IMPROVING THE INTERGRANULAR CORROSION RESISTANCE OF THE WELD HEAT-AFFECTED ZONE BY GRAIN BOUNDARY ENGINEERING IN 304 AUSTENITIC STAINLESS STEEL

  • Hui YANG ,
  • Shuang XIA ,
  • Zilong ZHANG ,
  • Qing ZHAO ,
  • Tingguang LIU ,
  • Bangxin ZHOU ,
  • Qin BAI
Expand
  • 1 Institute of Materials, Shanghai University, Shanghai 200072
    2 Key Laboratory for Microstructure, Shanghai University, Shanghai 200444

Revised date: 2014-10-09

  Online published: 2015-03-25

Supported by

Supported by National Basic Research Program of China (No.2011CB610502) and Shanghai Science and Technology Commission Key Support Project (No.13520500500)

Abstract

The heat-affected zone (HAZ) produced by welding in stainless steel has higher susceptibility to intergranular corrosion, which is attributed to the Cr depletion induced by grain-boundary carbide-precipitation. The grain boundary engineering can be used to control over the grain boundary structure, which has significant influence on the carbide precipitation and the associated Cr depletion and hence on the susceptibility to intergranular corrosion. The grain boundary network in a 304 austenite stainless steel can be controlled by grain boundary engineering (GBE) with 5% tensile deformation and subsequent annealing at 1100 ℃ for 30 min. The total length proportion of Σ3n coincidence site lattice (CSL) boundaries was increased to more than 75%, and the large-size highly-twinned grain-cluster microstructure was formed through the treatment of GBE. Specimens were welded by gas tungsten arc-welding. Then the microstructure and the corrosion resistance of HAZ were characterized. The result showed that the high proportion of low ΣCSL boundaries and the optimum grain boundary character distribution were stable in the HAZ of the grain boundary engineered stainless steel, and the grain size was nearly the same. The weld-decay region of GBE samples performed better intergranular corrosion resistance during the intergranular corrosion immersion experiment and electrochemical potentiokinetic reactivation (EPR) test. The reported results indicated that the grain boundary engineering can effectively improve the intergranular corrosion resistance of the heat-affected zone in 304 austenitic stainless steel.

Cite this article

Hui YANG , Shuang XIA , Zilong ZHANG , Qing ZHAO , Tingguang LIU , Bangxin ZHOU , Qin BAI . IMPROVING THE INTERGRANULAR CORROSION RESISTANCE OF THE WELD HEAT-AFFECTED ZONE BY GRAIN BOUNDARY ENGINEERING IN 304 AUSTENITIC STAINLESS STEEL[J]. Acta Metall Sin, 2015 , 51(3) : 333 -340 . DOI: 10.11900/0412.1961.2014.00552

References

[1] Yang W D. Nuclear Reactor Materials Science. Beijing: Atomic Energy Press, 2000: 195
[1] (杨文斗. 反应堆材料学. 北京: 原子能出版社, 2000: 195)
[2] Trillo E A, Murr L E. Acta Mater, 1998; 47: 235
[3] Zhou Y, Aust K T, Erb U, Palumbo G. Scr Mater, 2001; 45: 49
[4] Kokawa H, Shimada M, Michiuchi M, Wang Z J, Sato Y S. Acta Mater, 2007; 55: 5401
[5] Zhou Z F. Welding Metallurgy. Beijing: Mechanical Industry Press, 2001: 68
[5] (周振丰. 焊接冶金学. 北京: 机械工业出版社, 2001: 68)
[6] Li Y J. Welding of Structural Alloy Steel and Stainless Steel. Beijing: Chemical Industry Press, 2012: 218
[6] (李亚江. 合金结构钢及不锈钢的焊接. 北京: 化学工业出版社, 2012: 218)
[7] Watanable T. Res Mech, 1984; 11: 47
[8] Kronberg M L, Wilson F H. Trans AIME, 1949; 185: 501
[9] Randle V. Acta Mater, 2004; 52: 4067
[10] Lehockey E M, Limoges D, Palumbo G, Sklarchuk J, Tomantscher K, Vincze A. J Power Sour, 1999; 78: 79
[11] Thaveeprungsriporn V, Was G S. Metall Trans, 1997; 28: 2101
[12] Xia S, Zhou B X, Chen W J, Wang W G. Scr Mater, 2006; 54: 2019
[13] Xia S, Zhou B X, Chen W J. J Mater Sci, 2008; 43: 2990
[14] Xia S, Zhou B X, Chen W J. Metall Mater Trans, 2009; 40A: 3016
[15] Xia S, Zhou B X, Chen W J, Wang W G. Acta Metall Sin, 2006; 42: 129
[15] (夏 爽, 周邦新, 陈文觉, 王卫国. 金属学报, 2006; 42: 129)
[16] Wang W G, Zhou B X, Feng L, Zhang X, Xia S. Acta Metall Sin, 2006; 42: 715
[16] (王卫国, 周邦新, 冯 柳, 张 欣, 夏 爽. 金属学报, 2006; 42: 715)
[17] Hu C L, Xia S, Li H, Liu T G, Zhou B X, Chen W J. Acta Metall Sin, 2011; 47: 939
[17] (胡长亮, 夏 爽, 李 慧, 刘廷光, 周邦新, 陈文觉. 金属学报, 2011; 47: 939)
[18] Hu C L, Xia S, Li H, Liu T G, Zhou B X, Chen W J, Wang N. Corros Sci, 2011; 53: 1880
[19] Fang X Y, Zhang K, Guo H, Wang W G, Zhou B X. Mater Sci Eng, 2008; A487: 7
[20] Shimada M, Kokawa H, Wang Z J, Sato Y S, Karibe I. Acta Mater, 2002; 50: 2331
[21] Brandon D G. Acta Mater, 1966; 14: 1479
[22] Palumbo G, Aust K T, Lehockey E M. Scr Mater, 1998; 38: 1685
[23] de Lima-Neto P, Farias J P, Abreu H F G. Corros Sci, 2008; 50: 1149
[24] Arutunow A, Darowicki K. Electrochim Acta, 2009; 54: 1034
[25] Aydodu G H, Aydinol M K. Corros Sci, 2006; 48: 3565
[26] Yu X, Chen S, Liu Y, Ren F. Corros Sci, 2010; 52: 1939
[27] Leiva-García R, Mu?oz-Portero M J, García-Antón J. Corros Sci, 2009; 51: 2080
[28] Bi H Y, Kokawa H, Wang Z J. Scr Mater, 2003; 49: 21
[29] Li H, Xia S, Zhou B X, Chen W J, Hu C L. J Nucl Mater, 2010; 399: 108
Outlines

/

〈 〉