ULTRASONIC EVALUATION METHOD FOR GRAIN SIZE BASED ON MULTI-SCALE ATTENUATION

  • Xiongbing LI ,
  • Yongfeng SONG ,
  • Peijun NI ,
  • Feng LIU
Expand
  • 1 CAD/CAM Institute, Central South University, Changsha 410075
    2 State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083
    3 The Ningbo Branch of Ordnance Science Institute of China, Ningbo 315103

Revised date: 2014-07-07

  Online published: 2015-01-25

Supported by

Supported by National Natural Science Foundation of China (Nos.61271356, 51205031 and 51105045), High Technology Research and Development Program of China (No.2012AA03A514), Natural Science Foundation of Hunan Province (No.14JJ2002) and China Postdoctoral Science Foundation (No.2014M562126)

Abstract

To solve such problems as sensitivity to noise and low accuracy of grain size evaluation using traditional ultrasonic time-domain attenuation method, an ultrasonic nondestructive evaluation model based on multi-scale attenuation coefficient was proposed. The distribution of time-scale of ultrasonic energy was obtained by means of wavelet transformation, then to calculate the distribution of attenuation coefficient with scale, and to make a comprehensive analysis of attenuation characteristics of various scales. After the weighted multi-scale ultrasonic attenuation coefficient was defined, a multi-scale ultrasonic attenuation evaluation model was established on the basis of combination of optimal dimension and normalized weight distribution strategy designed by particle swarm optimization. 304 stainless steel was used in the test. The distribution of attenuation coefficient with scale shows that ultrasonic wave of small scales attenuates fast, presenting the frequency characteristics of ultrasonic attenuation among high scattering materials. Following increase of the sample grain size, ultrasonic attenuation of all scales was intensified significantly. Test results show that the sound velocity method, the traditional evaluation method and the proposed method have maximum systematic errors of +12.57%, +5.85% and -1.33%, respectively. With these 3 methods, evaluation results of the sample with a mean grain size of 103.5 mm measured by metallographic method are (110.4±7.8), (98.2±6.6) and (101.7±3.9) mm, respectively, showing that the presented method can not only reduce the systemic error, but also can effectively control the random error by constant Q filtering properties of wavelet transformation. This model can be extended to grain size evaluation of other metals.

Cite this article

Xiongbing LI , Yongfeng SONG , Peijun NI , Feng LIU . ULTRASONIC EVALUATION METHOD FOR GRAIN SIZE BASED ON MULTI-SCALE ATTENUATION[J]. Acta Metall Sin, 2015 , 51(1) : 121 -128 . DOI: 10.11900/0412.1961.2014.00369

References

[1] Prasad K S, Rao C S, Rao D N. Acta Metall Sin (Engl Lett), 2012; 25: 179
[2] Wang S H, Liu Z Y, Wang G D. Acta Metall Sin, 2009; 45: 61
[2] (王书晗, 刘振宇, 王国栋. 金属学报, 2009; 45: 61)
[3] Zhao Y, Chen Z, Long J, Yang T. Acta Metall Sin (Engl Lett), 2014; 27: 81
[4] Lehto P, Remes H, Saukkonen T, H?nninen H, Romanoff J. Mater Sci Eng, 2014; A592: 28
[5] Andrés R, Galvis E, Hormaza W. Eng Fail Anal, 2011; 18: 1791
[6] Voort G F V. Prakt Metall, 2013; 50: 239
[7] Schwartz A J, Kumar M, Adams B L, Field D P. Electron Backscatter Diffraction in Materials Science. New York: Springer, 2009: 1
[8] Sabbagh E H, Sabbagh H A, Murphy R K, Sheila-Vadde A, Blodgett M P, Knopp J, Aldrin J C. In: Thompson D O, Chimenti D E eds., Review of Progress in Quantitative Nondestructive Evaluation, New York: American Institute of Physics, 2009: 742
[9] Guo Y, Thompson R B, Margetan F J. In: Thompson D O, Chimenti D E, eds., Review of Progress in Quantitative Nondestructive Evaluation, New York: American Institute of Physics, 2003: 1347
[10] Panetta P D, Bland L G, Tracy M, Hassan W. In: The Minerals, Metals & Materials Society (TMS) ed., TMS2014 Annual Meeting Supplemental Proceedings, Hoboken: John Wiley & Sons Inc, 2014: 721
[11] ünal R, Sarpün I H, Yal?m H A, Erol A, ?zdemir T, Tuncel S. Mater Charact, 2006; 56: 241
[12] Zuev L B, Semukhin B S, Zarikovskaya N V. Int J Solids Struct, 2003; 40: 941
[13] Laux D, Cros B, Despaux G, Baron D. J Nucl Mater, 2002; 300: 192
[14] Aghaie-Khafri M, Honarvar F, Zanganeh S. J Nondestruct Eval, 2012; 31: 191
[15] ?zkan V, Sarpünb I H. Acta Phys Pol, 2012; 121A: 184
[16] Zeng F, Agnew S R, Raeisinia B, Myneni G R. J Nondestruct Eval, 2010; 29: 93
[17] Kumar A, Jayakumar T, Palanichamy P, Raj B. Scr Mater, 1999; 40: 333
[18] Sharma G K, Kumar A, Babu Rao C, Jayakumar T, Raj B. NDT&E Int, 2013; 53: 1
[19] Dong J K. Heat Treat Met, 2011; 36: 133
[19] (董加坤. 金属热处理, 2011; 36: 133)
[20] Eberhart R C, Shi Y. In: Zalzala A ed., IEEE Proceedings of the Congress Evolutionary Computation, New York: IEEE, 2000: 84
[21] Le T P, Argoul P. J Sound Vib, 2004; 277: 73
Outlines

/

〈 〉