NUMERICAL STUDY ON FREE-CUTTING PHASE PRECIPITATION BEHAVIOR IN Fe-Bi-Mn TERNARY ALLOY MULTIPHASE TRANSFORMATION- DIFFUSION SYSTEM

  • Zhe WANG ,
  • Fazhan WANG ,
  • Yinhua HE ,
  • Xin WANG ,
  • Shan MA ,
  • Huimian WANG
Expand
  • 1 College of Materials and Mineral Resources, Xi′an University of Architecture and Technology, Xi′an 710055
    2 School of Mechanical and Electrical Engineering, Xi′an University of Architecture and Technology, Xi′an 710055
    3 Technology Center, Shanxi Taigang Stainless Steel Co. Ltd., Taiyuan 030003

Received date: 2014-07-25

  Revised date: 2014-04-23

  Online published: 2014-11-25

Supported by

National Science and Technology Pillar Program During the Twelfth Five-Year Plan Period (No.2011BAE31B02) and Preparation and Processing of Non-ferrous Materials of High Performance for Innovative Research of Xi′an University of Architecture and Technology of China

Abstract

The solidification process of alloys are not just liquid to solid phase transformation, in fact in some alloys liquid to gas and gas to liquid phase transformation processes happen. A method incorporating the full diffusion-governed phase transformation kinetics into a multiphase volume average solidification model is presented. The motivation to develop such a model is to predict the multiple effect of inclusions precipitation behavior in castings. A key feature of this model, different from most previous ones which usually assume an infinite solute mixing in liquid lead to erroneous estimation of the multiphase diffusion path, is that diffusions in solid, liquid and gas phases are considered. Here solidification of Fe-Bi-Mn ternary alloy is examined. As MnS and Bi have large differences in the solute partition coefficient, diffusion coefficient and liquidus slope, the multiphase diffusion path shows differently from those predicted by infinite liquid mixing models. In this work, a three-dimensional mathematical model for a three-phase flow during its horizontai solidification was studied based on diffusion-governed phase transformation kinetics. Effects of Fe-Bi-Mn ternary alloy solidification on solid-liquid-gas phase transformation were considered. The free-cutting phase precipitation behavior was studied and multiphase transformation and multiphase diffusion path of free-cutting phase precipitation behavior were analyzed. Results show that the multiphase transformation-diffusion is strongly influenced by free-cutting phases precipitation behavior: MnS has a relatively large partition coefficient and small diffusion coefficient with larger Mls,MnS (solid-liquid mass transfer rate of MnS). During solidification, C*s,MnS (solid interface concentration of MnS) may become even larger than Cl,MnS (liquid concentration of MnS), MnS in liquid is assumed to be fully ‘trapped’ in solid and there is no longer any enrichment of MnS; however Bi has a relatively small partition coefficient and large diffusion coefficient with smaller Mls,Bi (solid-liquid mass transfer rate of Bi) and negative Mgl,Bi (liquid-gas mass transfer rate of Bi), during solidification, Cl,Bi (liquid concentration of Bi) always greater than C*s,Bi (solid interface concentration of Bi). In addition, due to the existence of Bi-gas phase, Bi continuous to flow, enriched in the solidified around MnS. Calculated results show good agreement with experimental data.

Cite this article

Zhe WANG , Fazhan WANG , Yinhua HE , Xin WANG , Shan MA , Huimian WANG . NUMERICAL STUDY ON FREE-CUTTING PHASE PRECIPITATION BEHAVIOR IN Fe-Bi-Mn TERNARY ALLOY MULTIPHASE TRANSFORMATION- DIFFUSION SYSTEM[J]. Acta Metall Sin, 2014 , 50(11) : 1393 -1402 . DOI: 10.11900/0412.1961.2014.00200

References

[1] Krishtal M A, Borgardt A A, Yashin Y D. Met Sci Heat Treat, 1977; 19: 178
[2] Lou D, Cui K, Jia Y. J Mater Eng Perform, 1997; 6: 215
[3] Akasawa T, Sakurai H, Nakamura M, Tanaka T, Takano K. J Mater Process Technol, 2003; 143: 66
[4] Iwamoto T, Murakami T. Jfe Tech Rep, 2004; 4: 64
[5] Wu D, Li Z. J Iron Steel Res Int, 2010; 17: 59
[6] Li Y, Suzuki T, Tang N, Koizumi Y, Chiba A. Mater Sci Eng, 2013; A583: 161
[7] Bhattacharya D. Metall Mater Trans, 1981; 12A: 973
[8] Yaguchi H. Mater Sci Tech-Lond, 1989; 5: 255
[9] Xu J L, Song B, Chen J K, Han Q Y, Jiang G C. Acta Metall Sin, 1993; 29: 65
[9] (徐建伦, 宋 波, 陈继开, 韩其勇, 蒋国昌. 金属学报, 1993; 29: 65)
[10] Wang Z, Wang F Z, Wang X, He Y H, Ma S, Wu Z. Acta Phys Sin, 2014; 63: 076101
[10] (王 哲, 王发展, 王 欣, 何银花, 马 姗, 吴 振. 物理学报, 2014; 63: 076101)
[11] Li J, Wu M, Hao J, Ludwig A. Comp Mater Sci, 2012; 55: 407
[12] Ueshima Y, Sawada Y, Mizoguchi S, Kajioka H. Metall Mater Trans, 1989; 20A: 1375
[13] Yamamoto K, Shibata H, Mizoguchi S. ISIJ Int, 2006; 46: 82
[14] Schneider M C, Beckermann C. Int J Heat Mass Transfer, 1995; 38: 3455
[15] Dupont J N. Metall Mater Trans, 2006; 37A: 1937
[16] Wang T M, Li T J, Cao Z Q, Jin J Z, Grimmig T, Bührig-Polaczek A, Wu M, Ludwig A. Acta Metall Sin, 2006; 42: 591
[16] (王同敏, 李廷举, 曹志强, 金俊泽, Grimmig T, Bührig-Polaczek A, Wu M, Ludwig A. 金属学报, 2006; 42: 591)
[17] Beckermann C, Viskanta R. Appl Mech Rev, 1993; 46: 1
[18] Ludwig A, Wu M. Metall Mater Trans, 2002; 33A: 3673
[19] Ahmad N, Rappaz J, Desbiolles J L, Jalanti T, Rappaz M, Combeau H. Metall Mater Trans, 1998; 29A: 617
[20] Wu M, Ludwig A, Bührig-Polaczek A, Fehlbier M, Sahm P R. Int J Heat Mass Transfer, 2003; 46: 2819
[21] Xu D, Bai Y, Fu H, Guo J. Int J Heat Mass Transfer, 2005; 48: 2219
[22] Wu M, K?n?zsy L, Ludwig A, Schutzenhofer W, Tanzer R. Steel Res Int, 2008; 79: 637
[23] Zalo?nik M, Combeau H. Int J Therm Sci, 2010; 49: 1500
[24] Zhao G W, Li X Z, Xu D M, Fu H Z, Du Y, He Y H. Acta Metall Sin, 2011; 47: 1135
[24] (赵光伟, 李新中, 徐达鸣, 傅恒志, 杜 勇, 贺跃辉. 金属学报, 2011; 47: 1135)
[25] Peng D J, Lin X, Zhang Y P, Guo X, Wang M, Huang W D. Acta Metall Sin, 2013; 49: 365
[25] (彭东剑, 林 鑫, 张云鹏, 郭 雄, 王 猛, 黄卫东. 金属学报, 2013; 49: 365)
[26] Kurz W, Fisher D J. Fundamentals of Solidification. Switzerland: Trans Tech Publication, 1998: 280
[27] Galenko P K, Danilov D A. J Cryst Growth, 1999; 197: 992
[28] Guttmann M. Metall Mater Trans, 1977; 8A: 1383
[29] Temmel C, Ingesten N G, Karlsson B. Metall Mater Trans, 2006; 37A: 2995
[30] Kang Y B. Calphad, 2010; 34: 232
[31] Rangel R H, Bian X. Numer Heat Transfer, 1995; 28A: 589
[32] Rangel R H, Bian X. Int J Heat Mass Transfer, 1996; 39: 1591
[33] Bian X, Rangel R H. Int J Heat Mass Transfer, 1998; 41: 244
[34] American Society for Metals. ASM Metals Handbook. Michigan: ASM International, 1987: 83
[35] Brandes E A, Brook G B. Smithell's Light Metals Handbook. Massachusetts: Elsevier Science and Technology, 1998: 36
[36] Ayyar A, Chawla N. Compos Sci Technol, 2006; 66: 1980
Outlines

/

〈 〉