DEVELOPMENT OF HIGH STRENGTH ALUMINUM ALLOYS AND PROCESSING TECHNIQUES FOR THE MATERIALS

  • Xinming ZHANG ,
  • Yunlai DENG ,
  • Yong ZHANG
Expand
  • School of Materials Science and Engineering, Central South University, Changsha 410083

Received date: 2014-06-30

  Online published: 2015-03-25

Supported by

Supported by National Basic Research Program of China (No.2012CB619500)

Abstract

The fundamental theories for the development of high strength aluminum alloys and processing techniques for the materials are briefly reviewed in this paper. It specifically focuses on alloying design, casting, homogenization, solution treatment, quenching, pre-stretching and ageing that have been extensively studied recently. Based on these discussions, some perspectives and suggestions have been proposed, which will benefit the development and applications of high strength aluminum alloys.

Cite this article

Xinming ZHANG , Yunlai DENG , Yong ZHANG . DEVELOPMENT OF HIGH STRENGTH ALUMINUM ALLOYS AND PROCESSING TECHNIQUES FOR THE MATERIALS[J]. Acta Metall Sin, 2015 , 51(3) : 257 -271 . DOI: 10.11900/0412.1961.2014.00406

References

[1] Mondolfo L F,translated by Wang Z T,Zhang Z L,Zhen X. Microstructure and Properties of Aluminum Alloy. Beijing: Metallurgical Industry Press, 1988: 1
[1] (Mondolfo L F 著,王祝堂,张振录,郑璇译. 铝合金的组织与性能. 北京: 冶金工业出版社, 1988: 1)
[2] Polmear I J. Light Alloys: Metallurgy of the Light Metals. 4th Ed., Melbourne: Elsevier′s Science and Technology, 2006: 1
[3] Immarigeon J P, Holt R T, Koul A K, Zhao L, Wallace W, Beddoes J C.?Mater Charact, 1995; 35: 41
[4] Rioja R J, Liu J. Metall Mater Trans, 2012; 43A: 3325
[5] Heinz A, Haszler A, Keidel C, Moldenhauer S, Benedictus R, Miller W S. Mater Sci Eng, 2000; A280: 102
[6] Wilm A. Metall: Zeitschrift für die Gesamte Hüttenkunde, 1911; 8: 225
[7] Sander W, Meissner K L. Zeitschrift für Metallkunde, 1923; 15: 181
[8] Aluminum Association. International Alloy Designations and Chemical Composition Limits for Wrought Aluminum and Wrought Aluminum Alloys. Arlington, Virginia: The Aluminum Association, 2006: 1
[9] Yao J S, Cai Y F, Li C G. Aero Manuf Technol, 2007; (10): 36
[9] (姚君山, 蔡益飞, 李程刚. 航空制造技术, 2007; (10): 36)
[10] Starke Jr E A, Staley J T. Prog Aerosp Sci, 1996; 32: 131
[11] Fisher J J, Kramer L S, Pickens J R. Adv Mater Processes, 2002; 160(9): 43
[12] Rioja R J. Mater Sci Eng, 1998; A257: 100
[13] Peel C J, Evans B, Mcdarmaid D. In: Davis J R ed., Proc Third Aluminium-Lithiun Conference, Materials Park, OH: ASM International, 1986: 26
[14] Bretz P E, Sawtell R R. In: Davis J R ed., Proc Third Aluminium-Lithiun Conference, Materials Park, OH: ASM International, 1986: 47
[15] Burton C L, Mayer L W, Spuhler E H. In: Van Horn K R ed., Aircraft and Aerospace Applications. Vol.2, Materials Park, OH: American Society for Metals, 1967: 1
[16] Fridlyander I N, Sandler V S, Nikolskaya T I. Met Sci Heat Treat, 1983; 25: 495
[17] Friedlander I N, Bratukhin A G, Davydov V A. Soviet Al-Li Alloys of Aerospace Applications. Garmisch-Partenkirchen: DMG Verlag, 1992: 1
[18] Aerospace Material Specification, AMS 4252, sae, March, 1999
[19] Aerospace Material Specification, AMS 4206A, sae, Jan., 1999
[20] Williams J C, Starke J E A. Acta Mater, 2003; 51: 5775
[21] Aerospace Material Specification, AMS 4296, Aug., 2003
[22] Shi Y J, Pan Q L, Li M J, Huang X, Li B. J Alloys Compd, 2012; 612: 42
[23] Wen S P, Gao K Y, Li Y, Huang H, Nie Z R. Scr Mater, 2011; 65: 592
[24] Wen S P, Xing Z B, Huang H, Li B L, Wang W, Nie Z R. Mater Sci Eng, 2009; A516: 42
[25] Nie Z R, Wen S P, Huang H, Li B L, Zuo T Y. Chin J Nonferrous Met, 2011; 21: 2361
[25] (聂祚仁, 文胜平, 黄 晖, 李伯龙, 左铁镛.中国有色金属学报, 2011; 21: 2361)
[26] Zhou X W, Liu Z Y, Bai S, Liu M, Ying P Y. Mater Sci Eng, 2013; A564: 186
[27] Kalu P N, Waller E A. Scr Mater, 1998; 39: 1599
[28] Hamilton B C, Saxena A. Eng Fract Mech, 1999; 62: 1
[29] Kermanidis A T, Zervaki A D, Haidemenopoulos G N, Pantelakis S G. Mater Des, 2010; 31: 42
[30] Vural M, Caro J. Mater Sci Eng, 2009; A520: 56
[31] Fridlyander I N. Met Sci Heat Treat, 2001; 43: 6
[32] Prasad N E, Gokhale A A, Wanhill R J H. Aluminium-Lithium Alloys. Amsterdam: Elsevier, 2014: 1
[33] Li J F, Zheng Z Q, Chen Y L, Zhang X H. Aerosp Mater Technol, 2012; (1): 13
[33] (李劲风, 郑子樵, 陈永来, 张绪虎. 宇航材料工艺, 2012; (1): 13)
[34] Dursun T, Soutis C. Mater Des, 2014; 56: 862
[35] Liu S D, Zhang X M, You J H, Huang Z B, Zhou Z P. Mater Sci Technol, 2008; 24: 1419
[36] Boselli J, Chakrabarti D J, Shuey R T. Al Alloys, 2008; 1: 202
[37] Fink W L, Willey L A. Trans AIME, 1948; 175: 414
[38] Shuey R T, Barlat F, Karabin M E, Chakrabarti D J. Metall Mater Trans, 2009; 40A: 365
[39] Lequeu P, Smith K P, Daniélou A. J Mater Eng Perform, 2010; 19: 841
[40] Zhang X M, Zhang X Y, Liu S D, Liu Y. J Cent South Univ (Sci Technol), 2007; 38: 789
[40] (张新明, 张小艳, 刘胜胆, 刘 瑛. 中南大学学报(自然科学版), 2007; 38: 789)
[41] Kumaran S M. Mater Sci Eng, 2011; A528: 4152
[42] Dursun T, Soutis C. Mater Des, 2014; 56: 862
[43] Engler O, Sachot E, Ehrstrom J C, Reeves A, Shahani R. Mater Sci Technol, 1996; 12: 717
[44] Starink M J, Wang S C. Acta Mater, 2003; 51: 5131
[45] Zhen L, Chen J Z, Yang S J, Shao W Z, Dai S L. Mater Sci Eng, 2009; A504: 55
[46] Deng Y L, Wan L, Zhang Y, Zhang X M. J Alloys Compd, 2010; 498: 88
[47] Ye L Y, Gu G, Liu J, Jiang H, Zhang X. Mater Sci Eng, 2013; A582: 84
[48] Zhang X M, Wang W T, Chen M A, Gao Z G, Jia Y Z, Ye L Y, Kuang X Y. Trans Nonferrous Met Soc, 2010; 20: 727
[49] Fang H C, Chen K H, Chen X, Chao H, Peng G S. Corros Sci, 2009; 51: 2872
[50] Zhang X M, Liu S D, Liu Y, Zhang X Y. J Cent South Univ (Sci Technol), 2007; 38: 181
[50] (张新明, 刘胜胆, 刘 瑛, 张小艳. 中南大学学报(自然科学版), 2007; 38: 181)
[51] Lin Z Q, Ru H Q, Zhao G, Sun G J. Key Eng Mater, 1991; 20: 2369
[52] Yang S J, Xie Y H, Zhu N, Dai S L, Lu Z, Su B, Yan M G. Chin J Mater Res, 2002; 16: 406
[52] (杨守杰, 谢优华, 朱 娜, 戴圣龙, 陆 政, 苏 彬, 颜鸣皋. 材料研究学报, 2002; 16: 406)
[53] He Y D, Zhang X M, You J H. Trans Nonferrous Met Soc, 2006; 16: 1228
[54] Ohnishi T, Ibaraki Y, Ito T. Mater Trans, 1989; 30: 601
[55] Avan A. Zeitschrift für Metallkunde, 1989; 80: 170
[56] Li J F, Birbilis N, Li C X, Jia Z Q, Cai B, Zheng Z Q. Mater Charact, 2009; 60: 1334
[57] Xiao Y P, Pan Q L, Li W B, Liu X Y, He Y B. Mater Des, 2011; 32: 2149
[58] Xu D K, Birbilis N, Rometsch P A. Corros Sci, 2012; 54: 17
[59] Zhang X M, Huang Z B, Liu S D, Liu W H, Zhang C, Du Y X. Chin J Nonferrous Met, 2006; 37: 1
[59] (张新明, 黄振宝, 刘胜胆, 刘文辉, 张 翀, 杜予暄. 中国有色金属学报, 2006; 37: 1)
[60] Deng Y L, Zhang Y Y, Wan L, Zhang X M. Mater Sci Eng, 2012; A554: 33
[61] Liu G, Zhang G J, Ding X D, Sun J, Chen?K H. Mater Sci Eng, 2003; A344: 113
[62] Steglich D, Brocks W, Heerens J,?Pardoen T. Eng Frac Mech, 2008; 75: 3692
[63] Liu G, Sun J, Nan C W, Chen?K H. Acta Mater, 2005; 53: 3459
[64] Zuo Y, Nagaumi H, Cui J. J Mater Process Technol, 2008; 197: 109
[65] Li S, Sun F, Li H. Acta Mater, 2010; 58: 1317
[66] Feng D, Zhang X M, Liu S D, Wu Z Z, Wang T. Chin J Nonferrous Met, 2014; 24: 2122
[66] (冯 迪, 张新明, 刘胜胆, 吴泽政, 王 婷. 中国有色金属学报, 2014; 24: 2122)
[67] Li S Y, Surya R K, Irene J B. Mater Sci Eng, 2005; A410: 207
[68] Zhang X M, Deng Y L, Zhang Y. Chin Pat, ZL200910043001.3, 2011
[68] (张新明, 邓运来, 张 勇. 中国专利, ZL200910043001.3, 2011)
[69] Zhang J, Deng Y L, Yang W, Hu S, Zhang X M. Mater Des, 2014; 56: 334
[70] Deng Y L, Wan L, Zhang Y Y, Zhang X M. J Alloys Compd, 2011; 509: 4636
[71] Toor P M. Eng Fract Mech, 1973; 5: 837
[72] Bucci R J, Warren C J, Starke E A. J Aircraft, 2000; 37: 122
[73] Dursun T, Soutis C. Mater Des, 2014; 56: 862
[74] Suzuki H, Kanno M, Saitoh H. J Jpn Inst Light Met, 1984; 34: 630
[75] Suzuki H, Kanno M, Saitoh H. J Jpn Inst Light Met, 1986; 36: 22
[76] Liu S D, Liu W J, Zhang Y, Zhang X M, Deng Y L. J Alloys Compd, 2010; 507: 53
[77] Zhang Y, Bettles C, Rometsch P A. J Mater Sci, 2014; 49: 1709
[78] He Y D, Zhang X M. Chin J Nonferrous Met, 2005; 15: 1917
[78] (贺永东, 张新明. 中国有色金属学报, 2005; 15: 1917)
[79] Lim S T, Yun S J, Nam S W. Mater Sci Eng, 2004; A371: 82
[80] Marlaud T, Deschamps A, Bley F, Lefebvre W, Baroux B. Acta Mater, 2010; 58: 248
[81] Feng D, Zhang X M, Liu S D, Wang T, Wu Z Z, Guo Y W. Mater Sci Eng, 2013; A588: 34
[82] Li S Y, Zhang J, Yang J L, Deng Y L, Zhang X M. Acta Metall Sin (Engl Lett), 2014; 27: 107
[83] Bakavos D, Prangnell P B, Bes B, Eberl F. Mater Sci Eng, 2008; A491: 214
[84] Chul O M, Byungmin A. Trans Nonferrous Met Soc, 2014; 24: 53
[85] Tang H G, Cheng Z Q, Liu J W, Ma X. Mater Sci Eng, 2012; A550: 51
[86] Eddahbi M, Carre?o F, Ruano O A. Mater Lett, 2006; 60: 3232
[87] Liu J Z, Yang S S, Wang S B, Chen J H, Wu C L. J Alloys Compd, 2014; 613: 139
[88] Bai S, Liu Z, Zhou X, Xia P, Liu M, Zeng S. Mater Sci Eng, 2014; A611: 69
[89] Ebrahimi G R, Zarei-Hanzaki A, Haghshenas M, Arabshahi H. J Mater Process Technol, 2008; 206: 25
[90] Feng Z Q, Yang Y Q, Huang B, Luo X, Li M H, Han M, Fu M S. Acta Mater, 2011; 59: 2412
[91] Marceau R K W, Sha G, Lumley R N, Ringer S P. Acta Mater, 2010; 58: 1795
[92] Wang S C, Starink M J, Gao N. Scr Mater, 2006; 54: 287
[93] Liu Y. Master Thesis, Central South University, Changsha, 2008
[93] (刘 瑛. 中南大学硕士学位论文, 长沙, 2008)
[94] Sun D X, Zhang X M, Ye L Y, Gu G, Jiang H C, Gui X H. Mater Sci Eng, 2014; A620: 241
[95] Gao Z G, Zhang X M, Chen M A. J Alloys Compd, 2009; 476: L1
[96] Gao Z G, Zhang X M, Zhao Y S, Chen M A, Li H J. J Alloys Compd, 2009; 481: 422
[97] Li H Z, Wang H J, Liang X P, Liu H T, Liu Y, Zhang X M. Mater Sci Eng, 2011; A528: 1548
[98] Ye L Y, Gu G, Zhang X M, Sun D, Jiang H, Zhang P. Mater Sci Eng, 2014; A590: 97
[99] Gu G. Master Thesis, Central South University, Changsha, 2014
[99] (顾 刚. 中南大学硕士学位论文, 长沙, 2014)
[100] Gu G, Ye L Y, Jiang H C, Sun D X, Zhang P, Zhang X M. Trans Nonferrous Met Soc, 2014; 24: 2295
[101] Liu W H, He Z T, Chen Y Q, Tang S W. Trans Nonferrous Met Soc, 2014; 24: 2179
[102] Wang W T, Zhang X M, Gao Z G, Jia Y Z, Ye L Y, Zheng D W, Liu L. J Alloys Compd, 2010; 491: 366
[103] Fu Y, Xie S S, Xiong B Q, Huang G J, Cheng L. J Plast Eng, 2010; 17(6): 103
[103] (付 垚, 谢水生, 熊柏青, 黄国杰, 程 磊. 塑性工程学报, 2010; 17(6): 103)
[104] Zhang T, Wu Y X, Gong H, Zheng X Z, Jiang S S. Trans Nonferrous Met Soc, 2014; 24: 2150
[105] Deng Y L, Zhang Y Y, Wan L, Zhu A F, Zhang X M. Metall Mater Trans, 2013; 44A: 2470
[106] Liu S D, You J H, Zhang X M, Deng Y, Yuan Y. Mater Sci Eng, 2010; A527: 1200
[107] Liu S D, Yuan Y B, Li C B, You J H, Zhang X M. Met Mater Int, 2012; 18: 679
[108] Yuan W J, Wu Y X. J Cent South Univ (Sci Technol),?2011; 42: 2303
[108] (袁望姣, 吴运新. 中南大学学报(自然科学版), 2011; 42: 2303
[109] Tang J G, Chen H, Zhang X M, Liu S D, Liu W J, Ouyang H, Li H P. Trans Nonferrous Met Soc, 2012; 22: 1255
[110] Rossini N S, Dassisti M, Benyounis K Y, Olabi A G. Mater Des, 2012; 35: 572
[111] Robinson J S, Tanner D A, Truman C E, Paradowska A M, Wimpory R C. Mater Charact, 2012; 65: 73
[112] Li P Y, Xiong B Q, Zhang Y A, Li Z H, Zhu B H, Wang F, Liu H W. Trans Nonferrous Met Soc, 2012; 22: 268
[113] Li P Y, Xiong B Q, Zhang Y A, Li Z H, Zhu B H, Wang F, Liu H W. Chin J Nonferrous Met, 2011; 21: 961
[113] (李培跃, 熊柏青, 张永安, 李志辉, 朱宝宏, 王 锋, 刘红伟. 中国有色金属学报, 2011; 21: 961)
[114] Shang B C, Yin Z M, Wang G, Liu B, Huang Z Q. Mater Des, 2011; 32: 3818
[115] Deng Y L, Guo S G, Xiong C X, Zhang X M. J Aero Mater, 2010; 30(6): 21
[115] (邓运来, 郭世贵, 熊创贤, 张新明. 航空材料学报, 2010; 30(6): 21)
[116] Qi L, Li M, Ma M, Jing Q, Li G, Liu R. Sci Chin-Phys Mech Astro, 2010; 53: 2037
[117] Mascarenhas N, Mudawar I. Int J Heat Mass Trans, 2010; 53: 5871
[118] Liu S D, Zhong Q M, Zhang Y, Liu W J, Zhang X M, Deng Y L. Mater Des, 2010; 31: 3116
[119] Sun H C, Chao L S. Mater Trans, 2009; 50: 1396
[120] Sugianto A, Narazaki M, Kogawara M, Shirayori A. J Mater Process Technol, 2009; 209: 4627
[121] Hewakandamby B N. Int J Heat Mass Trans, 2009; 52: 396
[122] Zhang Y, Deng Y L, Zhang X M. Chin J Nonferrous Met, 2008; 18: 1788
[122] (张 勇, 邓运来, 张新明. 中国有色金属报, 2008; 18: 1788)
[123] Silk E A, Golliher E L, Paneer S R. Energy Convers Manage, 2008; 49: 453
[124] Anna A P, Kiyoshi O, Michael A. Int J Heat Fluid Flow, 2008; 29: 131
[125] Jiang K D, Long C, Zhang Y Y, Deng Y L. Trans Nonferrous Met Soc, 2014; 24: 2117
[126] Cina B, Gan R. US Pat, 3856584, 1974
[127] Zhang X M, You J H, Zhang X Y, Liu S D. Chin J Nonferrous Met, 2007; 17: 1922
[127] (张新明, 游江海, 张小艳, 刘胜胆. 中国有色金属学报, 2007; 17: 1922)
[128] Ho K C, Lin J, Dean T A. Int J Plast, 2004; 20: 733
[129] Zhang J, Deng Y L, Zhang X M. Mater Sci Eng, 2013; A563: 8
[130] Zhang X M, Ye L Y, Liu Y W, Tang J G, Zheng D W. Mater Sci Technol, 2011; 27: 1588
[131] Ye L Y, Zhang X M, Zhen D W, Liu S D, Tang J G. J Alloys Compd, 2009; 487: 109
[132] Kaibyshev R, Osipova O. Mater Sci Technol, 2005; 21: 1209
[133] Threadgill P L, Leonard A J, Shercliff H R, Withers P J. Int Mater Rev, 2009; 54: 49
[134] Mishra R S, Ma Z Y. Mater Sci Eng, 2005; A50: 1
[135] Schubert E, Klassen M, Zerner I, Walz C, Sepold G. J Mater Process Technol, 2001; 115: 2
[136] Ion J C. Sci Technol Weld Joining, 2000; 5: 265
[137] Watchamk K. Mater World, 2004; 12(2): 10
[138] Zhu A W, Starke Jr E A. Mater Process Technol, 2001; 117: 354
[139] Zhu A W, Starke Jr E A. Acta Mater, 2001; 49: 2285
[140] Wang Z T,Tian R Z. Aluminum Alloy and Processing Manual. Changsha: Central South University Press, 2005: 1
[140] (王祝堂,田荣璋. 铝合金及其加工手册. 长沙: 中南大学出版社, 2005: 1)
[141] Zhang Y,Milkereit B,Weyland M,Rometsch A. Sci Rep, in press
Outlines

/

〈 〉