Abstract

In this paper, research progresses on gradient nanostructured materials in recent years is briefly reviewed. It includes classification of gradient nanostructures, properties and processing techniques of the gradient nanostructured materials. Perspectives and challenges on scientific understanding and industrial applications of gradient nanostructured materials are addressed.

Cite this article

Ke LU . GRADIENT NANOSTRUCTURED MATERIALS[J]. Acta Metall Sin, 2015 , 51(1) : 1 -10 . DOI: 10.11900/0412.1961.2014.00395

References

[1] Gleiter H. Prog Mater Sci, 1989; 33: 223
[2] Meyers M A, Mishra A, Benson D J. Prog Mater Sci, 2006; 51: 427
[3] Fang T H, Li W L, Tao N R, Lu K. Science, 2011; 331: 1587
[4] Lu K. In: Faester S, Hansen N, Juul Jensen D, Ralph B, Sun J eds., Proc 35th Riso International Symposium on Materials Science: New Frontiers of Nanometals, Department of Wind Energy, Riso Campus, Technical University of Denmark, 2014: 89
[5] Huang H W, Wang Z B, Lu K. Acta Mater, 2015, in revision
[6] Wang H T, Tao N R, Lu K. Scr Mater, 2013; 68: 22
[7] Liu X C, Zhang H W, Lu K. Science, 2013; 342: 337
[8] Han Z, Zhang Y S, Lu K. J Mater Sci Technol, 2008; 24: 483
[9] Zhang Y S, Han Z, Wang K, Lu K. Wear, 2006; 260: 942
[10] Wang Z B, Tao N R, Li S, Wang W, Liu G, Lu J, Lu K. Mater Sci Eng, 2003; A352: 144
[11] Li G B, Chen J, Guan D L. Tribology Int, 2010; 43: 2216
[12] Ba D M, Ma S N, Meng F J, Li C Q. Surf Coat Technol, 2007; 202: 254
[13] Arun P N, Gnanamoorthy R, Kamaraj M. Mater Sci Eng, 2010;B168: 176
[14] Yan W L, Fang L, Zheng Z G, Sun K, Xu Y H. Tribology Int, 2009; 42: 634
[15] Zhang Y S, Han Z. Tribology Lett, 2007; 27: 53
[16] Sun Y. Tribology Int, 2013; 57: 67
[17] Kumar S A, Raman S G S, Narayanan T S, Gnanamoorthy R. Surf Coat Technol, 2012; 206: 4425
[18] Zhou L, Liu G, Han Z, Lu K. Scr Mater, 2008; 58: 445
[19] Fang T H, Tao N R, Lu K. Scr Mater, 2014; 77: 17
[20] Yong X P. Master Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2001
[20] (雍兴平. 中国科学院金属研究所硕士学位论文, 沈阳, 2001)
[21] Roland T, Retraint D, Lu K, Lu J. Mater Sci Eng, 2007; A445-446: 281
[22] Wu X L, Jiang P, Chen L, Yuan F P, Zhu Y T. Proc Natl Acad Sci United State Am, 2014; 111: 7197
[23] Wei Y J, Li Y Q, Zhu L C, Liu Y, Lei X Q, Wang G, Wu Y X, Mi Z L, Liu J B, Wang H T, Gao H J. Nat Commun, 2014; 5: 3580-1
[24] Lu K. Science, 2014; 345: 1455
[25] Roland T, Retraint D, Lu K, Lu J. Scr Mater, 2006; 54: 1949
[26] Huang H W, Wang Z B, Yong X P, Lu K. Mater Sci Technol, 2013; 29: 1200
[27] Wang Z B, Tao N R, Tong W P, Lu J, Lu K. Acta Mater, 2003; 51: 4319
[28] Wang Z B, Lu K, Wilde G, Divinski S V. Acta Mater, 2010; 58: 2376
[29] Wang H L, Wang Z B, Lu K. Acta Mater, 2012; 60: 1762
[30] Tong W P, Tao N R, Wang Z B, Lu J, Lu K. Science, 2003; 299: 686
[31] Wang Z B, Lu J, Lu K. Acta Mater, 2005; 53: 2081
[32] Lu S D, Wang Z B, Lu K. Mater Sci Eng, 2010; A527: 995
[33] Zhang H W, Wang L, Hei Z K, Liu G, Lu J, Lu K. Z Metall, 2003; 94: 1143
[34] Tong W P, Han Z, Wang L M, Lu J, Lu K. Surf Coat Technol, 2008; 202: 4957
[35] Si X, Lu B N, Wang Z B. J Mater Sci Technol, 2009; 25: 433
[36] Guo S, Wang Z B, Wang L M, Lu K. Surf Coat Technol, 2014; 258: 329
[37] Sun H Q, Shi Y N, Zhang M X, Lu K. Surf Coat Technol, 2008; 202: 3947
[38] Chui P F, Sun K N, Sun C, Yang X Q, Shan T. Appl Surf Sci, 2011; 257: 6787
[39] Raja K S, Namjoshi S A, Misra M. Mater Lett, 2005; 59: 570
[40] Jelliti S, Richard C, Retraint D, Roland T, Chemkhi M, Demangel C. Surf Coat Technol, 2013; 224: 82
[41] Fu T, Zhou Z F, Zhou Y M, Zhu X D, Zeng Q F, Wang C P, Li K Y, Lu J. Surf Coat Technol, 2012; 207: 555
[42] Fu T, Wang C P, Hou B, Zhu X D, Ma S G. China Surf Eng, 2010; 23(5): 64
[42] (付 涛, 王长鹏, 侯 斌, 朱晓东, 马胜哥. 中国表面工程, 2010; 23(5): 64)
[43] Lu K, Lu J. J Mater Sci Technol, 1999; 15: 193
[44] Lu K, Lu J. Mater Sci Eng, 2004; A375-377: 38
[45] Li W L, Tao N R, Lu K. Scr Mater, 2008; 59: 546
[46] Li Y. To be published
Outlines

/

〈 〉