PRECIPITATION BEHAVIOR OF (Nb, Ti)C IN COILING PROCESS AND ITS EFFECT ON MICRO-MECHANICAL CHARACTERISTICS OF FERRITE

  • Yang XU ,
  • Mingxue SUN ,
  • Yanlei ZHOU ,
  • Zhenyu LIU
Expand
  • State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819

Revised date: 2014-05-17

  Online published: 2015-01-25

Supported by

Supported by Fundamental Research Funds for the Central Universities (Nos.N120807001 and N110607006)

Abstract

High strength micro-alloyed steel has been widely used in automobile and machines because of the remarkable high strength and forming property which are attributed to nano-precipitates and refinement of the organization. Since the nano-precipitates are mostly nucleated between austenite/ferrite transition and ferrite can significantly advance strength, it is important to investigate precipitate behavior in coiling process. Nanoindentation technology provides a chance to study the special influence of nano-precipitates on the micro-properties of ferrite. The effect of cooling rate during continuous cooling process and coiling process on microstructural evolution and micro-hardness of Nb-Ti micro-alloyed steel were studied by using the thermal mechanical simulator, micro-hardness instrument, TEM and nanoindentation instrument. The precipitate behaviors of (Nb,Ti)C in coiling process and its effect on nano-hardnesss of ferrite were discussed. Experiments results indicated that the increase of cooling rate in continuous cooling process and coiling process could promote the microstructure transition from ferrite and pearlite to bainite. The micro-hardness of the tested steel increased with the increase of cooling rate in continuous cooling process, and decreased with the cooling rate in coiling process because of the large number of the dispersive nano-precipitate in ferrite which could improve the strength of matrix. The smaller cooling rate could promote volume fraction of (Nb, Ti)C particles in ferrite because there was enough time for the nucleation and growth of (Nb, Ti)C precipitates. When the cooling rate in coiling process was 0.1 ℃/s, precipitates were dispersive in ferrite matrix with a diameter of less than 10 nm. The nanohardness and Young's modulus of ferrite were 4.13 and 249.3 GPa for Nb-Ti micro-alloyed steel, 2.64 and 237.4 GPa for C-Si-Mn steel. The contribution of nano-precipitates to nano-hardness of ferrite reached 1.49 GPa.

Cite this article

Yang XU , Mingxue SUN , Yanlei ZHOU , Zhenyu LIU . PRECIPITATION BEHAVIOR OF (Nb, Ti)C IN COILING PROCESS AND ITS EFFECT ON MICRO-MECHANICAL CHARACTERISTICS OF FERRITE[J]. Acta Metall Sin, 2015 , 51(1) : 31 -39 . DOI: 10.11900/0412.1961.2014.00265

References

[1] Charleux M, Poole W J, Militzer M, Deschamps A. Metall Trans, 2001; 32A: 1635
[2] Funakawa Y, Shiozaki T, Tomita K, Yamamoto T, Maeda E. ISIJ Int, 2004; 44: 1945
[3] Matlock D K, Krauss G, Speer J G. J. Mater Proc Technol, 2001; 117: 324
[4] Wang C J, Yong Q L, Sun X J, Mao X P, Li Z D, Yong X. Acta Metall Sin, 2011; 47: 1541
[4] (王长军, 雍岐龙, 孙新军, 毛新平, 李昭东, 雍 兮. 金属学报, 2011; 47: 1541)
[5] Liu Y C, Zhu F X, Li Y M, Wang G D. ISIJ Int, 2005; 45: 851
[6] Craven A J, He K, Garvie L A J, Baker T N. Acta Mater, 2000; 48: 3857
[7] Han Y, Shi J, Xu L, Cao W Q, Dong H. Mater Sci Eng, 2011; A530: 643
[8] Mao X P, Sun X J, Kang Y L, Lin Z Y, Zhou J. Iron Steel, 2005; 40(9): 65
[8] (毛新平, 孙新军, 康永林, 林振源, 周 建. 钢铁, 2005; 40(9): 65)
[9] Yen H W, Chen P Y, Huang C Y, Yang J R. Acta Mater, 2011; 59: 6264
[10] Yen H W, Chen C Y, Wang T Y, Huang C Y, Yang J R. Mater Sci Technol, 2010; 26: 421
[11] Okamoto R, Borgenstam A, Agren J. Acta Mater, 2010; 58: 4783
[12] Okamoto R, Agen J. Acta Mater, 2010; 58: 4791
[13] Lu J X, Wang G D. Iron Steel, 2005; 40(9): 69
[13] (陆匠心, 王国栋. 钢铁, 2005; 40(9): 69)
[14] Duan X G, Cai Q W, Wu H B. Acta Metall Sin, 2011; 47: 251
[14] (段修刚, 蔡庆伍, 武会宾. 金属学报, 2011; 47: 251)
[15] Yong Q L. Secondary Phases in Steels. Beijing: Metallurgical Industry Press, 2006: 384
[15] (雍岐龙. 钢铁材料中的第二相. 北京: 冶金工业出版社, 2006: 384)
[16] Yi H L, Du L X, Wang G D. ISIJ Int, 2006; 46: 754.
[17] Sun C F, Cai Q W, Wu H B, Mao H Y, Chen H Z. Acta Metall Sin, 2012; 48: 1451
[17] (孙超凡, 蔡庆伍, 武会宾, 毛红艳, 陈宏振. 金属学报, 2012; 48: 1415)
[18] Misra R D K, Nathani H, Hartmanm J E, Siciliano F. Mater Sci Eng, 2005; A394: 339
[19] Hong S G, Kang K B, Park C G. Scr Mater, 2002; 46: 163
[20] Wang X N, Di H S, Du L X. Acta Metall Sin, 2012; 48: 621
[20] (王晓南, 邸洪双, 杜林秀. 金属学报, 2012; 48: 621)
[21] Park D B, Huh M Y, Shim J H, Suh J Y, Lee K H, Jung W S. Mater Sci Eng, 2013; A560: 528
[22] Murakami T, Hatano H, Miymoto G, Furuhara T. ISIJ Int, 2012; 52: 616
[23] Bhadeshia H K D H. Bainite in Steels. London: IOM Communications Ltd, 2001: 19
[24] Bhadeshia H K D H, Christian J W. Metall Trans, 1990; 21A: 767
[25] Kulkarni A V, Bhushan B. Thin Solid Films, 1996; 290-291: 206
Outlines

/

〈 〉