INFLUENCE OF PARTICLES WITH DIFFERENT SIZES ON MICROSTRUCTURE, TEXTURE AND MECHAN-ICAL PROPERTIES OF Al-Mg-Si-Cu SERIES ALLOYS

  • Xiangyang PENG ,
  • Mingxing GUO ,
  • Xiaofeng WANG ,
  • Li CUI ,
  • Jishan ZHANG ,
  • Linzhong ZHUANG
Expand
  • State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083

Received date: 2014-05-23

  Revised date: 2014-08-26

  Online published: 2015-07-23

Supported by

Supported by National High Technology Research and Development Program of China (No. 2013AA032403), National Natural Science Foundation of China (No.51301016) and Beijing Higher Education Yong Elite Teacher Project (No.YETP0409)

Abstract

To reduce the weight of car body, Al-Mg-Si-Cu alloys have been used to produce outer body panels of automobiles due to their relatively good formability in the solution treated condition and high strength in the age hardened condition. However, their formability is significantly poor compared to that of steels, which are the major drawbacks to wide-scale application of aluminum in the automotive industry. The microstructural characteristics developed during recrystallization, most notably grain size and crystallographic texture, play a dominant role in controlling the mechanical properties and formability of sheet in the T4 condition. In this work, the effect of particles with different sizes on the mechanical properties, microstructure and texture of Al-Mg-Si-Cu alloys was studied through tensile test, OM, SEM, TEM and EBSD measurement. The results reveal that with increase of solute concentration, the average plastic strain ratio, yield strength and ultimate tensile strength increase, but the elongation decreases and with different extents in the three directions. In addition, the number of observed particles with different sizes in the alloy matrix such as Mg2Si, Al15Mn3Si2 and α-Al(Fe, Mn)Si phases also increases. When the size and concentration of these particles are controlled appropriately, lots of finer recrystallized grains can form during solution treatment due to the particle stimulated nucleation (PSN) effect of coarse particles and pinning effect of finer particles. The main texture components include CubeND18, Goss{011}<100>, P{011}<122> and Cu{112}<111> for the alloy with fine-grained structure. At last, according to the relationship among alloy composition, thermomechanical processing and microstructure, the model of nucleation and growth of recrystallized grains affected by the particles with different sizes was also proposed。

Cite this article

Xiangyang PENG , Mingxing GUO , Xiaofeng WANG , Li CUI , Jishan ZHANG , Linzhong ZHUANG . INFLUENCE OF PARTICLES WITH DIFFERENT SIZES ON MICROSTRUCTURE, TEXTURE AND MECHAN-ICAL PROPERTIES OF Al-Mg-Si-Cu SERIES ALLOYS[J]. Acta Metall Sin, 2015 , 51(2) : 169 -177 . DOI: 10.11900/0412.1961.2014.00276

References

[1] Miller W S, Zhuang L, Bottema J, Wettebrood A J, De S P, Haszler A, Vieregge A. Mater Sci Eng, 2000; A280: 37
[2] Burger G B, Gupta A K, Jeffrey P W, Lloyd D J. Mater Charact, 1995; 35(1): 23
[3] Engler O, Hirsch J. Mater Sci Forum, 1996; 217: 479
[4] Hirsch J, Al-Samman T. Acta Mater, 2013; 61: 818
[5] Ma M T. Iron Steel, 2001; 36(8): 64
[5] (马鸣图. 钢铁, 2001; 36(8): 64)
[6] Esmaeili S, Lloyd D J. Acta Mater, 2005; 53: 5257
[7] Miki Y, Koyama K, Noguchi O, Ueno Y, Komatsubara T. Mater Sci Forum, 2007; 539: 333
[8] Engler O, Hirsch J. Mater Sci Eng, 2002; A336: 249
[9] Singh R K, Singh A K. Scr Mater, 1998; 38: 1299
[10] Engler O, Kong X W, Yang P. Scr Mater, 1997; 37: 1665
[11] Bennett T A, Petrov R H, Kestens L A I, Zhuang L, De S P. Scr Mater, 2010; 63: 461
[12] Liu Q, Yao Z Y, Godfrey A, Liu W. J Alloys Compd, 2009; 482: 264
[13] Vatne H E, Engler O, Nes E. Mater Sci Technol, 1997; 13: 93
[14] Engler O. Mater Sci Technol, 1996; 12: 859
[15] Engler O, Hirsch J, Lücke K. Acta Mater, 1995; 43: 121
[16] Higginson R L, Aindow M, Bate P S. Mater Sci Eng, 1997; A225: 9
[17] Zhuang L, Bottema J, Kaasenbrood P, Miller W S, De S P. Mater Sci Forum, 1996; 217: 487
[18] Jeniski R A, Thanaboonsombut B, Sanders T H. Metall Mater Trans, 1996; 27A: 19
[19] Cao L Y, Guo M X, Cui H, Cai Y H, Zhang Q X, Hu X Q, Zhang J S. Acta Metall Sin, 2013; 49: 428
[19] (曹零勇, 郭明星, 崔 华, 蔡元华, 张巧霞, 胡晓倩, 张济山. 金属学报, 2013; 49: 428)
[20] Sidor J, Petrov R H, Kestens L A I. Mater Sci Eng, 2010; A528: 413
[21] Inoue H, Takasugi T. Mater Trans, 2007; 48: 2014
[22] Hirsch J, Lücke K. Acta Metall, 1988; 36: 2863
[23] Rollett A, Humphreys F J, Rohrer G S, Hatherly M. Recrystallization and Related Annealing Phenomena. 2nd Ed., Amsterdam: Elsevier Ltd, 2004: 408
[24] Bennett T A, Petrov R H, Kestens L A I. Scr Mater, 2010; 62: 78
[25] Benum S, Nes E. Acta Mater, 1997; 45: 4593
Outlines

/

〈 〉