EFFECT OF OXIDATION TIME UNDER HIGH MAG- NETIC FIELD ON THE MICROSTRUCTURE AND OPTICAL PROPERTIES OF OXIDIZED Co-DOPED ZnO FILMS
Revised date: 2014-07-09
Online published: 2014-12-25
Supported by
Supported by National Natural Science Foundation of China (No.51101034), Fundamental Research Funds for the Central Universities (Nos.N130509002, N120609001 and N110809001)
The effects of the oxidation time under high magnetic field on the microstructure and optical properties of oxidized Co-doped Zn prepared by vacuum evaporation were studied by FESEM, XRD and ultraviolet visible spectrophotometer. The results show that the growth of coral dendritic structures of ZnO films is inhibited by high magnetic field. Spherical particles of ZnO film oxidized for 60 min without magnetic field transforms to leaf like morphologies with the application of a 6 T magnetic field. With increasing oxidation time under high magnetic field, the preferred orientation of (101) transforms to (002); distribution of magnetic Co atoms in ZnO is influenced; the band gap is decreased to the range of 2.95~3.13 eV. The transmittance is decreased by the spherical morphologies. However, it is increased by the application of high magnetic field. These results give a new method to tune the microstructure and optical properties of surface morphology, preferred orientation, magnetic atomic distribution, transmittance, and band gap.
Key words: ZnO film; Zn oxide; transmittance; high magnetic field; vacuum evaporation
Guojian LI , Zhen WANG , Qiang WANG , Huimin WANG , Jiaojiao DU , Yonghui MA , Jicheng HE . EFFECT OF OXIDATION TIME UNDER HIGH MAG- NETIC FIELD ON THE MICROSTRUCTURE AND OPTICAL PROPERTIES OF OXIDIZED Co-DOPED ZnO FILMS[J]. Acta Metall Sin, 2014 , 50(12) : 1538 -1542 . DOI: 10.11900/0412.1961.2014.00376
| [1] | ?zgür ü, Alivov Y I, Liu C, Teke A, Reshchikov M A, Do?an S, Avrutin V, Cho S J, Morko? H. J Appl Phys, 2005; 98: 041301 |
| [2] | Look D C, Claflin B, Alivov Y I, Park S J. Phys Status Solidi, 2004; 201A: 2203 |
| [3] | Pan F, Song C, Liu X J, Yang Y C, Zeng F. Mater Sci Eng, 2008; R62: 1 |
| [4] | Hosono H. Thin Solid Films, 2007; 515: 6000 |
| [5] | Becheri A, Dürr M, Lo Nostro P, Baglioni P. J Nanopart Res, 2008; 10: 679 |
| [6] | Huang X H, Zhang C B, Tay C B, Venkatesan T, Chua S J. Appl Phys Lett, 2013; 102: 111106 |
| [7] | Behan A J, Mokhtari A, Blythe H J, Score D, Xu X H, Neal J R, Fox A M, Gehring G A. Phys Rev Lett, 2008; 100: 047206 |
| [8] | Li H L, Zhang Z, Lü Y B, Huang J Z, Liu R X. Acta Metall Sin, 2013; 29: 506 |
| [8] | (李泓霖, 张 仲, 吕英波, 黄金昭, 刘如喜. 金属学报, 2013; 29: 506) |
| [9] | Aravind A, Hasna K, Jayaraj M K, Kumar M, Chandra R. Appl Phys, 2014; 115A: 843 |
| [10] | Li Q, Wang Y Y, Fan L L, Liu J D, Kong W, Ye B J. Scr Mater, 2013; 69: 694 |
| [11] | Ney A, Ney V, Kieschnick M, Wilhelm F, Ollefs K, Rogalev A. J Appl Phys, 2014; 115: 172603 |
| [12] | Li B B, Richard A, Chen Z F, Shen H L, Luo J. J Sol-Gel Sci Technol, 2014; 70: 19 |
| [13] | He R L, Tang B, Ton-That C, Phillips M, Tsuzuki T. J Nanopart Res, 2013; 15: 2030 |
| [14] | Rusu G G, Rambu A P, Buta V E, Dobromir M, Luca D, Rusu M. Mater Chem Phys, 2010; 123: 314 |
| [15] | Rambu A P, Sirbu D, Iftimie N, Rusu G I. Thin Solid Films, 2011; 520: 1303 |
| [16] | Condurache-Bota S, Tigau N, Rambu A P, Rusu G G, Rusu G I. Appl Surf Sci, 2011; 257: 10545 |
| [17] | Yildiz A, Kayhan B, Yurduguzel B, Rambu A P, Iacomi F, Simon S. J Mater Sci, 2011; 22: 1473 |
| [18] | Wang Q,He J C. Material Science Under High Magnetic Field. Beijing: Science Press, 2014: 1 |
| [18] | (王 强,赫冀成. 强磁场材料科学. 北京: 科学出版社, 2014: 1) |
| [19] | Tahashi M, Sassa K, Hirabayashi I, Asai S. Mater Trans, 2000; 41: 985 |
| [20] | Ren S Y, Ren Z M, Ren W L, Cao G H. Acta Phys Sin, 2009; 58: 5567 |
| [20] | (任树洋, 任忠鸣, 任维丽, 操光辉. 物理学报, 2009; 58: 5567) |
| [21] | Li G J, Du J J, Wang H M, Wang Q, Ma Y H, He J C. Mater Lett, 2014; 133: 53 |
| [22] | Wang Q, Cao Y Z, Li G J, Wang K, Du J J, He J C. Sci Adv Mater, 2013; 5: 447 |
| [23] | Cao Y Z, Wang Q, Li G J, Du J J, Wu C, He J C. J Magn Magn Mater, 2013; 332: 38 |
| [24] | Wang Q, Liu T, Gao A, Zhang C, Wang C J, He J C. Scr Mater, 2007; 56: 10587 |
| [25] | Rambu A P, Rusu G I. Superlattice Mirost, 2010; 47: 300 |
| [26] | Huang X H, Li G H, Cao B Q, Wang M, Hao C Y. J Phys Chem, 2009; 113C: 4381 |
| [27] | Rambu A P, Sirbu D, Dobromir M, Rusu G G. Solid State Sci, 2012; 14: 1543 |
| [28] | Huang X H, Tay C B, Zhan Z Y, Zhang C, Zheng L X, Venkatesan T, Chua S J. Cryst Eng Comm, 2011; 13: 447 |
| [29] | Huang X H, Zhang Z Y, Pramoda K P, Zhang C, Zheng L X, Chua S J. Cryst Eng Comm, 2012; 14: 5163 |
/
| 〈 |
|
〉 |