EFFECT OF Si ADDITION ON THE MICROSTRUCTURE AND ROOM TEMPERATURE TENSILE PROPERTIES OF HIGH Nb-TiAl ALLOY

  • Liang YANG ,
  • Shubo GAO ,
  • Yanli WANG ,
  • Teng YE ,
  • Lin SONG ,
  • Junpin LIN
Expand
  • State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083

Accepted date: 2015-03-23

  Online published: 2015-04-15

Supported by

Supported by National Basic Research Program of China (No.2011CB605500) and National Natural Science Foundation of China (No.51271016)

Abstract

High Nb-TiAl alloys, which being regarded as a new generation TiAl alloy, had attracted more and more attention for their higher operating temperature and better oxidation resistance than conventional TiAl alloys. It was found that silicide particles in high Nb-TiAl alloys were Nb5Si3 rather than Ti5Si3 precipitated in TiAl alloys. In this work, the effect of Nb5Si3 phase on the microstructure and room-temperature tensile properties of high Nb-TiAl alloy was studied. The experimental results showed that the precipitation temperature of silicide was between 1000~1200 ℃. Precipitates located in the colony boundary, b(B2) segregation and between g/a2 lamella. The tensile properties of as-cast alloy with Si addition increased. Because the formation of Nb5Si3 precipitates resulted in the reduction of Nb content, which was one of b(B2) phase stable elements. Therefore, the volume fraction of b(B2) phase obviously decreased due to Si addition. However, after heat treatments, the tensile properties of Si containing high Nb-TiAl alloy gradually reduced with the increasing of heat treatment temperature. Silicide particles which precipitated along lamella leaded to generation and propagation of cracks. Moreover, silicide particles further precipitated due to tensile stress which increased the rate of crack propagation. Si addition leaded to g phase area expanded. g single-phase region formed between 1280~1300 ℃. Silicide precipitated in colony boundary resulted in bulk g+b(B2) phases, which weaken the grain boundaries. While silicide precipitated in lamella leaded to formation of secondary g lath which split the initial lamella microstructure.

Cite this article

Liang YANG , Shubo GAO , Yanli WANG , Teng YE , Lin SONG , Junpin LIN . EFFECT OF Si ADDITION ON THE MICROSTRUCTURE AND ROOM TEMPERATURE TENSILE PROPERTIES OF HIGH Nb-TiAl ALLOY[J]. Acta Metall Sin, 2015 , 51(7) : 859 -865 . DOI: 10.11900/0412.1961.2015.00075

References

[1] Kim Y W. Mater Sci Eng, 1995; A192-193: 519
[2] Loria E A. Intermetallics, 2000; 8: 1339
[3] Dimiduk D M. Mater Sci Eng, 1999; A263: 281
[4] Imayev R M, Imayev V M, Oehring M, Appel F. Intermetallics, 2007; 15: 451
[5] Yoshihara M, Miura K. Intermetallics, 1995; 3: 357
[6] Liu Z C, Lin J P, Li S J, Chen G L. Intermetallics, 2002; 10: 653
[7] Zollinger J, Witusiewicz V, Drevermann A, Daloz D, Hecht U. Int J Cast Metal Res, 2009; 22: 339
[8] Jin Y G, Wang J N, Yang J, Wang Y. Scr Mater, 2004; 51: 113
[9] Paul J D H, Appel F, Wagner R. Acta Mater, 1998; 46: 1075
[10] Beschliesser M, Chatterjee A, Lorich A, Knabl W, Kestler H, Dehm G, Clemens H. Mater Sci Eng, 2002; A329-331: 124
[11] Lin J P, Xu X J, Wang Y L, He S F, Zhang Y, Song X P, Chen G L. Intermetallics, 2007; 15: 668
[12] Huang Z W, Cong T. Intermetallics, 2010; 18: 161
[13] Wang J G, Nieh T G. Intermetallics, 2000; 8: 737
[14] Zhang W, Liu Y, Huang J S, Liu B, He Y H, Huang B Y. Rare Metal Mater Eng, 2009; 38: 1711
[15] Xu Z F, Xu X J, Lin J P, Zhang Y, Wang Y L, Lin Z, Chen G L. J Mater Eng, 2007; (9): 42 (许正芳, 徐向俊, 林均品, 张 勇, 王艳丽, 林 志, 陈国良. 材料工程, 2007; (9): 42)
[16] Hsu F Y, Wang G X, Klaar H J. Scr Metall Mater, 1995; 33: 597
[17] Gouma P I, Subramanian K, Kim Y W, Mills M J. Intermetallics, 1998; 6: 689
[18] Wunderlich W, Kremser T, Frommeyer G. Z Metallkd, 1990; 81: 802
[19] Wang G X, Dogan B, Hsu F Y, Klaar H J, Dahms M. Metall Mater Trans, 1995; 26A: 691
[20] Hornauer U, Richter E, Matz W, Reuther H, Mucklich A, Wieser E, Moller W, Schumacher G, Schutze M. Surf Coat Technol, 2000; 128-129: 418
[21] Dong L M, Cui Y Y, Yang R, Wang F H. Acta Metall Sin, 2004; 40: 383 (董利民, 崔玉友, 杨 锐, 王福会. 金属学报, 2004; 40: 383)
[22] Kim Y W, Kim S L. Intermetallics, 2014; 53: 92
[23] Karadge M, Kim Y W, Gouma P I. Metall Mater Trans, 2003; 34A: 2129
[24] Sun F S, Kim S E, Cao C X, Lee Y T, Yan M G. Scr Mater, 2001; 45: 383
[25] Chen G L, Zhang W J, Liu Z C, Li S J, Kim Y W. In: Kim Y W, Dimiduk D M, Loretto M H eds., Gamma Titanium Aluminides 1999, Warrendale, PA: TMS, 1999: 31
[26] Wang Y H, Lin J P, He Y H, Wang Y L, Chen G L. Mater Sci Eng, 2007; A471: 82
[27] Gouma P I, Karadge M. Mater Lett, 2003; 57: 3581
Outlines

/

〈 〉