STUDY OF SOLIDIFICATION FOR GAS-ATOMIZED DROPLET OF Cu-Co-Fe ALLOY

  • Lei ZHAO ,
  • Hongxiang JIANG ,
  • Tauseef AHMAD ,
  • Jiuzhou ZHAO
Expand
  • 1 School of Mechanical Engineering, Liaoning Shihua University, Fushun 113001
    2 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Accepted date: 2015-01-16

  Online published: 2015-02-04

Supported by

Supported by National Natural Science Foundation of China (Nos.51271185, 51031003 and 51471173)

Cite this article

Lei ZHAO , Hongxiang JIANG , Tauseef AHMAD , Jiuzhou ZHAO . STUDY OF SOLIDIFICATION FOR GAS-ATOMIZED DROPLET OF Cu-Co-Fe ALLOY[J]. Acta Metall Sin, 2015 , 51(7) : 883 -888 . DOI: 10.11900/0412.1961.2014.00469

References

[1] Song J S, Hong S I. J Alloys Compd, 2000; 311: 265
[2] Berkowitz A E, Mitchell J R, Carey M J, Young A P, Zhang S, Spada F E, Parker F T, Hutten A, Thomas G. Phys Rev Lett, 1992; 68: 3745
[3] Dai F P, Cao C D, Wei B B. Chin Sci Bull, 2009; 54: 402 (代富平, 曹崇德, 魏炳波. 科学通报, 2009; 54: 402)
[4] He J, Zhao J Z. Acta Metall Sin, 2005; 41: 407 (何 杰, 赵九洲. 金属学报, 2005; 41: 407)
[5] Kim D I, Abbaschian R. J Phase Equilib, 2000; 21: 25
[6] Cao C D, G?rler G P. Chin Phys Lett, 2005; 22: 482
[7] Curiotto S, Battezzati L, Johnson E, Palumbo M, Pryds N. J Mater Sci, 2008; 43: 3253
[8] Munitz A, Bamberger A M, Wannaparhun S, Abbaschian R. J Mater Sci, 2006; 41: 2749
[9] Turchanin M A, Dreval L A, Abdulov A R, Agraval P G. Powder Metall Met Ceram, 2011; 50: 98
[10] Bamberger M, Munitz A, Kaufman L, Abbaschian R. Calphad, 2002; 26: 375
[11] Wang C P, Liu X J, Ohnuma I, Kainuma R, Ishida K. J Phase Equilib, 2002; 23: 236
[12] Palumbo M, Curiotto S, Battezzati L. Calphad, 2006; 30: 171
[13] Munitz A, Abbaschian R. J Mater Sci, 1998; 33: 3639
[14] Dai F P, Cao C D, Wei B B. Sci Chin, 2007; 37G: 376 (代富平, 曹崇德, 魏炳波. 中国科学, 2007; 37G: 376)
[15] Zhou F M, Sun D K, Zhu M F. Acta Phys Sin, 2010; 59: 3394 (周丰茂, 孙东科, 朱鸣芳. 物理学报, 2010; 59: 3394)
[16] Cui H B, Guo J J, Su Y Q, Wu S P, Li X Z, Fu H Z. Acta Metall Sin, 2007; 43: 907 (崔红保, 郭景杰, 苏彦庆, 吴士平, 李新中, 傅恒志. 金属学报, 2007; 43: 907)
[17] Ranz W E, Marshall W R. Chem Eng Prog, 1952; 48: 141
[18] Grant P S, Cantor B, Katgerman L. Acta Metall Mater, 1993; 41: 3097
[19] Zhao L, Zhao J Z. J Mater Res, 2013; 28: 1203
[20] Granasy L, Ratke L. Scr Metall Mater, 1993; 28: 1329
[21] Zhao J Z. Mater Sci Eng, 2007; A454-455: 637
[22] Dinsdale A T. Calphad, 1991; 15: 317
[23] Turchanin M A, Agraval P G. Powder Metall Met Ceram, 2007; 46: 77
[24] Turchanin M A, Agraval P G, Nikolaenko I V. J Phase Equilib, 2003; 24: 307
[25] Ohnuma I, Enoki H, Ikeda O, Kainuma R, Ohtani H, Sundman B, Ishida K. Acta Mater, 2002; 50: 379
[26] Moldover M R. Phys Rev, 1985; 31A: 1022
[27] Brandes E A, Brook G B. Smithells Metals Reference Book. 7th Ed., Oxford: Butterworth-Heinemann Ltd, 1992: 14
[28] Roy A K. Chhabra R P. Metall Trans, 1988; 19A: 273
[29] Moir S A, Jones H. Mater Sci Eng, 1993; A173: 161
Outlines

/

〈 〉