INFLUENCE OF TEMPERATURE ON LOW-CYCLE FATIGUE BEHAVIOR OF INCONEL 625 NICKEL-BASED SUPERALLOY WELDING JOINT

  • Yuanyuan WANG ,
  • Lijia CHEN ,
  • Baosen WANG
Expand
  • 1 School of Materials Science and Engineering, Shenyang University of Technology, Shenyang 110870
    2 Institute for Welding and Surface Technology of R&D Center, Baoshan Iron & Steel Co. LTD Research Institute, Shanghai 201900

Revised date: 2014-05-06

  Online published: 2014-12-25

Abstract

The low-cycle fatigue tests of Inconel 625 nickel-based superalloy welding joints at 25 and 760 ℃ were performed . The strain-fatigue life data and cyclic stress-strain data were analyzed to determine the strain fatigue parameters of Inconel 625 superalloy welding joints. The result showed that the relationship between elastic strain amplitude, plastic strain amplitude and reversals to failure could be described by Basquin and Coffin-Manson equations, respectively. Under the strain control, the continuous cyclic softening was observed at 25 ℃, however, the cyclic hardening appeared at 760 ℃. At 25 ℃, the fatigue crack of Inconel 625 superalloy welding joints initiated transgranularly at the specimen surface and propagated in the transgranular mode. Differently, at 760 ℃, the fatigue crack initiated transgranularly at the specimen surface, but propagated in mixed transgranular and intergranular modes.

Cite this article

Yuanyuan WANG , Lijia CHEN , Baosen WANG . INFLUENCE OF TEMPERATURE ON LOW-CYCLE FATIGUE BEHAVIOR OF INCONEL 625 NICKEL-BASED SUPERALLOY WELDING JOINT[J]. Acta Metall Sin, 2014 , 50(12) : 1485 -1490 . DOI: 10.11900/0412.1961.2014.00241

References

[1] Yan S C, Cheng M, Zhang S H, Zhang H Y, Zhang W H, Zhang L W. Chin J Mater Res, 2010; 24: 239
[1] (闫士彩, 程 明, 张士宏, 张海燕, 张伟红, 张立文. 材料研究学报, 2010; 24: 239)
[2] Mathew M, Parameswaran P. Mater Charact, 2008; 59: 5
[3] Thomas C,Tait P. Int J Pressure Vessels Piping, 1994; 59: 1
[4] Wang H Y, An Y Q, Li C Y, Chao B, Ni Y, Liu G B, Li P. Mater Rev, 2011; 25: 482
[4] (王会阳, 安云岐, 李承宇, 晁 兵, 倪 雅, 刘国彬, 李 萍. 材料导报, 2011; 25: 482)
[5] Zhang B, Xiao D M. Mech Res Appl, 2011; (3): 19
[5] (张 彬, 肖德明. 机械研究与应用, 2011; (3): 19)
[6] Guo Y, Hou S F, Zhou R C. J Chin Soc Power Eng, 2010; 30: 966
[6] (郭 岩, 侯淑芳, 周荣灿. 动力工程学报, 2010; 30: 966)
[7] Li W Y, Liu H F, Wang T, Zhao S Q. Mater Mech Eng, 2008; 32(7): 46
[7] (李维银, 刘红飞, 王 婷, 赵双群. 机械工程材料, 2008; 32(7): 46)
[8] Huang Z W, Yuan F H, Wang Z G, Zhu S J, Wang F G. Acta Metall Sin, 2007; 43: 678
[8] (黄志伟, 袁福河, 王中光, 朱世杰, 王富岗. 金属学报, 2007; 43: 678)
[9] Chen L J, Wu W, Liaw P K. Acta Metall Sin, 2006; 42: 952
[9] (陈立佳, 吴 崴, Liaw P K. 金属学报, 2006; 42: 952)
[10] Chen L J, Wang Z G, Yao G, Tian J F. Acta Metall Sin, 1999; 35:1144
[10] (陈立佳, 王中光, 姚 戈, 田继丰. 金属学报, 1999; 35: 1144)
[11] Lord D C, Coffin L F. Metall Trans, 1973; 4: 1647
[12] Antolovich S D, Liu S, Baur R. Metall Trans, 1981; 12A: 473
[13] Reuchet J, Remy L. Mater Sci Eng, 1983; A58: 19
[14] Rao K B S, Schiffers H, Schuster H, Nickel H. Metall Trans, 1988; 19A: 359
[15] Valsan M, Shastry D H, Rao K B, Mannan S L. Metall Trans, 1994; 25A: 159
[16] Li S X, Smith D J. Fatigue Fract Eng Mater Struct, 1995; 18: 631
[17] Hwang S K, Lee H N, Yoon B H. Metall Trans, 1989; 20: 2793
[18] Liu Y, Chen L J, Wang Z G. Acta Metall Sin, 1999; 35: 955
[18] (刘 毅, 陈立佳, 王中光. 金属学报, 1999; 35: 955)
[19] Hwang S K, Lee H N, Yoon B H. Metall Trans, 1989; 20: 2793
[20] Worithem D W, Robertson I M, Leckie F A, Socie D F, Altstetter C J. Metall Trans, 1990; 21: 3215
[21] Leverant G R, Kear B H. Metall Trans, 1970; 1: 491
[22] Kim T K, Yu Y, Jeon T Y. Metall Trans, 1992; 23: 2581
[23] Link T, Feller-Kniepmeier M. Metall Trans, 1992; 23: 99
[24] Carry C S, Strudel J L. Acta Metall, 1977; 25: 767
[25] Carry C S, Strudel J L. Acta Metall, 1978; 26: 859
[26] Portella P D, Bertram A, Fahlbusch E, Frenz H, Kinder J. In: Lutjering G, Mowalk H eds., Proceedings of the Sixth International Fatigue Congress, 1996: 795
[27] Henderson P J, Lindblom J. Scr Mater, 1997; 37: 491
[28] Zhang J H, Hu Z Q, Xu Y B, Wang Z G. Metall Trans, 1992; 23: 1253
[29] Monier C, Bertrand J P, Trichet M F, Cornet M. Mater Sci Eng, 1994; A188: 133
[30] Mason S S. Exp Mech, 1965; 5: 193
Outlines

/