MICROSTRUCTURES AND PROPERTIES OF LEAD-FREE FREE-CUTTING GRAPHITE-BRASS PREPARED BY GRAPHITIZATION OF CEMENTITE

  • Yingyu XUE ,
  • Jiancheng TANG ,
  • Haiou ZHUO ,
  • Nan YE ,
  • Tong WU ,
  • Xusheng ZHOU
Expand
  • School of Materials Science and Engineering, Nanchang University, Nanchang 330031

Received date: 2014-07-10

  Revised date: 2014-10-18

  Online published: 2015-07-23

Supported by

Supported by National Natural Science Foundation of China (Nos.51471083, 51271090 and 51364036)

Abstract

Graphite is believed to be an attractive candidate substituting for lead to produce free-cutting brasses, because of its lubricating property and the role in chip breaking. The major hindrances of developing graphite-brass are the large density difference and nonwetting characteristic between graphite and copper. In this work, eutectic cast iron (ECI) was added into brasses instead of other form of carbon source. Cementite particles were in situ formed during casting, then annealing treatment was conducted to facilitate the graphitization of cementite particles, and finally uniformly dispersed graphite particles with the size of 3~6 mm were obtained in brass alloys. SEM and EDS observation indicate that the microstructures of the graphite-brass are refined with the cast iron content increased from 1% to 7%. The tensile strength and microhardness are increased, and the chip morphologies are improved gradually with the cast iron content increased from 1% to 7%. However, the graphite brass with 7% addition shows suboptimal chip morphologies because of the segregation of graphite particles. The chips of graphite brasses with 5% addition are desired, which are short and discontinuous. Its tensile strength, elongation and Vickers hardness are 502.00 MPa, 22.6% and 148.9 HV, respectively. The graphite brass shows comparable machinability to conventional lead brass HPb59-1。

Cite this article

Yingyu XUE , Jiancheng TANG , Haiou ZHUO , Nan YE , Tong WU , Xusheng ZHOU . MICROSTRUCTURES AND PROPERTIES OF LEAD-FREE FREE-CUTTING GRAPHITE-BRASS PREPARED BY GRAPHITIZATION OF CEMENTITE[J]. Acta Metall Sin, 2015 , 51(2) : 223 -229 . DOI: 10.11900/0412.1961.2014.00380

References

[1] Kuyucak S, Sahoo M. Can Metall Quart, 1996; 35: 1
[2] Huang J S, Peng C Q, Zhang S Q, Huang B Y. Chin J Nonferrous Met, 2006; 16: 1486
[2] (黄劲松, 彭超群, 章四琪, 黄伯云. 中国有色金属学报, 2006; 16: 1486)
[3] EI-Sherif R M, Ismail K M, Badawy W A. Electrochim Acta, 2004; 49: 5139
[4] Nakano A, Higashiiriki K, Rochman N T. J Jpn Inst Met, 2005; 69: 198
[5] Fontaine A L, Keast V J. Mater Charact, 2006; 57: 424
[6] Vilarinho C, Davim J P, Soares D, Castro F. J Mater Process Technol, 2005; 170: 441
[7] Jang Y, Kim S, Han S. Metall Mater Trans, 2005; 36: 1060
[8] Xiao L R, Shu X P, Yi D Q, Zhang L H, Qin J L, Hu J R. J Cent South Univ (Sci Technol), 2009; 40: 117
[8] (肖来荣, 舒学鹏, 易丹青, 张路怀, 覃静丽, 胡加瑞. 中南大学学报(自然科学版), 2009; 40: 117)
[9] Peters D T. Mod Cast, 1997; 87: 57
[10] Zhang M, Zhang S Q, Cai J H, Lou H R, Xie X. US Pat, 0289094, 2006
[11] Taha M A, E-Mahallawy N A, Mousa T M, Hamouda R M, Yousef A F A G. Mater Wiss Werkst, 2012; 40: 699
[12] Xu C K, Hu Z Q, Zhang S Q. US Pat, 8273193, 2010
[13] Oishi K. US Pat, 6413330, 2002
[14] Dienwiebel M, Verhoeven G S, Pradeep N, Frenken J W, Heimberg J A, Zandbergen H W. Phys Rev Lett, 2004; 92: 126101
[15] Nath D, Gupta A K, Rohatgi P K. J Mater Sci Lett, 1997; 16: 1595
[16] Kim J K, Rohatgi P K, Choi J O. Met Mater Int, 2005; 11: 333
[17] Imai H, Kosaka Y, Kojima A, Li S F, Kondoh K, Umeda J, Atumi H. Powder Technol, 2010; 198: 417
[18] Rohatgi P K, Nath D, Kim J K. Corros Sci, 2000; 42: 1553
[19] Rohatgi P K, Ray S, Church N. AFS Trans, 1992; 100: 1
[20] Rohatgi P K, Nath D, Ray S. AFS Trans, 1993; 104: 49
[21] Huang J S, Zhou Z C. Chin Pat, 10030662, 2008
[21] (黄劲松, 周忠诚. 中国专利, 10030662, 2008)
[22] Huang J S, Zhou Z C. Chin Pat, 10030409, 2008
[22] (黄劲松, 周忠诚. 中国专利, 10030409, 2008)
[23] Song J M, Lui T S, Chen L H, Kuo B C. Metall Mater Trans, 2000; 31A: 275
[24] Johnson W, Mehl R. Trans AIME, 1939; 135: 461
[25] Avrami M. J Chem Phys, 1940; 8: 212
[26] Dai F P, Cao C D, Wei B B. Sci China, 2007; 50G: 509
[27] Trent E M, Wright P K. Metal Cutting. 4th Ed, Woburn: Butterworth-Heinemann, 2000: 23
[28] Garcia P, Rivera S, Palacios M, Belzunce J. Eng Fail Anal, 2010; 17: 771
Outlines

/

〈 〉