TENSILE AND HIGH CYCLE FATIGUE PROPERTIES OF Ti-47Al-2Cr-2Nb DIRECTIONALLY SOLIDIFIED BY COLD CRUCIBLE METHOD

  • Hongsheng DING ,
  • Zibo SHANG ,
  • Yongzhe WANG ,
  • Ruirun CHEN ,
  • Jingjie GUO ,
  • Hengzhi FU
Expand
  • National Key Laboratory for Precision Hot Processing of Metals, School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001

Received date: 2014-08-09

  Online published: 2015-03-09

Supported by

National Natural Science Foundation of China (Nos.51171053 and 51471062) and National Basic Research Program of China (No.2011CB605504)

Abstract

TiAl-based alloys have recently received considerable attention as one of the promising candidates for application in aero engine blades by replacing the Ni-based superalloys because of their unique properties, such as high specific strength, high specific stiffness and good oxidation resistance. However, there are some shortcomings limiting the application of TiAl-based alloys, namely, their brittleness and poor processing properties. Nevertheless, aero engine blades usually suffer a variety of cyclic loadings during the period of services, which finally results in fatigue failure. According to statistics, fatigue failure, mainly high cycle fatigue (HCF), occupies almost 80% failure modes of gas turbine blades in aero engines. Consequently, more and more researches about fatigue behavior of blade materials have been done in the last tens of years. However, there are less relevant results about TiAl-based alloys, especially HCF properties. Recently, the advancement of directional solidification (DS) of TiAl-based alloys using cold crucible has revealed that the ductility can be enhanced at room and elevated temperature. For purpose to verify the influence of DS structures on the tensile and HCF properties, TiAl-based alloy in composition with Ti-47Al-2Cr-2Nb (atomic fraction, %) was prepared and evaluated in this work. Directionally solidified Ti-47Al-2Cr-2Nb alloy ingots with different withdrawal rates (1.0, 1.2 and 1.4 mm/min) were prepared by cold crucible method under alter electromagnetic field in a vacuum furnace. Based on these ingots, macro and microstructures have been characterized by methods of digital camera, OM, SEM and XRD. Furthermore, the tensile properties at room and high temperature (800 ℃) as well as HCF properties at room temperature have been measured respectively. So, the relationship between microstructures and mechanical properties of TiAl-based alloy, especially HCF properties, was demonstrated reasonably and mechanism in which HCF cracks propagated was discussed. The results show that the comprehensive mechanical properties of Ti-47Al-2Cr-2Nb alloy can be significantly improved after directionally solidified using cold crucible. The tensile strength reaches 652 MPa at room temperature with the maximum elongation of 1.5%. Meanwhile, the tensile strength at 800 ℃ attains 490 MPa with the elongation of 5.0%. Based on the data of HCF test at room temperature with the stress ratio of 0.1, the equations of stress amplitude-number of cycles to failure (S-N) curve at different withdrawal rates are calculated. The fatigue limits are 300 and 247 MPa with the withdrawal rates of 1.0 and 1.2 mm/min, respectively, namely, with the increase of withdrawal rate, the fatigue fracture resistance decreases. The mode of HCF fracture of directionally solidified Ti-47Al-2Cr-2Nb alloy behaves in brittle cleavage fracture. And micro-cracks which can propagate along and perpendicular to the lamellae at the same time are observed between α2/g lamellae and around B2 phases.

Cite this article

Hongsheng DING , Zibo SHANG , Yongzhe WANG , Ruirun CHEN , Jingjie GUO , Hengzhi FU . TENSILE AND HIGH CYCLE FATIGUE PROPERTIES OF Ti-47Al-2Cr-2Nb DIRECTIONALLY SOLIDIFIED BY COLD CRUCIBLE METHOD[J]. Acta Metall Sin, 2015 , 51(5) : 569 -579 . DOI: 10.11900/0412.1961.2014.00447

References

[1] Lin J P, Zhang L Q, Song X P, Ye F, Chen G L. Mater China, 2010; 29(2): 1 (林均品, 张来启, 宋西平, 叶 丰, 陈国良. 中国材料进展, 2010; 29(2): 1)
[2] Suresh S. Fatigue of Materials. Cambridge: Cambridge University Press, 1998; 2: 345
[3] He Y H, Su B. Aeroengine, 2005; 31(2): 51 (何玉怀, 苏 彬. 航空发动机, 2005; 31(2): 51)
[4] Li Q H, Wang Y R, Wang J J. Aeroengine, 2003; 29(4): 16 (李其汉, 王延荣, 王建军. 航空发动机, 2003; 29(4): 16)
[5] Li J S, Zhang T B, Chang H, Kou H C, Zhou L. Mater China, 2010; 29(3): 1 (李金山, 张铁邦, 常 辉, ?寇宏超, 周 廉. 中国材料进展, 2010; 29(3): 1)
[6] Chen G L,Lin J P. Physical Metallurgy for the Structural Ordered Intermetallics. Beijing: Metallurgical Industry Press, 1999: 285 (陈国良,林均品. 有序金属间化合物结构材料物理金属学基础. 北京: 冶金工业出版社, 1999: 285)
[7] Kim Y W. Trans Nonferrous Met Soc China, 1999; 9: 298
[8] Yamaguchi M, Inui H. Acta Mater, 2000; 48: 307
[9] Kim S W, Wang P, Oh M H, Wee D M, Kumarb K S. Intermetallics, 2004; 12: 499
[10] Chan K S, Kim Y W. Acta Metall, 1995; 43: 439
[11] Qian J H, Qi X Z. Chin J Rare Met, 2002; 26: 477 (钱九红, 祁学忠. 稀有金属, 2002; 26: 477 )
[12] Fu H Z, Ding H S, Chen R R, Bi W S. Rare Met Mater Eng, 2008; 37: 565 (傅恒志, 丁宏升, 陈瑞润, 毕维生. 稀有金属材料与工程, 2008; 37: 565)
[13] Wang Y L, Ding H S, Bi W S, Guo J J, Fu H Z. Rare Met Mater Eng, 2006; 35: 1597 (王艳丽, 丁宏升, 毕维生, 郭景杰, 傅恒志. 稀有金属材料与工程, 2006; 35: 1597)
[14] Fu H Z, Shen J, Hao Q T, Li S M, Li J S. Chin J?Nonferrous Met, 2002; 12: 1081? (傅恒志, 沈 军, 郝启堂, 李双明, 李金山. 中国有色金属学报, 2002; 12: 1081)
[15] Pericleous K, Bojarevics V, Djambazov G. Appl Math Model, 2006; 30: 1262
[16] Sastry S M L, Lipsitt H A. Metall Trans, 1977; 8A: 299
[17] Henaff G, Gloanec A L. Intermetallics, 2005; 13: 543
[18] Zhang W J, Deevi S C, Chen G L. Intermetallics, 2002; 10: 403
[19] Jones P E, Eylon D. Mater Sci Eng, 1999; A263: 296
[20] Jha S K, Larsen J M, Rosenberger A H. Acta Mater, 2005; 53: 1293
[21] Zhang Y G,Han Y F,Chen G L,Guo J T,Wan X J,Feng D. Structural Intermetallics. Beijing: National Defense Industry Press, 2001: 705 (张永刚,韩雅芳,陈国良,郭建亭,万小景,冯 涤. 金属间化合物结构材料. 北京: 国防工业出版社, 2001: 705)
[22] Gloanec A L, Milani T, Henaff G. Int J Fatigue, 2010; 32: 1015
[23] Meyers M A, Mishra A, Benson D J. Prog Mater Sci, 2006; 51: 427
[24] Xu R P, Fu H M, Gao Z T. J Mech Strength, 1994; 16(1): 58 (徐人平, 傅惠民, 高镇同. 机械强度, 1994; 16(1): 58)
[25] Mine Y J, Fujisaki H, Matsuda M, Takeyama M, Takashima K. Scr Mater, 2011; 65: 707
[26] Kumpfer J, Kim Y W, Dimiduk D M. Mater Sci Eng, 1995; A192-193: 465
[27] Tsutsumi M, Takano S. Intermetallics, 1996; 4: 77
[28] Cao R, Lin Y Z, Hu D. Eng Fract Mech, 2008; 75: 4343
[29] Jones P E, Eylon D. Mater Sci Eng, 1999; A263: 296
[30] Laird C. Fracture, 1984; 84: 261
Outlines

/