INTERNAL FRICTION STUDY OF MECHANISM OF BAKE-HARDENING ON LOW CARBON STEEL

  • Weijuan LI ,
  • Hengyi ZHANG ,
  • Hao FU ,
  • Jianping ZHANG ,
  • Xiangyu QI
Expand
  • School of Materials and Metallurgy, University of Science and Technology Liaoning, Anshan 114051

Revised date: 2014-08-04

  Online published: 2015-05-01

Supported by

Supported by National Natural Science Foundation of China (No.51274121)

Abstract

High strength steel plates are being applied more extensively in automobile industry under higher demands of weight reduction, safety and environmental protection. As one of the high strength steel plates for automobile body panel, bake-hardening steel plate is featured by low yield strength and good formability during stamping, and is particularly featured by improved yield strength through following paint baking process, exhibiting higher strength and anti-dent ability in service. Bake-hardening (BH) is closely related to interactions between interstitial atoms and crystal defects during baking process. In this work, BH mechanisms in low carbon steel are studied under different annealing temperatures by measuring and analyzing stress-strain curves and BH values in baked conditions, and internal friction curves in both deformed and baked conditions. The results show that when the annealing temperature increases gradually from 750 to 880 ℃, the stress-strain curves exhibit discontinuous yielding behavior with stronger serration of yield platform and continuous elongation of yield point. With the increase of the annealing temperature from 750 to 780 ℃, BH value decreases, difference between Snoek peak values in deformed and baked conditions increases, SKK peak value decreases, and Kê peak value does not change significantly, which indicates that solid solution strengthening dominates the BH. When the annealing temperature increases from 780 to 880 ℃, BH value continuously increases, difference between Snoek peak values in deformed and baked conditions gradually decreases, relaxation strength of SKK peak gradually increases, and Kê peak is stable, which indicates that Cottrell atmosphere strengthening is playing an increasing role in the BH. The BH is due to a combined mechanism contributed by solid solution strengthening Cottrell atmosphere strengthening and precipitation strengthening.

Cite this article

Weijuan LI , Hengyi ZHANG , Hao FU , Jianping ZHANG , Xiangyu QI . INTERNAL FRICTION STUDY OF MECHANISM OF BAKE-HARDENING ON LOW CARBON STEEL[J]. Acta Metall Sin, 2015 , 51(4) : 385 -392 . DOI: 10.11900/0412.1961.2014.00434

References

[1] De A K, Vandeputte S, De Coomana B C. Scr Mater, 1999; 41: 831
[2] De A K, Blauwe K D, Vandeputteb S, De Cooman B C. J Alloys Compd, 2000; 310: 405
[3] Zhao J Z, De A K, De Cooman B C. ISIJ Int, 2000; 40: 725
[4] Speer G J, Matlock K D. JOM, 2002; 54(7): 19
[5] Jiang H T, Kang Y L, Yu H. Auto Technol Mater, 2005; (3): 1
[5] (江海涛, 康永林, 于 浩. 汽车工艺与材料, 2005; (3): 1)
[6] Zhao J Z, De A K, De Cooman B C. Metall Mater Trans, 2001; 32A: 417
[7] Baird J D. Int Mater Rev, 1971; 16(1): 1
[8] Vasilyev A A, Leeb H C, Kuzmin L N. Mater Sci Eng, 2008; A485: 282
[9] Zhao J Z, De A K, De Cooman B C. Mater Lett, 2000; 44: 374
[10] De A K, Vandeputte S, De Cooman B C. Scr Mater, 2001; 44: 695
[11] Cottrell A H, Bilby B A. Phys Soc London, 1949; 62(1)A: 49
[12] Soenen B, De A K, Vandeputte S, De Cooman B C. Acta Mater, 2004; 52: 3483
[13] Wert C, Marx J. Acta Metall, 1953; 1: 113
[14] Wert C A. Phys Rev, 1950; 79: 601
[15] Wert C A. Physics, 1949; 20: 943
[16] Bagramov R, Mari D, Benoit W. Philos Mag, 2001; 81A: 2797
[17] Ji J W, Yu N. Prog Phys, 2006; 26: 296
[17] (戢景文, 于 宁. 物理学进展, 2006; 26: 296)
[18] Fang Q F, Wang X P, Wu X B, Lu H. Physics, 2011; 40: 786
[18] (方前锋, 王先平, 吴学邦, 鲁 卉. 物理, 2011; 40: 786)
[19] Ji J W, Liu F D, Wang D J, Che Y Y, Hua Q Z, Liu J M, Huang Z R. Acta Metall Sin, 1999; 35: 913
[19] (戢景文, 刘芬娣, 王登京, 车韵怡, 华桥柱, 刘建民, 黄镇如. 金属学报, 1999; 35: 913)
[20] Yu N, Liu Y G, Zhang Z B, Zhan H, Zhang J, Ji J W. J ShangHai JiaoTong Univ, 2010; 44: 624
[20] (于 宁, 刘永刚, 张志波, 詹 华, 张 建, 戢景文. 上海交通大学学报, 2010; 44: 624)
[21] Che Y Y, Sun Y J, Ji J W. J Northeastern Univ (Nat Sci), 1997; 18: 676
[21] (车韵怡, 孙玉杰, 戢景文. 东北大学学报(自然科学版), 1997; 18: 676)
[22] Che Y Y, Liu F D, Zeng G Y, Xu Y C, Ji J W. Acta Metall Sin, 1998; 34: 831
[22] (车韵怡, 刘芬娣, 曾桂仪, 许余昌, 戢景文. 金属学报, 1998; 34: 831)
[23] Yu N, Ji J W. Acta Metall Sin, 2002; 38: 230
[23] (于 宁, 戢景文. 金属学报, 2002; 38: 230)
[24] Ge T S. Solid Internal Friction Theoretical Basis. Beijing: Science Press, 2000: 62
[24] (葛庭燧. 固体内耗理论基础. 北京: 科学出版社, 2000: 62)
[25] De A K, Vandeputte S, De Cooman B C. J Mater Eng Perform, 2001; 10: 567
Outlines

/

〈 〉