EFFECT OF Mo CONTENT ON THE MICROSTRUC-TURE AND PROPERTIES OF CrMoN COMPOSITE COATINGS

  • Dongli QI ,
  • Hao LEI ,
  • Di FAN ,
  • Zhiliang PEI ,
  • Jun GONG ,
  • Chao SUN
Expand
  • Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Revised date: 2014-10-08

  Online published: 2015-03-25

Supported by

Supported by National Basic Research Program of China (No.2012CB625100), National Natural Science Foundation of China (No.51171197) and Natural Science Foundation of Liaoning Province ( Nos.2013020132 and 2013010442-401)

Abstract

Ceramic coatings are usually used as protective coatings to improve performance and durability of tools and components now. Compared with conventional TiN based hard coating, CrN based coating like Cr-X-N (X=Ti, Al, Si, C, B, Ta, Nb, Ni) is a more interesting choice because of low friction coefficient, superior oxidation resistance and excellent corrosion resistance under severe environment conditions. The CrMoN is among these coatings and attractive since self-lubricating phase MoO3 may be formed in tribological process. However the effect of Mo content on structure and tribological properties of CrMoN coatings is not still clear. In the present study, CrMoN composite coatings with different Mo content were deposited on M2 high speed steel (HSS) substrates by DC reactive magnetron sputtering. The effect of Mo content on the microstructure and properties was investigated systematically, including the chemical composition, phase structure, chemical valence, cross-section morphologies, microhardness and tribological properties. The results showed that the phase transformation of the as-deposited coatings occurred with the increase of Mo content. The phase structure changed to (Cr, Mo)N substitutional solid solution based on CrN-type firstly, and then to mixed phase with g-Mo2N as main phase, and a small amount of elemental bcc-Mo phase appeared when the Mo content is 69.3%. The microhardness of the CrMoN composite coatings always increased until the highest hardness when the Mo content reached to 45.4%, and then decreased; a relatively low friction coefficient was obtained compared with that of the CrN coating when more than 45.4%Mo content was doped. The reason is that the more MoO3 lubricant phase could be formed in tribological process.

Cite this article

Dongli QI , Hao LEI , Di FAN , Zhiliang PEI , Jun GONG , Chao SUN . EFFECT OF Mo CONTENT ON THE MICROSTRUC-TURE AND PROPERTIES OF CrMoN COMPOSITE COATINGS[J]. Acta Metall Sin, 2015 , 51(3) : 371 -377 . DOI: 10.11900/0412.1961.2014.00549

References

[1] Navinšek B, Panjan P, Milošev I. Surf Coat Technol, 1997; 97: 182
[2] Barshilia H C, Selvakumar N, Deepthi B, Rajam K S. Surf Coat Technol, 2006; 201: 2193
[3] Budna K P, Neidhardt J, Mayrhofer P H, Mitterer C. Vacuum, 2008; 82: 771
[4] Choi E Y, Kang M C, Kwon D H, Dong Woo, Kim K H. Mater Processing Technol, 2007; 188: 566
[5] Homhuan P, Chaiyakun S, Thonggoom R, Panich N, Tungasmita S. Mater Trans, 2010; 51: 1651
[6] Benkahoul M, Robin P, Gujrathi S C, Martinu L, Klemberg-Sapieha J E. Surf Coat Technol, 2008; 202: 3975
[7] Fuentes G G, de Cerio M J D, Garcia J A, Martinez R, Bueno R, Rodriguez R J, Rico M, Montala F, Qin Y. Surf Coat Technol, 2008; 203: 670
[8] Kim K H, Choi E Y, Hong S G, Park B G, Yoon J H, Yong J H. Surf Coat Technol, 2006; 201: 4068
[9] Lyo I W, Ahn H S, Lim D S. Surf Coat Technol, 2003; 163: 413
[10] Suszko T, Gulbinski W, Jagielski J. Surf Coat Technol, 2005; 194: 319
[11] Tian S F. PhD Dissertation, Harbin Institute of Technology, 2013
[11] (田首夫. 哈尔滨工业大学博士学位论文, 2013)
[12] Jacob K T, Raj S, Rannesh L. Int J Mater Res, 2007; 98: 776
[13] Fang Q F, Yang J F, Yuan Z G, Zhang G G, Wang X P. Mater Res Bull, 2009; 44: 1948
[14] Bertóti I. Surf Coat Technol, 2002; 151-152: 194
[15] Sanjinés R, Wiemer C, Almeida J, Lévy F. Thin Solid Films, 1996; 290-291: 334
[16] de Vries J E, Yao H C, Baird R J, Gandhi H S. J Catal, 1983; 84: 8
[17] Liu C H, Du X S, Wang D Z, Huang N K, Yang B. J Funct Mater, 2007; 38: 176
[17] (刘春海, 杜晓松, 汪德志, 黄宁康, 杨 斌. 功能材料, 2007; 38: 176)
[18] Wan X S, Zhao S S, Yang Y, Gong J, Sun C. Surf Coat Technol, 2010; 204: 1800
[19] Pande C S, Masumura R A, Armstrong R W. Nanostruct Mater, 1993; 2: 323
[20] Wang C C, Peng C Q, Feng Y, Wei X F. Chin J Nonferrous Met, 2012; 22: 1945
[20] (王常川, 彭超群, 冯 艳, 韦小凤. 中国有色金属学报, 2012; 22: 1945)
[21] Blau P J. Wear, 1982; 81: 187
Outlines

/