] Fang F, Jiang J Q, Tan S Y, Ma A B. Surf Coat Technol, 2010; 204: 2381
[20] Fang F, Hu X J, Zhang B M, Xie Z H, Jiang J Q. Mater Sci Eng, 2013; A583: 78
[21] Zhou L C, Zhao Y F, Hu X J, Wang L, Li F, Fang F, Jiang J Q. Chin J Mater Res, 2014; 28: 615 (周立初, 赵宇飞, 胡显军, 王 雷, 李 凡, 方 峰, 蒋建清. 材料研究学报, 2014; 28: 615)
[22] Zhang B M, Zhao Y F, Hu X J, Ma H, Fang F, Jiang J Q. Trans Mater Heat Treat, 2014; 35(1):115 (张必明, 赵宇飞, 胡显军, 麻 晗, 方 峰, 蒋建清. 材料热处理学报, 2014; 35(1): 115)
[23] Tomota Y, Suzuki T, Kanie A, Shiota Y, Uno M, Moriai A, Minakawa N, Morii Y. Acta Mater, 2005; 53: 463
[24] Won J N, Chu M B. Mater Sci Eng,1995; A203: 278
[25] Zhang X, Godfrey A, Huang X, Hansen N, Huang X X. Acta Mater, 2013; 61: 4898
Outlines

/

〈 〉