EFFECTS OF ELECTROMAGNETIC STIRRING WITH LOW CURRENT FREQUENCY ON RE DISTRIBUTION IN SEMISOLID ALUMINUM ALLOY

  • Zheng LIU ,
  • Xiaomei LIU ,
  • Tao ZHU ,
  • Qingchun CHEN
Expand
  • 1 School of Mechanical and Electrical Engineering, Jiangxi University of Science and Technology, Ganzhou 341000
    2 School of Material Science and Engineering, Jiangxi University of Science and Technology, Ganzhou 341000

Revised date: 2014-06-30

  Online published: 2015-03-25

Supported by

Supported by National Natural Science Foundation of China (No.51361012), Natural Science Foundation of Jiangxi Province (No.20114bab206014) and Science and Technology Program of the Education Department of Jiangxi Province (No.GJJ14407)

Abstract

When solidification of Al alloy melt was disturbed by electromagnetic field, its microstructure and properties were influenced by the diffusion and distribution of the solute and refinement in the melt. So it was necessary to study the metallurgical behavior of RE with electromagnetic stirring and to probe its diffusion and distribution under the forced convection in the melt. The magnetic induction intensity in the electromagnetic crystallizer and its variations with current frequency were simulated by Maxwell 2D software. The distribution of RE in the A356-Y alloy melt and its effect to the microstructure were studied with low frequency electromagnetic stirring. The results indicated that current frequency with stronger magnetic induction could be obtained during the range of low frequency under the working frequency. The slurry of semisolid A356-Y alloy was prepared by electromagnetic stirring at the frequency. The size and shape factor of the primary phase in the alloy were below 65 mm and above 0.80, respectively, which could satisfy the requirement of semisolid alloy rheoforming. The distribution of Y enriched at the edge of the ingot along its radius direction by the driving of electromagnetic field, but was effected by the frequency. Y presented the enriching at the edge of the ingot with the increase of the frequency under the range of the frequency tested.

Cite this article

Zheng LIU , Xiaomei LIU , Tao ZHU , Qingchun CHEN . EFFECTS OF ELECTROMAGNETIC STIRRING WITH LOW CURRENT FREQUENCY ON RE DISTRIBUTION IN SEMISOLID ALUMINUM ALLOY[J]. Acta Metall Sin, 2015 , 51(3) : 272 -280 . DOI: 10.11900/0412.1961.2014.00347

References

[1] Li T J, Wen B, Zhang Z F, Jin J Z. J Dalian Univ Technol, 2000; 40(s1): 61
[1] (李廷举, 温 斌, 张志峰, 金俊泽. 大连理工大学学报, 2000; 40(增刊1): 61)
[2] Bai Y F, Zhou Y M, Yan B, Zhang Y J, Xu D M, Guo J J, Fu H Z. Foundry, 2008; 57: 105
[2] (白云峰, 周月明, 严 彪, 张永杰, 徐达鸣, 郭景杰, 傅恒志. 铸造, 2008; 57: 105)
[3] Barman N, Kumar P, Dutta P. J Mater Process Technol, 2009; 209: 5912
[4] Liu Z, Hu Y M, Liu X M. Acta Metall Sin (Engl Lett), 2010; 23: 277
[5] Maja V, Stanislav K, Primo M, Jo?ef M. J Alloys Compd, 2011; 509: 7349
[6] Wan D Q. Rare Met, 2010; 29: 460
[7] Nogita K, Yasuda H, Yoshiya M. J Alloys Compd, 2010; 489: 415
[8] Kaur P, Dwivedi D K, Pathak P M. Int J Adv Manuf Technol, 2012; 58: 219
[9] Yurko J A. Die Cast Eng, 2002; (4): 20
[10] Mao W M, Bai Y L, Tang G X. J Mater Sci Technol, 2006; 22: 447
[11] Zuo Y B, Zhao Z H, Zhu Q F, Cui J Z. Chin J Nonferrous Met, 2013; 23: 51
[11] (左玉波, 赵志浩, 朱庆丰, 崔建忠. 中国有色金属学报, 2013; 23: 51)
[12] Liu Z, Mao W M, Zhao Z D. Trans Nonferrous Met Soc China, 2006; 16: 71
[13] Liu Z, Mao W M, Zhao Z D. Acta Metall Sin, 2009; 45: 507
[13] (刘 政, 毛卫民, 赵振铎. 金属学报, 2009; 45: 507)
[14] Liu Z, Wang F Y, Cao K, Xu H B, Huang M Y. Adv Mater Res, 2012; 430-432: 886
[15] Yao C F, Guo X P, Guo H S. Acta Metall Sin, 2008; 44: 579
[15] (姚成方, 郭喜平, 郭海生. 金属学报, 2008; 44: 579)
[16] Prodhan A, Sivaramakrishnan C S, Chakrabarti A K. Metall Mater Trans, 2001; 32B: 372
[17] Dao V L, Zhao S D, Lin W J. J Mech Eng, 2012; 48(14): 50
[17] (陶文琉, 赵升吨, 林文捷. 机械工程学报, 2012; 48(14): 50)
[18] Zhang B J, Cui J Z, Lu G M, Zhang Q, Ban C Y. Acta Metall Sin, 2002; 38: 215
[18] (张北江, 崔建忠, 路贵民, 张 勤, 班春燕. 金属学报, 2002; 38: 215)
[19] Barman N, Dutta P. Trans Indian Inst Met, 2009; 62: 469
[20] Chen D D, Zhang H T, Wang X J, Cui J Z. Acta Metall Sin, 2011; 47: 185
[20] (陈丹丹, 张海涛, 王向杰, 崔建中. 金属学报, 2011; 47: 185)
[21] Vives C. Metall Trans, 1992; 23B: 189
[22] Chen X R, Zhang Z F, Xu J, Shi L K. Chin J Nonferrous Met, 2010; 20: 937
[22] (陈兴润, 张志峰, 徐 骏, 石力开. 中国有色金属学报, 2010; 20: 937)
[23] Yang M S, Zhao A M, Mao W M, Gao J F, Zhong X Y. J Iron Steel Res, 2003; 15(4): 18
[23] (杨卯生, 赵爱民, 毛卫民, 高军芳, 钟雪友. 钢铁研究学报, 2003; 15(4): 18)
[24] Takamichi I,Roderick I L G. The Physical Properties of Liquid Metals. New York: Oxford University Press Inc., 1988: 255
[25] Sun Q X, Zhong Y B, Ren Z M, Lou L, Deng K, Xu K D. Acta Metall Sin, 2005; 41: 321
[25] (孙秋霞, 钟云波, 任忠鸣, 楼 磊, 邓 康, 徐匡迪. 金属学报, 2005; 41: 321)
[26] Kang C G, Bae J W, Kim B M. J Mater Process Technol, 2007; 187-188: 344
[27] Willers B, Eckert S, Nikrityuk P A, Rabiger D, Dong J, Eckert K, Gerbeth G. Metall Mater Trans, 2008; 39B: 304
[28] Chung I G, Bolouri A, Kang C G. Int J Adv Manuf Technol, 2012; 58: 237
[29] Meng X H, Chen C L, Hong Z Y, Wang J Y. Sci China, 2006; 49E: 274
[30] Kaur P, Dwivedi D K, Pathak P M. Int J Adv Manuf Technol, 2012; 63: 415
Outlines

/

〈 〉