MODELING AND SIMULATION OF STRUCTURAL FORMATION OF POROUS ALUMINUM IN GASAR SOLIDIFICATION

  • Qianqian YANG ,
  • Yuan LIU ,
  • Yanxiang LI
Expand
  • 1 School of Materials Science and Engineering, Tsinghua University, Beijing 100084
    2 Key Laboratory for Advanced Materials Processing Technology (Ministry of Education), Tsinghua University, Beijing 100084

Received date: 2014-09-04

  Revised date: 2014-06-09

  Online published: 2014-11-25

Supported by

National Natural Science Foundation of China (No.51271096) and New Century Excellent Talents in University (No.NCET-12-0310)

Abstract

The solid/gas eutectic unidirectional solidification process is a new kind of technology fabricating the lotus-type porous structure. Besides having the properties of large specific surface area, excellent sound absorption, penetrating performance etc. of traditional porous materials, the particularity of the lotus-type porous structure makes it has extraordinary mechanical and thermal properties. There is a great potential for lotus-type porous aluminum in the field of lightweight engineering and heat dissipation of chip owing to its low density, outstanding corrosion resistance and high thermal conductivity. However, the fabrication of lotus-type porous aluminum has always been more difficulty than other metals. Until porous aluminum with excellent pore structure was fabricated under very small solidification rates (0.008~0.015 mm/s) and high superheat degrees of melt (240~340 K), the proper processing parameters were recognized to be essential for the coupled growth of solid/gas phases for Al-H2 system, especially the solidification rate. In this work, a three-dimensional time-dependent model describing the evolution of single pore was established based on the theoretical analysis of mass transfer, gas bubble nucleation, pore growth, interruption and detachment. The morphology of single pore under different solidification rates were simulated during the Gasar process by using the finite difference method for Al-H2 system. The research reveals: coupled growth of solid/gas phases can be achieved under the solidification rates from 0.15 mm/s to 0.005 mm/s. The average pore diameter which ranges from 100 mm to 1100 mm increases with decreasing the solidification rate. The pore length also increases while the pore aspect ratio is nearly a constant about 40 with decreasing the solidification rate. The simulated average pore diameter is in good agreement with the experimental values when solidification rate equals to 0.015 mm/s, and then being slightly lower than the experimental ones with decreasing the solidification rate. The diffusion of hydrogen into the melt during the solidification process is regarded as the main reason of the discrepancy between simulated and experimental average pore diameters. The maximum value of the simulated solidification rates for coupled growth of solid/gas phases in Al-H2 system first increases from less than 0.01 mm/s to 0.15 mm/s and then being a constant, while the minimum ones increase from about 0.0001 mm/s to 0.01 mm/s with improving the overheat degree of melt and hydrogen partial pressure. By comparing the relative parameters of Al-H2 and Cu-H2 systems, the solubility of hydrogen is regarded to be the main parameter which determines solidification rates of coupled growth of solid/gas phases for Al-H2 system.

Cite this article

Qianqian YANG , Yuan LIU , Yanxiang LI . MODELING AND SIMULATION OF STRUCTURAL FORMATION OF POROUS ALUMINUM IN GASAR SOLIDIFICATION[J]. Acta Metall Sin, 2014 , 50(11) : 1403 -1412 . DOI: 10.11900/0412.1961.2014.00300

References

[1] Banhart J. Prog Mater Sci, 2001; 46: 559
[2] Nakajima H. Prog Mater Sci, 2007; 52: 1091
[3] Jiang G R, Li Y X, Liu Y. Metall Mater Trans, 2010; 41A: 3405
[4] Li Z J, Jin Q L, Yang T W, Jiang Y H, Zhou R. Acta Metall Sin, 2013; 49: 757
[4] (李再久, 金青林, 杨天武, 蒋业华, 周 荣. 金属学报, 2013; 49: 757)
[5] Shapovalov V I. US Pat, 5181549, 1993
[6] Simone A E, Gibson L J. Acta Mater, 1996; 44: 1437
[7] Hyun S K, Nakajima H. Mater Sci Eng, 2003; A340: 258
[8] Muramatsu K, Ide T, Nakajima H, Eaton J K. J Heat Transfer, 2013; 135: 072601
[9] Chen L T, Zhang H W, Liu Y, Li Y X. Acta Metall Sin, 2012; 48: 329
[9] (陈刘涛, 张华伟, 刘 源, 李言祥. 金属学报, 2012; 48: 329)
[10] Zhang H W, Chen L T, Liu Y, Li Y X. Int J Heat Mass Transfer, 2013; 56: 172
[11] Nakajima H. Proc Jpn Acad Ser B, 2010; 86: 884
[12] Zhang H W, Li Y X, Liu Y. Acta Metall Sin, 2006; 42: 1165
[12] (张华伟, 李言祥, 刘 源. 金属学报, 2006; 42: 1165)
[13] Park J S, Hyun S K, Suzuki S, Nakajima H. Acta Mater, 2007; 55: 5646
[14] Zhou R, Li Z H, Jiang Y H, Zhou R F, Yang T W, Jin Q L. Chin Pat, 200910094262.8, 2009
[14] (周 荣, 黎振华, 蒋业华, 周荣锋, 杨天武, 金青林. 中国专利, 200910094262.8, 2009)
[15] Zahrani M M, Meratian M, Kabiri Y. Mater Lett, 2012; 85: 14
[16] Zhou R, Jiang Y H, Li Z H, Jin Q L, Yang T W, Zhou R F. Chin Pat, 200910094261.3, 2009
[16] (周 荣, 蒋业华, 黎振华, 金青林, 杨天武, 周荣锋. 中国专利, 200910094261.3, 2009)
[17] Tane M, Nakajima H. J Mater Res, 2008; 23: 849
[18] Liu Y, Li Y X, Zhang H W. Acta Metall Sin, 2004; 40: 1121
[18] (刘 源, 李言祥, 张华伟. 金属学报, 2004; 40: 1121)
[19] Zhang H W, Li Y X, Liu Y. Acta Metall Sin, 2007; 43: 11
[19] (张华伟, 李言祥, 刘 源. 金属学报, 2007; 43: 11)
[20] Komissarchuk O, Xu Z B, Hao H, Zhang X L, Vladimir K. China Foundry, 2014; 11: 1
[21] Ide T, Iio Y, Nakajima H. Metall Mater Trans, 2012; 43A: 5140
[22] Drenchev L, Sobczak J, Malinov S, Sha W. Modell Simul Mater Sci Eng, 2006; 14: 663
[23] Li Y X,Wu A P. Principle of Materials Processing. Beijing: Tsinghua University Press, 2005: 83
[23] (李言祥,吴爱萍. 材料加工原理. 北京: 清华大学出版社, 2005: 83)
[24] Zhang H W, Li Y X, Liu Y. Acta Metall Sin, 2007; 43: 113
[24] (张华伟, 李言祥, 刘 源. 金属学报, 2007; 43: 113)
[25] Kurz W, Fisher D J. Fundamental of Solidification. Switzerland: Trans Tech Publications, 1998: 22
[26] Zhang H W, Li Y X. Acta Phys Sin, 2007; 56: 4864
[26] (张华伟, 李言祥. 物理学报, 2007; 56: 4864)
[27] Chen Z F. Bachelor Thesis, Tsinghua University, Beijing, 2011
[27] (陈自发. 清华大学学士学位论文, 北京, 2011)
[28] Liu Y, Li Y X. Scr Mater, 2003; 49: 379
[29] Li Z J, Jin Q L, Yang T W, Zhou R, Jiang Y H. Acta Metall Sin, 2014; 50: 507
[29] (李再久, 金青林, 杨天武, 周 荣, 蒋业华. 金属学报, 2014; 50: 507)
[30] Zhang H W. PhD Dissertation, Tsinghua University, Beijing, 2006
[30] (张华伟. 清华大学博士学位论文, 北京, 2006)
[31] Fisher D J. Hydrogen Diffusion in Metals—A 30 Year Retrospective. Switzerland: Scitec Publications Ltd, 1999: 37
[32] Sigrist P, Feichtinger H K, Marincek B. Z Phys Chem-Frankfurt, 1977; 107: 211
Outlines

/

〈 〉