EFFECT OF 114 418 TEXTURE ON ABNORMAL GROWTH DURING SECONDARY RECRYSTALLI- ZATION IN GRAIN-ORIENTED STEEL

  • Zhiqiao LIU ,
  • Ping YANG ,
  • Weimin MAO ,
  • Feng'e CUI
Expand
  • School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083

Accepted date: 2015-04-27

  Online published: 2015-05-11

Supported by

Supported by National High Technology Research and Development Program of China (No.2012AA03A505)

Abstract

To find out the reason of poor secondary recrystallization behavior in thin-gauged grain-oriented steel, EBSD technique is applied to reveal the grain growth behavior of thin-gauged steel processed by HiB steel method under high cold-rolling reduction. Nitriding treatment with different times is conducted to ensure the occurrence of secondary recrystallization in thin-gauged grain-oriented steel and to determine the effect of nitrogen content. Attention is put on the influence of 114 418 texture on the abnormal growth of Brass and Goss grains. Results show that, at initial stage of secondary recrystallization, 114 418 grains in the surface region of sheets possess obvious growth advantage than the other oriented grains. If these grains in the surface region grew to the central layer of sheet and swallowed the nucleus of secondary recrystallization, abnormal growth could not occur. In contrast, reinforcing the inhibitors at surface region of sheet by nitriding treatment will avoid the excessive growth of surface grains and therefore improve magnetic properties of steel significantly. The {114}<418> grains are adverse to the abnormal growth of Brass-oriented and scattered Goss grains in way of island grains, but their effect on the abnormal growth of Goss grains is weaker.

Cite this article

Zhiqiao LIU , Ping YANG , Weimin MAO , Feng'e CUI . EFFECT OF 114 418 TEXTURE ON ABNORMAL GROWTH DURING SECONDARY RECRYSTALLI- ZATION IN GRAIN-ORIENTED STEEL[J]. Acta Metall Sin, 2015 , 51(7) : 769 -776 . DOI: 10.11900/0412.1961.2014.00665

References

[1] Goss N P. US Pat, 1965559, 1934
[2] Littmann M F, Heek J E. US Pat, 2599340, 1952
[3] Littmann M F. J Appl Phys, 1967; 38: 1104
[4] Park H K, Park C S, Na T W, Han C H, Hwang N M. Mater Trans JIM, 2012; 53: 658
[5] Yoshitomi Y, Ushigami Y, Harase J, Nakayama T, Masui H, Takahashi N. Mater Sci Forum, 1993; 113-115: 715
[6] Park J Y, Szpunar J A. Mater Sci Forum, 2002; 408-412: 821
[7] Hayakawa Y, Kurosawa M. Acta Mater, 2002; 50: 4527
[8] Nakashima S, Takashima K, Harase J. ISIJ Int, 1991; 31: 1013
[9] Yoshitomi Y, Masui H, Harase J, Takahashi N. Mater Trans JIM, 1995; 36: 1234
[10] Park J Y, Han K S, Woo J S, Chang S K, Rajmohan N, Szpunar J A. Acta Mater, 2002; 50: 1825
[11] Harase J, Shimizu R. J Magn Magn Mater, 2000; 215-216: 89
[12] Chang S K. Mater Sci Eng, 2007; A452-453: 93
[13] Matsuo M. ISIJ Int, 1989; 29: 809
[14] Yan M Q, Qian H, Yang P, Mao W M, Jian Q W, Jin W X. J Mater Sci Technol, 2011; 27: 1065
[15] Kumano T, Haratani T, Ushigami Y. ISIJ Int, 2003; 43: 736
[16] Shimazu T, Arai S, Sakai T, Tsubakino H. Tetsu Hagané, 2002; 88: 49 (岛津 高英, 新井 聪, 酒井 知彦, 椿野 晴繁. 铁と钢, 2002; 88: 49)
[17] Yan M Q, Qian H, Yang P, Song H J, Shao Y Y, Mao W M. Acta Metall Sin, 2012; 48: 16 (颜孟奇, 钱 浩, 杨 平, 宋惠军, 邵缓缓, 毛卫民. 金属学报, 2012; 48: 16)
[18] Gobernado P, Petrov R, Ruiz D, Leunis E, Kestens L A I. Adv Eng Mater, 2010; 12: 1077
[19] Lin P, Palumbo G, Harase J, Aust K T. Acta Mater, 1996; 44: 4677
[20] Oyarzábal M, Martínez-de-Guerenu A, Gutiérrez I. Mater Sci Eng, 2008; A485: 200
[21] Gobernado P, Petrov R H, Kestens L A I. Scr Mater, 2012; 66: 623
[22] Gobernado P, Petrov R H, Moerman J, Barbatti C, Kestens L A I. Mater Sci Forum, 2012; 702-703: 790
[23] Quadir M Z, Duggan B J. Acta Mater, 2004; 52: 4011
[24] Toge T, Muraki M, Komatsubara M, Obara T. ISIJ Int, 1998; 38: 524
[25] Nakamura S, Homma H. Mater Sci Forum, 2004; 467-470: 159
[26] Homma H, Nakamura S, Yoshinaga N. Mater Sci Forum, 2004; 467-470: 269
[27] Zhan N, Yang P, Mao W M. Acta Metall Sin, 2012; 48: 782 (张 宁, 杨 平, 毛卫民. 金属学报, 2012; 48: 782)
[28] Kumano T, Haratani T, Ushigami Y. ISIJ Int, 2003; 48: 400
[29] Rajmohan N, Szpunar J A. Scr Mater, 2001; 44: 2387
Outlines

/

〈 〉